Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.614 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.99 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.312 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 0> | 248.0 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 265.1 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 231.3 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 309.3 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 261.0 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 237.6 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 209.6 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 176.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 149.1 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 158.4 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 176.8 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 265.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 82.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 335.5 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 335.5 |
Te2W (mp-22693) | <1 0 0> | <0 1 1> | 289.1 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 176.8 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 279.5 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 186.4 |
Ag (mp-124) | <1 1 1> | <1 0 1> | 237.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 69.9 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 309.3 |
BN (mp-984) | <1 1 1> | <0 0 1> | 298.2 |
LiNbO3 (mp-3731) | <1 1 1> | <0 0 1> | 261.0 |
Al (mp-134) | <1 1 0> | <0 0 1> | 335.5 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 223.7 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 149.1 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 261.0 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 220.9 |
LiTaO3 (mp-3666) | <1 1 0> | <1 1 0> | 248.0 |
LiTaO3 (mp-3666) | <1 1 1> | <0 0 1> | 261.0 |
Fe3O4 (mp-19306) | <1 0 0> | <0 1 1> | 289.1 |
MgO (mp-1265) | <1 0 0> | <1 1 0> | 165.4 |
TiO2 (mp-2657) | <1 0 0> | <1 1 0> | 82.7 |
LaAlO3 (mp-2920) | <1 1 1> | <1 1 0> | 248.0 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 209.6 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 165.4 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 279.5 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 176.8 |
KCl (mp-23193) | <1 0 0> | <1 1 0> | 82.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 186.4 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 165.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 298.2 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 158.4 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 82.7 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 261.0 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 158.4 |
TePb (mp-19717) | <1 0 0> | <1 1 0> | 82.7 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 335.5 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 279.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
17.55 | 0.00 | 0.00 |
0.00 | 15.71 | 0.00 |
0.00 | 0.00 | 16.42 |
Dielectric Tensor εij (total) |
||
---|---|---|
32.15 | 0.00 | 0.00 |
0.00 | 27.61 | 0.00 |
0.00 | 0.00 | 29.95 |
Polycrystalline dielectric constant
εpoly∞
16.56
|
Polycrystalline dielectric constant
εpoly
29.90
|
Refractive Index n4.07 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
KRbS (mp-28760) | 0.2600 | 0.008 | 3 |
SrCaSn (mp-20726) | 0.3160 | 0.000 | 3 |
MoPRu (mp-22451) | 0.3145 | 0.000 | 3 |
VAsRh (mp-934092) | 0.2132 | 0.002 | 3 |
VAsRh (mp-20395) | 0.2085 | 0.002 | 3 |
Yb3In3Ge2Au (mp-981207) | 0.6877 | 0.000 | 4 |
Na2LiGaAs2 (mp-9722) | 0.5957 | 0.000 | 4 |
KNa4SnSb3 (mp-6758) | 0.5687 | 0.005 | 4 |
K3Na2SnBi3 (mp-568329) | 0.6290 | 0.000 | 4 |
K2NaInSb2 (mp-505767) | 0.6589 | 0.000 | 4 |
Ca2Si (mp-2517) | 0.0184 | 0.000 | 2 |
Na2S (mp-556978) | 0.1790 | 0.040 | 2 |
Sr2Ge (mp-2576) | 0.1335 | 0.000 | 2 |
Ba2Sn (mp-1981) | 0.1850 | 0.000 | 2 |
Sr2Si (mp-1106) | 0.1284 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv Ge_d |
Final Energy/Atom-3.4920 eV |
Corrected Energy-41.9042 eV
-41.9042 eV = -41.9042 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)