Material Details

Final Magnetic Moment
0.002 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.298 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.39 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Immm [71]
Hall
-I 2 2
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 58885 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
LiTaO3 (mp-3666) <0 0 1> <1 1 0> 0.001 187.6
PbS (mp-21276) <1 1 0> <0 1 0> 0.005 152.5
YAlO3 (mp-3792) <1 1 0> <0 1 1> 0.010 223.3
AlN (mp-661) <1 0 1> <0 1 0> 0.012 266.9
TbScO3 (mp-31119) <0 1 0> <1 0 1> 0.012 219.0
Mg (mp-153) <1 0 0> <0 1 1> 0.013 134.0
LiTaO3 (mp-3666) <1 1 0> <1 1 0> 0.016 125.1
GdScO3 (mp-5690) <0 1 1> <1 0 1> 0.017 54.7
PbS (mp-21276) <1 1 1> <0 0 1> 0.017 186.1
Mg (mp-153) <0 0 1> <0 0 1> 0.018 69.8
Mg (mp-153) <1 1 0> <0 0 1> 0.018 116.3
InP (mp-20351) <1 0 0> <0 1 1> 0.020 178.7
WSe2 (mp-1821) <1 0 0> <1 1 0> 0.021 250.1
LiNbO3 (mp-3731) <0 0 1> <1 1 0> 0.022 187.6
MoSe2 (mp-1634) <1 0 1> <0 1 1> 0.026 312.7
MgO (mp-1265) <1 1 0> <0 1 0> 0.026 76.3
PbS (mp-21276) <1 0 0> <0 1 1> 0.028 178.7
DyScO3 (mp-31120) <0 1 0> <1 0 1> 0.029 219.0
ZrO2 (mp-2858) <0 1 1> <1 1 0> 0.035 312.6
InP (mp-20351) <1 1 1> <0 0 1> 0.039 186.1
NdGaO3 (mp-3196) <0 0 1> <0 0 1> 0.040 93.1
SiO2 (mp-6930) <1 0 0> <1 0 1> 0.042 54.7
C (mp-48) <0 0 1> <0 0 1> 0.045 116.3
GdScO3 (mp-5690) <0 1 0> <1 0 1> 0.047 219.0
Bi2Te3 (mp-34202) <0 0 1> <0 1 0> 0.047 343.2
GaN (mp-804) <1 1 0> <0 0 1> 0.047 116.3
LiNbO3 (mp-3731) <1 0 1> <0 1 1> 0.047 312.7
C (mp-48) <1 1 1> <0 1 1> 0.048 134.0
KCl (mp-23193) <1 1 0> <0 1 0> 0.050 114.4
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.050 69.8
WS2 (mp-224) <0 0 1> <0 0 1> 0.051 69.8
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.054 93.1
Au (mp-81) <1 0 0> <0 0 1> 0.057 69.8
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.059 148.7
ZrO2 (mp-2858) <0 0 1> <0 1 1> 0.059 223.3
LiAlO2 (mp-3427) <1 0 0> <0 1 1> 0.060 134.0
Si (mp-149) <1 0 0> <1 0 0> 0.061 148.7
InP (mp-20351) <1 1 0> <0 1 0> 0.062 152.5
CsI (mp-614603) <1 0 0> <0 0 1> 0.063 186.1
SrTiO3 (mp-4651) <1 1 0> <0 0 1> 0.065 186.1
WS2 (mp-224) <1 1 0> <0 0 1> 0.067 232.6
SrTiO3 (mp-4651) <1 0 0> <1 0 1> 0.072 219.0
Bi2Se3 (mp-541837) <1 0 1> <0 0 1> 0.073 255.9
TbScO3 (mp-31119) <0 1 1> <1 0 1> 0.073 54.7
MgO (mp-1265) <1 0 0> <0 1 1> 0.075 89.3
MoS2 (mp-1434) <1 1 0> <0 0 1> 0.075 116.3
KCl (mp-23193) <1 0 0> <1 0 0> 0.079 247.8
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.080 279.2
GaN (mp-804) <1 0 0> <0 1 1> 0.082 134.0
Ag (mp-124) <1 0 0> <0 0 1> 0.082 69.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
79 24 56 0 0 0
24 76 29 0 0 0
56 29 84 0 0 0
0 0 0 19 0 0
0 0 0 0 46 0
0 0 0 0 0 25
Compliance Tensor Sij (10-12Pa-1)
24.4 -1.5 -15.7 0 0 0
-1.5 15.2 -4.4 0 0 0
-15.7 -4.4 24 0 0 0
0 0 0 53 0 0
0 0 0 0 21.9 0
0 0 0 0 0 39.3
Shear Modulus GV
27 GPa
Bulk Modulus KV
51 GPa
Shear Modulus GR
22 GPa
Bulk Modulus KR
49 GPa
Shear Modulus GVRH
24 GPa
Bulk Modulus KVRH
50 GPa
Elastic Anisotropy
1.10
Poisson's Ratio
0.29

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Sr2CdPt2 (mp-1068157) 0.4424 0.000 3
Nd2AlNi2 (mp-1069330) 0.3480 0.000 3
Er2AlNi2 (mp-1068244) 0.4466 0.000 3
Ca2GaPt2 (mp-1078428) 0.3987 0.000 3
Ca2GePt2 (mp-1078483) 0.2798 0.000 3
K2Au3 (mp-8700) 0.7499 0.000 2
La2Ni3 (mp-1691) 0.7497 0.009 2
Nd2Co3 (mp-1084826) 0.7332 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ca_sv Ga_d Cu_pv
Final Energy/Atom
-3.3432 eV
Corrected Energy
-16.7159 eV
Uncorrected energy = -16.7159 eV Corrected energy = -16.7159 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 58885
Submitted by
User remarks:
  • Calcium copper gallium (2/2/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)