Final Magnetic Moment0.030 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.699 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density13.24 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 340.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 275.1 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 1> | 168.5 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 194.6 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 206.4 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 252.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 68.8 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 84.2 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 145.9 |
Al (mp-134) | <1 1 0> | <1 1 0> | 68.8 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 291.8 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 340.5 |
C (mp-66) | <1 1 0> | <1 1 1> | 252.7 |
C (mp-66) | <1 1 1> | <1 0 0> | 340.5 |
GdScO3 (mp-5690) | <1 0 1> | <1 1 1> | 168.5 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 243.2 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 145.9 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 206.4 |
PbS (mp-21276) | <1 1 1> | <1 1 1> | 252.7 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 48.6 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 68.8 |
Ni (mp-23) | <1 1 1> | <1 1 1> | 84.2 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 194.6 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 340.5 |
AlN (mp-661) | <1 0 0> | <1 1 1> | 252.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 243.2 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 137.6 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 275.1 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 194.6 |
NdGaO3 (mp-3196) | <0 0 1> | <1 1 0> | 275.1 |
NdGaO3 (mp-3196) | <0 1 1> | <1 1 0> | 275.1 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 243.2 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 243.2 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 340.5 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 206.4 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 194.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 275.1 |
SiC (mp-11714) | <0 0 1> | <1 0 0> | 291.8 |
SiC (mp-11714) | <1 0 0> | <1 1 0> | 275.1 |
SiC (mp-11714) | <1 1 0> | <1 1 0> | 206.4 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 0> | 194.6 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 243.2 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 137.6 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 275.1 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 206.4 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 68.8 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 84.2 |
Si (mp-149) | <1 0 0> | <1 0 0> | 243.2 |
Au (mp-81) | <1 1 0> | <1 1 0> | 275.1 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 194.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
UInAu2 (mp-20358) | 0.0000 | 0.008 | 3 |
Li2AgPb (mp-30349) | 0.0000 | 0.000 | 3 |
HfAlPd2 (mp-16501) | 0.0000 | 0.000 | 3 |
Li2AlPt (mp-30818) | 0.0000 | 0.000 | 3 |
LiGa2Rh (mp-4913) | 0.0000 | 0.000 | 3 |
LiMgSnPd (mp-7555) | 0.0000 | 0.000 | 4 |
VFeCoGe (mp-1063914) | 0.0000 | 0.000 | 4 |
TiFeCoGe (mp-1018012) | 0.0000 | 0.028 | 4 |
LiMgSbPd (mp-10179) | 0.0000 | 0.074 | 4 |
LiMgSnPt (mp-11806) | 0.0000 | 0.000 | 4 |
Li3Bi (mp-23222) | 0.0000 | 0.000 | 2 |
Sr3In (mp-31349) | 0.0000 | 0.131 | 2 |
Fe3Ge (mp-20711) | 0.0000 | 0.000 | 2 |
GdMg3 (mp-20534) | 0.0000 | 0.000 | 2 |
Li3Sb (mp-2074) | 0.0000 | 0.000 | 2 |
Eu (mp-20071) | 0.0000 | 0.083 | 1 |
Ce (mp-10024) | 0.0000 | 0.228 | 1 |
Lu (mp-10190) | 0.0000 | 0.132 | 1 |
Np (mp-10207) | 0.0000 | 0.447 | 1 |
Na (mp-127) | 0.0000 | 0.004 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Er_3 In_d Au |
Final Energy/Atom-4.1663 eV |
Corrected Energy-16.6651 eV
-16.6651 eV = -16.6651 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)