Final Magnetic Moment1.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.382 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.013 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.52 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToRbF3 + RbF + RbTb3F10 |
Band Gap0.039 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 270.6 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 271.7 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 210.6 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 217.4 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 210.6 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 271.7 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 205.1 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 326.1 |
CdS (mp-672) | <1 1 1> | <0 1 1> | 102.5 |
YVO4 (mp-19133) | <0 0 1> | <0 1 1> | 102.5 |
YVO4 (mp-19133) | <1 0 1> | <0 1 1> | 205.1 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 86.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 270.6 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 217.4 |
GaSe (mp-1943) | <1 0 0> | <1 0 0> | 270.6 |
GaSe (mp-1943) | <1 0 1> | <1 0 0> | 270.6 |
BN (mp-984) | <1 0 0> | <1 1 0> | 210.6 |
TeO2 (mp-2125) | <0 1 0> | <1 0 0> | 270.6 |
TeO2 (mp-2125) | <1 0 0> | <1 0 0> | 270.6 |
SiC (mp-7631) | <1 0 1> | <0 1 0> | 326.1 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 260.8 |
MgO (mp-1265) | <1 1 1> | <1 0 1> | 126.6 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 180.4 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 217.4 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 326.1 |
C (mp-66) | <1 0 0> | <0 1 1> | 102.5 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 260.8 |
LaF3 (mp-905) | <1 0 0> | <0 1 1> | 102.5 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 1> | 253.2 |
BaTiO3 (mp-5986) | <1 0 1> | <0 1 0> | 217.4 |
BaTiO3 (mp-5986) | <1 1 0> | <0 1 0> | 217.4 |
Si (mp-149) | <1 1 0> | <1 1 0> | 210.6 |
WS2 (mp-224) | <1 0 1> | <0 1 0> | 326.1 |
C (mp-48) | <1 0 0> | <0 0 1> | 173.9 |
C (mp-48) | <1 0 1> | <0 0 1> | 260.8 |
ZrO2 (mp-2858) | <0 0 1> | <0 1 0> | 54.3 |
ZrO2 (mp-2858) | <0 1 1> | <0 1 0> | 271.7 |
ZrO2 (mp-2858) | <1 1 -1> | <0 1 0> | 217.4 |
ZrO2 (mp-2858) | <1 1 0> | <0 1 0> | 271.7 |
YAlO3 (mp-3792) | <0 1 0> | <1 0 0> | 270.6 |
CdWO4 (mp-19387) | <0 1 0> | <0 1 0> | 54.3 |
CdWO4 (mp-19387) | <0 1 1> | <0 1 0> | 163.0 |
CdWO4 (mp-19387) | <1 0 0> | <1 0 1> | 126.6 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 86.9 |
CdWO4 (mp-19387) | <1 1 0> | <0 1 0> | 163.0 |
CdWO4 (mp-19387) | <1 1 1> | <0 1 1> | 102.5 |
MgF2 (mp-1249) | <1 0 1> | <1 0 0> | 180.4 |
MgF2 (mp-1249) | <1 1 1> | <0 1 0> | 271.7 |
ZnO (mp-2133) | <1 0 0> | <0 1 0> | 326.1 |
Cu (mp-30) | <1 0 0> | <0 0 1> | 260.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZrTlF5 (mp-30997) | 0.6228 | 0.000 | 3 |
Th(InBr3)2 (mp-617543) | 0.4299 | 0.000 | 3 |
K2ZrF6 (mp-5450) | 0.3250 | 0.000 | 3 |
K2HfF6 (mp-14128) | 0.3928 | 0.000 | 3 |
K2TbF6 (mp-4377) | 0.3549 | 0.017 | 3 |
SbF4 (mvc-15178) | 0.5861 | 0.183 | 2 |
ThI4 (mp-27697) | 0.5946 | 0.000 | 2 |
Sr2Sb3 (mp-16897) | 0.5207 | 0.000 | 2 |
Ba2Sb3 (mp-16922) | 0.6072 | 0.000 | 2 |
NaTe (mp-28353) | 0.5942 | 0.007 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Rb_sv Tb_3 F |
Final Energy/Atom-5.0614 eV |
Corrected Energy-91.1058 eV
-91.1058 eV = -91.1058 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)