material

YCuP2

ID:

mp-30208

DOI:

10.17188/1204620


Tags: Yttrium copper phosphide (1/1/2)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.870 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.25 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P4/nmm [129]
Hall
P 4ab 2ab 1ab
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CdSe (mp-2691) <1 0 0> <0 0 1> 0.000 347.3
Au (mp-81) <1 0 0> <0 0 1> 0.003 69.5
GaSb (mp-1156) <1 0 0> <0 0 1> 0.004 347.3
Ag (mp-124) <1 0 0> <0 0 1> 0.006 69.5
Ni (mp-23) <1 0 0> <0 0 1> 0.007 111.1
GaN (mp-804) <1 1 0> <1 0 1> 0.012 116.9
PbSe (mp-2201) <1 0 0> <0 0 1> 0.017 347.3
SrTiO3 (mp-4651) <1 0 0> <1 0 1> 0.017 350.8
SrTiO3 (mp-4651) <1 1 0> <0 0 1> 0.017 125.0
Ni (mp-23) <1 1 0> <1 0 1> 0.030 155.9
Ni (mp-23) <1 1 1> <1 0 0> 0.037 254.9
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.045 125.0
C (mp-48) <0 0 1> <0 0 1> 0.047 111.1
DyScO3 (mp-31120) <0 1 0> <0 0 1> 0.049 347.3
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.051 111.1
YAlO3 (mp-3792) <1 1 0> <0 0 1> 0.051 55.6
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.053 27.8
GaN (mp-804) <1 0 1> <0 0 1> 0.055 208.4
ZrO2 (mp-2858) <1 0 1> <1 1 1> 0.059 213.4
LiGaO2 (mp-5854) <1 1 0> <1 0 0> 0.062 145.7
BaTiO3 (mp-5986) <1 0 1> <1 0 0> 0.067 327.8
LiNbO3 (mp-3731) <1 0 0> <0 0 1> 0.081 222.2
CdWO4 (mp-19387) <1 1 1> <1 0 1> 0.082 155.9
TbScO3 (mp-31119) <0 1 0> <0 0 1> 0.089 347.3
Mg (mp-153) <1 0 1> <0 0 1> 0.095 208.4
CsI (mp-614603) <1 0 0> <0 0 1> 0.096 125.0
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.098 206.0
KCl (mp-23193) <1 1 0> <1 0 1> 0.100 116.9
MgF2 (mp-1249) <1 0 1> <0 0 1> 0.124 208.4
Ga2O3 (mp-886) <1 1 1> <1 0 0> 0.125 254.9
Al (mp-134) <1 1 0> <1 1 0> 0.125 206.0
MgO (mp-1265) <1 1 1> <0 0 1> 0.128 222.2
LaF3 (mp-905) <1 1 0> <0 0 1> 0.129 277.8
DyScO3 (mp-31120) <1 1 0> <0 0 1> 0.134 125.0
LiGaO2 (mp-5854) <0 1 0> <1 1 1> 0.139 266.7
SrTiO3 (mp-4651) <1 0 1> <1 0 0> 0.141 109.3
SiC (mp-7631) <1 0 0> <0 0 1> 0.142 236.1
LiNbO3 (mp-3731) <1 0 1> <1 1 0> 0.146 154.5
LiTaO3 (mp-3666) <1 0 1> <1 1 0> 0.149 154.5
MgO (mp-1265) <1 1 0> <1 0 1> 0.154 78.0
LiAlO2 (mp-3427) <1 0 1> <1 1 1> 0.160 213.4
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.162 27.8
Mg (mp-153) <1 1 0> <1 0 1> 0.168 116.9
NdGaO3 (mp-3196) <1 0 0> <0 0 1> 0.170 347.3
CdWO4 (mp-19387) <0 0 1> <1 0 1> 0.172 272.8
CdWO4 (mp-19387) <0 1 1> <1 1 1> 0.172 160.0
Te2Mo (mp-602) <0 0 1> <1 0 1> 0.174 194.9
C (mp-48) <1 0 0> <1 1 0> 0.178 154.5
ZrO2 (mp-2858) <1 0 -1> <1 1 1> 0.182 106.7
ZnO (mp-2133) <1 0 0> <1 1 0> 0.182 51.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
198 62 63 0 0 0
62 198 63 0 0 0
63 63 171 0 0 0
0 0 0 33 0 0
0 0 0 0 33 0
0 0 0 0 0 66
Compliance Tensor Sij (10-12Pa-1)
6 -1.3 -1.7 0 0 0
-1.3 6 -1.7 0 0 0
-1.7 -1.7 7.1 0 0 0
0 0 0 30.3 0 0
0 0 0 0 30.3 0
0 0 0 0 0 15.1
Shear Modulus GV
52 GPa
Bulk Modulus KV
105 GPa
Shear Modulus GR
46 GPa
Bulk Modulus KR
105 GPa
Shear Modulus GVRH
49 GPa
Bulk Modulus KVRH
105 GPa
Elastic Anisotropy
0.56
Poisson's Ratio
0.30

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TbCuAs2 (mp-7194) 0.2443 0.000 3
HoCuP2 (mp-30195) 0.0295 0.000 3
YCuAs2 (mp-10991) 0.2225 0.000 3
ErCuAs2 (mp-10993) 0.2509 0.000 3
DyCuAs2 (mp-10992) 0.2423 0.000 3
ZrCuSiP (mp-20588) 0.2307 0.000 4
ZrCuGeAs (mp-1078698) 0.2778 0.000 4
ZrCuSiAs (mp-9929) 0.3236 0.000 4
HfCuGeAs (mp-1080723) 0.3265 0.000 4
HfCuSiAs (mp-1079332) 0.3650 0.000 4
CuSe (mp-580226) 0.7020 0.044 2
CaPd2 (mp-1063133) 0.5421 0.297 2
ThFe2 (mp-1062988) 0.5661 0.384 2
NiSe (mp-571033) 0.6900 0.064 2
EuPd2 (mp-1063311) 0.5781 0.313 2
Ce8Fe8As8O7F (mp-705511) 0.7412 0.123 5
Na (mp-1079952) 0.6881 0.086 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Y_sv Cu_pv P
Final Energy/Atom
-6.2178 eV
Corrected Energy
-49.7421 eV
-49.7421 eV = -49.7421 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 95177
Submitted by
User remarks:
  • Yttrium copper phosphide (1/1/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)