Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.456 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.741 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.79 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTi2Co |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFd3m [227] |
HallF 4d 2 3 1d |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 1 1> | 260.6 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 250.7 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 212.8 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 250.7 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 250.7 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 141.8 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 283.7 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 200.6 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 212.8 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 260.6 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 86.9 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 212.8 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 200.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 283.7 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 212.8 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 250.7 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 200.6 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 212.8 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 260.6 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 250.7 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 141.8 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 283.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 70.9 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 86.9 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 150.4 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 141.8 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 70.9 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 86.9 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 283.7 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 212.8 |
BN (mp-984) | <1 0 0> | <1 0 0> | 150.4 |
BN (mp-984) | <1 1 0> | <1 1 1> | 260.6 |
Te2W (mp-22693) | <1 1 0> | <1 1 0> | 212.8 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 50.1 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 200.6 |
YVO4 (mp-19133) | <1 1 1> | <1 0 0> | 250.7 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 212.8 |
Al (mp-134) | <1 1 0> | <1 1 0> | 70.9 |
Al (mp-134) | <1 1 1> | <1 1 1> | 86.9 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 150.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 150.4 |
Fe3O4 (mp-19306) | <1 1 0> | <1 1 0> | 212.8 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 283.7 |
LiGaO2 (mp-5854) | <0 1 0> | <1 1 1> | 260.6 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 250.7 |
TeO2 (mp-2125) | <0 0 1> | <1 1 0> | 283.7 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 200.6 |
C (mp-66) | <1 0 0> | <1 0 0> | 50.1 |
GdScO3 (mp-5690) | <1 0 1> | <1 1 1> | 173.7 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 250.7 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
147 | 123 | 123 | 8 | 6 | -6 |
123 | 147 | 123 | 6 | 8 | -6 |
123 | 123 | 147 | 6 | 6 | -8 |
8 | 6 | 6 | 21 | 0 | 0 |
6 | 8 | 6 | 0 | 21 | 0 |
-6 | -6 | -8 | 0 | 0 | 21 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
28.6 | -13 | -13 | -3.2 | 0.4 | -0.4 |
-13 | 28.6 | -13 | 0.4 | -3.2 | -0.4 |
-13 | -13 | 28.6 | 0.4 | 0.4 | 3.2 |
-3.2 | 0.4 | 0.4 | 48 | 0.6 | -0.6 |
0.4 | -3.2 | 0.4 | 0.6 | 48 | -0.6 |
-0.4 | -0.4 | 3.2 | -0.6 | -0.6 | 48 |
Shear Modulus GV18 GPa |
Bulk Modulus KV131 GPa |
Shear Modulus GR16 GPa |
Bulk Modulus KR125 GPa |
Shear Modulus GVRH17 GPa |
Bulk Modulus KVRH128 GPa |
Elastic Anisotropy0.51 |
Poisson's Ratio0.44 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YbNi4Au (mp-1024977) | 0.0000 | 0.040 | 3 |
TmInCu4 (mp-1024957) | 0.0028 | 0.000 | 3 |
GdNi4Au (mp-1077131) | 0.0027 | 0.855 | 3 |
YbCu4Au (mp-1077165) | 0.0028 | 0.000 | 3 |
GdInCu4 (mp-1077293) | 0.0009 | 0.000 | 3 |
YbAl2 (mp-969) | 0.0000 | 0.000 | 2 |
ScAl2 (mp-813) | 0.0000 | 0.000 | 2 |
NpMn2 (mp-1859) | 0.0000 | 0.222 | 2 |
NdNi2 (mp-1343) | 0.0000 | 0.001 | 2 |
PuNi2 (mp-30803) | 0.0000 | 0.387 | 2 |
Co (mp-1072089) | 0.0000 | 0.199 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ti_pv Co |
Final Energy/Atom-7.1767 eV |
Corrected Energy-43.0602 eV
-43.0602 eV = -43.0602 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)