Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.288 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.83 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.758 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 154.3 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 207.8 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 154.3 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 103.9 |
Te2W (mp-22693) | <1 1 0> | <1 0 0> | 113.6 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 103.9 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 227.1 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 207.8 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 113.6 |
MgO (mp-1265) | <1 1 0> | <1 0 1> | 154.3 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 207.8 |
C (mp-66) | <1 0 0> | <1 0 1> | 154.3 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 1> | 154.3 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 1> | 154.3 |
KP(HO2)2 (mp-23959) | <0 1 1> | <1 0 0> | 113.6 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 103.9 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 207.8 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 207.8 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 0> | 227.1 |
WS2 (mp-224) | <1 0 0> | <1 0 0> | 227.1 |
ZrO2 (mp-2858) | <1 1 -1> | <1 0 0> | 227.1 |
YAlO3 (mp-3792) | <0 1 0> | <1 0 0> | 113.6 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 103.9 |
ZnO (mp-2133) | <1 0 0> | <1 0 0> | 227.1 |
MgF2 (mp-1249) | <1 1 0> | <1 0 0> | 227.1 |
Cu (mp-30) | <1 0 0> | <0 0 1> | 103.9 |
LiAlO2 (mp-3427) | <1 1 0> | <1 0 0> | 227.1 |
Al2O3 (mp-1143) | <1 0 1> | <0 0 1> | 207.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na2Al2As3 (mp-17473) | 0.2991 | 0.000 | 3 |
K2In2As3 (mp-21741) | 0.3811 | 0.000 | 3 |
Rb2In2Sb3 (mp-21760) | 0.4210 | 0.000 | 3 |
K2In2Sb3 (mp-579637) | 0.3182 | 0.000 | 3 |
Na2Ga2As3 (mp-15431) | 0.2224 | 0.000 | 3 |
SrLi4NiO4 (mp-778288) | 0.5835 | 0.263 | 4 |
BaLi4NiO4 (mp-776790) | 0.5864 | 0.105 | 4 |
Li8Mn(O2F)2 (mp-780086) | 0.6185 | 0.071 | 4 |
LiCaGaN2 (mp-570948) | 0.5080 | 0.000 | 4 |
LiCaAlN2 (mp-1020031) | 0.4677 | 0.000 | 4 |
MgSi2 (mp-1073528) | 0.6343 | 0.150 | 2 |
Mg3Si4 (mp-1075152) | 0.6344 | 0.150 | 2 |
Mg5Si9 (mp-1075658) | 0.6358 | 0.198 | 2 |
Mg5Si9 (mp-1075724) | 0.5786 | 0.253 | 2 |
CdO2 (mp-1096876) | 0.6427 | 0.515 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Al Sb |
Final Energy/Atom-3.5026 eV |
Corrected Energy-200.7509 eV
Uncorrected energy = -196.1429 eV
Composition-based energy adjustment (-0.192 eV/atom x 24.0 atoms) = -4.6080 eV
Corrected energy = -200.7509 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)