Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.511 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.21 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.686 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 102.3 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 -1> | 71.8 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 67.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 172.6 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 134.2 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 201.3 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 67.1 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 204.6 |
SiO2 (mp-6930) | <1 0 0> | <1 0 -1> | 215.5 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 -1> | 215.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 -1> | 215.5 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 230.1 |
BN (mp-984) | <1 0 0> | <1 0 -1> | 215.5 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 287.7 |
Al (mp-134) | <1 0 0> | <0 0 1> | 287.7 |
Al (mp-134) | <1 1 0> | <1 1 1> | 163.4 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 -1> | 215.5 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 134.2 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 230.1 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 201.3 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 287.7 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 230.1 |
C (mp-66) | <1 1 0> | <1 0 0> | 268.4 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 172.6 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 57.5 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 268.4 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 0 1> | 230.1 |
KP(HO2)2 (mp-23959) | <1 0 1> | <1 0 0> | 134.2 |
KP(HO2)2 (mp-23959) | <1 1 0> | <1 0 0> | 134.2 |
LaF3 (mp-905) | <1 1 1> | <1 0 0> | 201.3 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 287.7 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 57.5 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 57.5 |
GaAs (mp-2534) | <1 1 1> | <1 0 -1> | 287.3 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 268.4 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 287.7 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 172.6 |
ZnSe (mp-1190) | <1 1 1> | <1 0 -1> | 287.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 287.7 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 143.7 |
LiF (mp-1138) | <1 1 0> | <1 1 1> | 163.4 |
Te2W (mp-22693) | <1 0 1> | <1 0 0> | 201.3 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 230.1 |
Ag (mp-124) | <1 1 0> | <1 1 -1> | 146.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 172.6 |
BN (mp-984) | <0 0 1> | <1 0 0> | 201.3 |
BN (mp-984) | <1 0 1> | <1 0 0> | 201.3 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 230.1 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 172.6 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 287.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
7.54 | -0.00 | -0.93 |
-0.00 | 7.72 | 0.00 |
-0.93 | 0.00 | 6.48 |
Dielectric Tensor εij (total) |
||
---|---|---|
10.67 | -0.00 | -1.13 |
-0.00 | 11.61 | 0.00 |
-1.13 | 0.00 | 8.64 |
Polycrystalline dielectric constant
εpoly∞
7.25
|
Polycrystalline dielectric constant
εpoly
10.31
|
Refractive Index n2.69 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca4SnS6 (mp-866473) | 0.6333 | 0.146 | 3 |
Cd2PCl2 (mp-31276) | 0.5738 | 0.015 | 3 |
CaSiN2 (mp-568965) | 0.6156 | 0.000 | 3 |
SrGeN2 (mp-1029497) | 0.5898 | 0.000 | 3 |
NaNbN2 (mp-1030657) | 0.4661 | 0.000 | 3 |
NaLi3GeO4 (mp-561254) | 0.5866 | 0.000 | 4 |
K2Ag6Sn3S10 (mp-559880) | 0.5452 | 0.000 | 4 |
NaLi3SiO4 (mp-559904) | 0.5551 | 0.000 | 4 |
K2CdSiO4 (mp-541538) | 0.5662 | 0.000 | 4 |
Sr2Y2Sn2O7 (mvc-3361) | 0.5692 | 0.268 | 4 |
AgP2 (mp-8200) | 0.6982 | 0.015 | 2 |
Sn3P4 (mp-684588) | 0.6568 | 0.211 | 2 |
Cd7P10 (mp-29576) | 0.6706 | 0.036 | 2 |
Li3P7 (mp-28336) | 0.7376 | 0.000 | 2 |
Sr2AlCr2GaO7 (mvc-312) | 0.6899 | 0.186 | 5 |
Sr2YGaW2O7 (mvc-359) | 0.6170 | 0.412 | 5 |
Sr2AlV2GaO7 (mvc-350) | 0.6858 | 0.223 | 5 |
Sr2AlGaFe2O7 (mvc-13325) | 0.5712 | 0.108 | 5 |
Run TypeGGA |
Energy Cutoff700 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv B Se |
Final Energy/Atom-4.3621 eV |
Corrected Energy-78.5184 eV
-78.5184 eV = -78.5184 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)