material

ZnCdPt2

ID:

mp-30493

DOI:

10.17188/1204897


Tags: Cadmium platinum zinc (1/2/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.448 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
14.63 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P4/mmm [123]
Hall
-P 4 2
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 102057 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
LaF3 (mp-905) <1 1 0> <1 1 0> 0.003 92.6
KP(HO2)2 (mp-23959) <0 0 1> <0 0 1> 0.004 226.9
Ge3(BiO3)4 (mp-23560) <1 0 0> <0 0 1> 0.004 113.4
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.007 109.1
Au (mp-81) <1 0 0> <0 0 1> 0.008 17.5
Y3Fe5O12 (mp-19648) <1 0 0> <0 0 1> 0.015 157.1
Mg (mp-153) <1 0 1> <1 0 1> 0.018 94.0
SiC (mp-11714) <1 1 0> <0 0 1> 0.019 270.5
BaF2 (mp-1029) <1 0 0> <0 0 1> 0.023 78.5
Fe2O3 (mp-24972) <1 0 1> <1 1 1> 0.025 224.5
WSe2 (mp-1821) <1 0 1> <1 1 1> 0.028 256.6
Ag (mp-124) <1 1 0> <0 0 1> 0.028 122.2
GaTe (mp-542812) <1 0 1> <0 0 1> 0.042 296.7
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.043 183.3
CdTe (mp-406) <1 0 0> <0 0 1> 0.043 43.6
Ag (mp-124) <1 1 1> <0 0 1> 0.043 209.4
KTaO3 (mp-3614) <1 1 0> <1 1 1> 0.043 160.4
ZrO2 (mp-2858) <1 0 -1> <0 0 1> 0.051 288.0
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.056 43.6
Ag (mp-124) <1 0 0> <0 0 1> 0.057 17.5
MoSe2 (mp-1634) <1 0 0> <1 1 1> 0.059 256.6
InSb (mp-20012) <1 0 0> <0 0 1> 0.059 43.6
LiAlO2 (mp-3427) <1 1 1> <1 0 0> 0.061 109.1
GdScO3 (mp-5690) <1 1 1> <1 1 1> 0.067 288.7
Au (mp-81) <1 1 0> <0 0 1> 0.068 122.2
TiO2 (mp-390) <1 0 1> <1 1 1> 0.077 160.4
Al (mp-134) <1 1 0> <1 1 1> 0.079 160.4
KP(HO2)2 (mp-23959) <1 0 0> <0 0 1> 0.079 113.4
SiO2 (mp-6930) <1 0 0> <0 0 1> 0.080 165.8
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.083 43.6
TeO2 (mp-2125) <0 1 1> <0 0 1> 0.084 305.4
Au (mp-81) <1 1 1> <0 0 1> 0.085 209.4
SrTiO3 (mp-4651) <1 1 0> <1 0 1> 0.085 188.0
MoS2 (mp-1434) <0 0 1> <1 1 0> 0.088 61.7
WS2 (mp-224) <0 0 1> <1 1 0> 0.088 61.7
NdGaO3 (mp-3196) <1 0 1> <1 1 0> 0.091 216.0
KP(HO2)2 (mp-23959) <0 1 0> <0 0 1> 0.096 226.9
InP (mp-20351) <1 1 1> <1 1 0> 0.099 61.7
Mg (mp-153) <0 0 1> <1 1 0> 0.100 61.7
SiC (mp-7631) <1 0 1> <0 0 1> 0.103 331.6
TiO2 (mp-2657) <1 1 0> <0 0 1> 0.109 78.5
LiAlO2 (mp-3427) <1 1 0> <1 1 0> 0.118 92.6
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.118 109.1
SiC (mp-11714) <1 0 0> <0 0 1> 0.119 218.2
TePb (mp-19717) <1 0 0> <0 0 1> 0.120 43.6
CdS (mp-672) <0 0 1> <1 1 0> 0.121 30.9
LiGaO2 (mp-5854) <0 1 1> <1 1 1> 0.121 128.3
GaTe (mp-542812) <1 0 -1> <1 1 0> 0.121 154.3
LiAlO2 (mp-3427) <1 0 0> <0 0 1> 0.121 130.9
TiO2 (mp-2657) <1 1 1> <0 0 1> 0.125 235.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
242 95 129 0 0 0
95 242 129 0 0 0
129 129 204 0 0 0
0 0 0 66 0 0
0 0 0 0 66 0
0 0 0 0 0 48
Compliance Tensor Sij (10-12Pa-1)
6.3 -0.5 -3.6 0 0 0
-0.5 6.3 -3.6 0 0 0
-3.6 -3.6 9.5 0 0 0
0 0 0 15.2 0 0
0 0 0 0 15.2 0
0 0 0 0 0 20.6
Shear Modulus GV
58 GPa
Bulk Modulus KV
155 GPa
Shear Modulus GR
55 GPa
Bulk Modulus KR
155 GPa
Shear Modulus GVRH
57 GPa
Bulk Modulus KVRH
155 GPa
Elastic Anisotropy
0.30
Poisson's Ratio
0.34

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
LuAl2Pd5 (mp-1025564) 0.1920 0.000 3
NpAl2Pd5 (mp-569227) 0.3961 0.154 3
UAl2Pd5 (mp-569698) 0.3832 0.075 3
YAl2Pd5 (mp-1078938) 0.3261 0.000 3
PuAl2Pd5 (mp-1091385) 0.4031 0.227 3
Al3Cu (mp-985825) 0.4508 0.044 2
Mn2Au (mp-30409) 0.5524 0.235 2
Mn3Pd5 (mp-1078895) 0.5992 0.000 2
VIr (mp-1079131) 0.5518 0.019 2
Ga3Ni5 (mp-11398) 0.5120 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Zn Cd Pt
Final Energy/Atom
-4.0253 eV
Corrected Energy
-16.1010 eV
Uncorrected energy = -16.1010 eV Corrected energy = -16.1010 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 102057
Submitted by
User remarks:
  • Cadmium platinum zinc (1/2/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)