Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.457 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.62 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.179 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 0 -1> | 216.1 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 163.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 169.8 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 283.0 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 120.8 |
GaN (mp-804) | <0 0 1> | <1 0 -1> | 72.0 |
GaN (mp-804) | <1 0 0> | <1 1 1> | 153.1 |
SiO2 (mp-6930) | <1 0 0> | <1 0 -1> | 216.1 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 81.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 -1> | 216.1 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 188.1 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 163.5 |
CdS (mp-672) | <0 0 1> | <1 0 -1> | 216.1 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 113.2 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 169.8 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 120.8 |
YVO4 (mp-19133) | <1 0 0> | <1 0 -1> | 144.1 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 339.6 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 283.0 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 219.6 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 339.6 |
GaSe (mp-1943) | <1 1 0> | <0 0 1> | 113.2 |
BN (mp-984) | <0 0 1> | <0 0 1> | 283.0 |
BN (mp-984) | <1 0 1> | <0 0 1> | 339.6 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 245.3 |
MoS2 (mp-1434) | <1 0 0> | <0 0 1> | 283.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 -1> | 216.1 |
MoS2 (mp-1434) | <1 0 1> | <0 0 1> | 283.0 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 163.5 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 226.4 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 169.8 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 282.2 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 -1> | 72.0 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 -1> | 144.1 |
CdTe (mp-406) | <1 1 0> | <1 0 1> | 120.8 |
SiC (mp-7631) | <0 0 1> | <1 0 -1> | 216.1 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 226.4 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 339.6 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 339.6 |
TiO2 (mp-2657) | <1 1 0> | <1 0 -1> | 216.1 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 163.5 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 169.8 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 339.6 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 56.6 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 -1> | 216.1 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 245.3 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 282.2 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 169.8 |
KP(HO2)2 (mp-23959) | <1 1 0> | <1 0 -1> | 144.1 |
PbS (mp-21276) | <1 1 1> | <0 1 0> | 188.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ScPS4 (mp-6999) | 0.2476 | 0.000 | 3 |
LaOsN3 (mp-989632) | 0.6495 | 0.020 | 3 |
Ge(PbS2)2 (mp-560370) | 0.6638 | 0.000 | 3 |
Cs3DyO3 (mp-779546) | 0.6921 | 0.009 | 3 |
Cs3HoO3 (mp-753923) | 0.6947 | 0.010 | 3 |
CaBiAsO6 (mvc-11848) | 0.5306 | 0.114 | 4 |
CsGdSiS4 (mp-630711) | 0.5136 | 0.000 | 4 |
CsSmGeS4 (mp-556979) | 0.5480 | 0.000 | 4 |
CsSmSiS4 (mp-561635) | 0.5330 | 0.000 | 4 |
CsErSiS4 (mp-16972) | 0.5189 | 0.000 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Lu_3 P S |
Final Energy/Atom-5.4281 eV |
Corrected Energy-140.8886 eV
-140.8886 eV = -130.2733 eV (uncorrected energy) - 10.6154 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)