material

Y3Al

ID:

mp-30338

DOI:

10.17188/1204754


Tags: Aluminum yttrium (1/3)

Material Details

Final Magnetic Moment
0.036 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.185 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.051 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.46 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Y2Al + Y
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pm3m [221]
Hall
-P 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 58212 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Cu (mp-30) <1 1 1> <1 1 1> 0.000 158.5
Ni (mp-23) <1 1 1> <1 1 1> 0.001 277.4
CaF2 (mp-2741) <1 1 0> <1 1 0> 0.004 129.4
CaF2 (mp-2741) <1 1 1> <1 1 1> 0.004 158.5
KP(HO2)2 (mp-23959) <0 1 0> <1 0 0> 0.013 228.8
C (mp-66) <1 0 0> <1 0 0> 0.013 114.4
SiC (mp-7631) <0 0 1> <1 1 1> 0.018 158.5
KP(HO2)2 (mp-23959) <1 0 0> <1 0 0> 0.018 114.4
Ge3(BiO3)4 (mp-23560) <1 0 0> <1 0 0> 0.019 114.4
GaP (mp-2490) <1 1 0> <1 1 0> 0.020 129.4
GaP (mp-2490) <1 1 1> <1 1 1> 0.020 158.5
KP(HO2)2 (mp-23959) <0 0 1> <1 0 0> 0.020 228.8
SiC (mp-11714) <0 0 1> <1 1 1> 0.021 158.5
Al2O3 (mp-1143) <0 0 1> <1 0 0> 0.024 160.2
KCl (mp-23193) <1 0 0> <1 0 0> 0.024 205.9
Ga2O3 (mp-886) <1 1 0> <1 1 0> 0.032 291.2
Ag (mp-124) <1 1 0> <1 1 0> 0.039 97.1
Ag (mp-124) <1 1 1> <1 1 1> 0.040 118.9
Fe2O3 (mp-24972) <0 0 1> <1 1 1> 0.046 158.5
Bi2Te3 (mp-34202) <0 0 1> <1 1 1> 0.048 118.9
Mg (mp-153) <1 1 0> <1 1 0> 0.050 258.9
MgO (mp-1265) <1 0 0> <1 0 0> 0.051 91.5
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.060 205.9
C (mp-48) <0 0 1> <1 0 0> 0.063 183.0
Te2W (mp-22693) <1 1 1> <1 1 0> 0.065 226.5
CsI (mp-614603) <1 1 0> <1 1 0> 0.079 258.9
NdGaO3 (mp-3196) <0 1 0> <1 1 0> 0.081 129.4
TiO2 (mp-390) <0 0 1> <1 0 0> 0.084 114.4
DyScO3 (mp-31120) <1 0 1> <1 0 0> 0.097 274.6
Au (mp-81) <1 1 0> <1 1 0> 0.101 97.1
Ni (mp-23) <1 1 0> <1 1 0> 0.101 194.2
Au (mp-81) <1 1 1> <1 1 1> 0.103 118.9
BaF2 (mp-1029) <1 1 1> <1 1 1> 0.105 277.4
YVO4 (mp-19133) <0 0 1> <1 0 0> 0.109 205.9
GaN (mp-804) <1 1 0> <1 1 0> 0.117 258.9
PbS (mp-21276) <1 0 0> <1 0 0> 0.120 183.0
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.139 355.9
NdGaO3 (mp-3196) <0 1 1> <1 1 0> 0.146 258.9
CdS (mp-672) <1 1 1> <1 0 0> 0.156 205.9
BN (mp-984) <1 0 1> <1 1 0> 0.159 355.9
GaTe (mp-542812) <1 0 0> <1 1 0> 0.161 226.5
BaTiO3 (mp-5986) <1 0 1> <1 1 1> 0.162 277.4
TbScO3 (mp-31119) <1 0 1> <1 0 0> 0.166 274.6
TiO2 (mp-390) <1 0 0> <1 0 0> 0.166 183.0
C (mp-48) <1 0 1> <1 1 0> 0.168 161.8
TiO2 (mp-390) <1 1 0> <1 1 0> 0.169 258.9
Te2Mo (mp-602) <1 0 1> <1 1 0> 0.175 226.5
LiGaO2 (mp-5854) <1 0 0> <1 1 0> 0.176 323.6
NdGaO3 (mp-3196) <1 0 0> <1 1 0> 0.199 355.9
Si (mp-149) <1 1 0> <1 1 0> 0.202 129.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
83 33 33 0 0 0
33 83 33 0 0 0
33 33 83 0 0 0
0 0 0 38 0 0
0 0 0 0 38 0
0 0 0 0 0 38
Compliance Tensor Sij (10-12Pa-1)
15.5 -4.4 -4.4 0 0 0
-4.4 15.5 -4.4 0 0 0
-4.4 -4.4 15.5 0 0 0
0 0 0 26.4 0 0
0 0 0 0 26.4 0
0 0 0 0 0 26.4
Shear Modulus GV
33 GPa
Bulk Modulus KV
49 GPa
Shear Modulus GR
32 GPa
Bulk Modulus KR
49 GPa
Shear Modulus GVRH
32 GPa
Bulk Modulus KVRH
49 GPa
Elastic Anisotropy
0.20
Poisson's Ratio
0.23

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ZnCu2Ni (mp-30593) 0.1125 0.005 3
CrCoPt2 (mp-570863) 0.0492 0.034 3
LiCa6Ge (mp-12609) 0.0000 0.183 3
GaFeNi2 (mp-1065359) 0.0412 0.065 3
GaCo2Ni (mp-1018060) 0.0157 0.075 3
Cr8Ni50Mo15W2 (mp-767372) 0.2155 0.028 4
CrFeCoNi (mp-1012640) 0.3608 0.065 4
CrFeCoNi (mp-1096923) 0.4019 0.193 4
TmAl3 (mp-768) 0.0000 0.000 2
In3As (mp-973466) 0.0000 0.201 2
Pr3Pb (mp-21481) 0.0000 0.017 2
Fe3Ge (mp-20344) 0.0000 0.005 2
SmPt3 (mp-30845) 0.0000 0.000 2
H2 (mp-634659) 0.0000 2.277 1
Sn (mp-1022725) 0.0000 0.054 1
Sr (mp-76) 0.0000 0.006 1
Ni (mp-1056486) 0.0000 0.000 1
Cd (mp-1096861) 0.0000 0.000 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Y_sv Al
Final Energy/Atom
-5.9713 eV
Corrected Energy
-23.8851 eV
Uncorrected energy = -23.8851 eV Corrected energy = -23.8851 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 58212
Submitted by
User remarks:
  • Aluminum yttrium (1/3)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)