Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.617 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.62 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.698 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP212121 [19] |
HallP 2ac 2ab |
Point Group222 |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 167.2 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 239.7 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 191.7 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 287.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 253.2 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 0> | 167.2 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 117.2 |
CdS (mp-672) | <1 1 0> | <0 1 1> | 253.2 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 257.2 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 117.2 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 335.5 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 239.7 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 287.6 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 335.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 191.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 239.7 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 239.7 |
BN (mp-984) | <0 0 1> | <0 0 1> | 287.6 |
BN (mp-984) | <1 0 0> | <0 0 1> | 239.7 |
BN (mp-984) | <1 0 1> | <0 0 1> | 239.7 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 239.7 |
Al (mp-134) | <1 1 0> | <0 1 1> | 253.2 |
Al (mp-134) | <1 1 1> | <1 1 0> | 167.2 |
TeO2 (mp-2125) | <0 1 1> | <0 1 0> | 234.3 |
TeO2 (mp-2125) | <1 0 1> | <0 1 0> | 234.3 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 287.6 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 239.7 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 287.6 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 191.7 |
C (mp-66) | <1 0 0> | <1 0 1> | 128.6 |
C (mp-66) | <1 1 0> | <0 0 1> | 143.8 |
C (mp-66) | <1 1 1> | <0 0 1> | 335.5 |
GdScO3 (mp-5690) | <1 0 1> | <1 1 0> | 167.2 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 239.7 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 239.7 |
KP(HO2)2 (mp-23959) | <1 0 0> | <0 0 1> | 239.7 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 239.7 |
TbScO3 (mp-31119) | <1 0 1> | <1 1 0> | 167.2 |
Ni (mp-23) | <1 1 0> | <1 1 1> | 174.0 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 191.7 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 143.8 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 239.7 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 239.7 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 287.6 |
Ga2O3 (mp-886) | <1 0 -1> | <0 0 1> | 191.7 |
C (mp-48) | <1 0 0> | <0 0 1> | 335.5 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 239.7 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 143.8 |
ZrO2 (mp-2858) | <1 0 0> | <0 0 1> | 239.7 |
Si (mp-149) | <1 0 0> | <0 0 1> | 239.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.11093 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.16088 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.07660 |
Piezoelectric Modulus ‖eij‖max0.16088 C/m2 |
Crystallographic Direction vmax |
---|
0.00000 |
1.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
5.66 | 0.00 | 0.00 |
0.00 | 6.01 | 0.00 |
0.00 | 0.00 | 6.40 |
Dielectric Tensor εij (total) |
||
---|---|---|
16.63 | 0.00 | 0.00 |
0.00 | 19.08 | 0.00 |
0.00 | 0.00 | 15.18 |
Polycrystalline dielectric constant
εpoly∞
6.02
|
Polycrystalline dielectric constant
εpoly
16.96
|
Refractive Index n2.45 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TeS7Br2 (mp-683875) | 0.6954 | 0.003 | 3 |
KPO3 (mp-675976) | 0.5931 | 1.511 | 3 |
CsSbS6 (mp-28701) | 0.6548 | 0.000 | 3 |
NaClO2 (mp-676673) | 0.6798 | 0.299 | 3 |
Se2NCl3 (mp-571134) | 0.6975 | 0.180 | 3 |
Se2S(NCl)2 (mp-559231) | 0.5599 | 0.208 | 4 |
Se2SN2Cl (mp-628633) | 0.6367 | 0.246 | 4 |
SrH2I2O (mp-703295) | 0.6166 | 0.000 | 4 |
TeS2(NCl)2 (mp-556430) | 0.5548 | 0.168 | 4 |
Se2S(NCl)2 (mp-653096) | 0.5324 | 0.217 | 4 |
SeCl (mp-504825) | 0.5367 | 0.022 | 2 |
SeBr (mp-570589) | 0.4591 | 0.006 | 2 |
SBr (mp-28099) | 0.5971 | 0.000 | 2 |
Rb2S5 (mp-16911) | 0.5822 | 0.000 | 2 |
K2S5 (mp-17146) | 0.5560 | 0.000 | 2 |
TeSeS(NCl)2 (mp-23650) | 0.6657 | 0.199 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tl_d S |
Final Energy/Atom-3.7720 eV |
Corrected Energy-118.8863 eV
-118.8863 eV = -105.6171 eV (uncorrected energy) - 13.2692 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)