material

Hf2Cu

ID:

mp-30581

DOI:

10.17188/1204969


Tags: Copper hafnium (1/2)

Material Details

Final Magnetic Moment
0.002 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.158 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
12.40 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4/mmm [139]
Hall
-I 4 2
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 102966 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
MgO (mp-1265) <1 0 0> <0 0 1> 0.000 90.5
Fe3O4 (mp-19306) <1 0 0> <0 0 1> 0.002 291.7
TiO2 (mp-390) <0 0 1> <0 0 1> 0.007 130.8
Te2W (mp-22693) <1 0 1> <0 0 1> 0.008 100.6
LiAlO2 (mp-3427) <1 1 0> <0 0 1> 0.009 140.8
KP(HO2)2 (mp-23959) <0 0 1> <0 0 1> 0.017 150.9
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.019 80.5
CdWO4 (mp-19387) <1 0 1> <1 0 1> 0.020 221.4
NdGaO3 (mp-3196) <1 0 1> <1 0 0> 0.021 106.5
CdS (mp-672) <1 0 1> <1 0 1> 0.036 295.2
WS2 (mp-224) <1 0 0> <0 0 1> 0.049 90.5
SrTiO3 (mp-4651) <1 0 0> <1 0 0> 0.052 177.5
Mg (mp-153) <1 0 0> <0 0 1> 0.053 50.3
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.058 160.9
ZnSe (mp-1190) <1 0 0> <0 0 1> 0.060 130.8
C (mp-66) <1 1 0> <0 0 1> 0.064 251.5
NaCl (mp-22862) <1 0 0> <0 0 1> 0.066 130.8
AlN (mp-661) <1 1 0> <0 0 1> 0.067 191.1
Te2W (mp-22693) <0 0 1> <0 0 1> 0.070 201.2
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.073 80.5
TeO2 (mp-2125) <0 1 1> <1 1 0> 0.074 150.6
MoS2 (mp-1434) <1 0 1> <0 0 1> 0.084 271.6
MgO (mp-1265) <1 1 0> <1 0 1> 0.094 258.3
BaTiO3 (mp-5986) <1 0 1> <1 0 1> 0.101 184.5
GdScO3 (mp-5690) <0 0 1> <1 0 1> 0.103 258.3
YVO4 (mp-19133) <1 1 0> <0 0 1> 0.103 321.9
GaAs (mp-2534) <1 0 0> <0 0 1> 0.104 130.8
LiF (mp-1138) <1 1 0> <0 0 1> 0.110 261.5
WS2 (mp-224) <0 0 1> <1 0 0> 0.114 35.5
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.115 35.5
BaTiO3 (mp-5986) <1 1 0> <0 0 1> 0.125 120.7
GdScO3 (mp-5690) <1 0 0> <1 0 1> 0.139 184.5
WS2 (mp-224) <1 1 1> <1 0 0> 0.139 319.5
KP(HO2)2 (mp-23959) <0 1 0> <0 0 1> 0.141 150.9
MoSe2 (mp-1634) <1 0 1> <0 0 1> 0.147 311.8
LaF3 (mp-905) <1 1 0> <0 0 1> 0.147 281.6
Al (mp-134) <1 0 0> <0 0 1> 0.148 80.5
NdGaO3 (mp-3196) <1 1 1> <0 0 1> 0.152 271.6
GaN (mp-804) <1 1 0> <1 0 0> 0.157 177.5
MgF2 (mp-1249) <1 0 1> <1 0 0> 0.161 106.5
LiAlO2 (mp-3427) <1 0 0> <0 0 1> 0.162 100.6
SiO2 (mp-6930) <1 0 0> <0 0 1> 0.165 191.1
MoS2 (mp-1434) <1 0 0> <0 0 1> 0.166 201.2
Mg (mp-153) <0 0 1> <1 0 0> 0.168 35.5
GdScO3 (mp-5690) <0 1 0> <1 0 0> 0.180 177.5
GaN (mp-804) <0 0 1> <1 0 0> 0.188 35.5
Bi2Te3 (mp-34202) <1 0 0> <0 0 1> 0.199 140.8
Ge (mp-32) <1 0 0> <0 0 1> 0.202 130.8
Cu (mp-30) <1 1 1> <0 0 1> 0.204 160.9
C (mp-66) <1 0 0> <0 0 1> 0.211 50.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
205 69 98 0 0 0
69 205 98 0 0 0
98 98 173 0 0 0
0 0 0 71 0 0
0 0 0 0 71 0
0 0 0 0 0 51
Compliance Tensor Sij (10-12Pa-1)
6.8 -0.6 -3.5 0 0 0
-0.6 6.8 -3.5 0 0 0
-3.5 -3.5 9.7 0 0 0
0 0 0 14.1 0 0
0 0 0 0 14.1 0
0 0 0 0 0 19.6
Shear Modulus GV
60 GPa
Bulk Modulus KV
123 GPa
Shear Modulus GR
56 GPa
Bulk Modulus KR
123 GPa
Shear Modulus GVRH
58 GPa
Bulk Modulus KVRH
123 GPa
Elastic Anisotropy
0.31
Poisson's Ratio
0.30

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Li2CuGe (mp-676117) 0.6686 0.008 3
YHfMg6 (mp-1022697) 0.4118 0.089 3
FeSnRh2 (mp-1018062) 0.5848 0.000 3
MnGaNi2 (mp-601285) 0.6662 0.000 3
Hf2Zn (mp-1014231) 0.1811 0.000 2
Zr2Cu (mp-193) 0.2341 0.000 2
Tb2Mg (mp-13498) 0.2219 0.016 2
Sm2Mg (mp-980558) 0.1610 0.017 2
Zr2Au (mp-2348) 0.2395 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Hf_pv Cu_pv
Final Energy/Atom
-8.1623 eV
Corrected Energy
-24.4869 eV
-24.4869 eV = -24.4869 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 627900
  • 102966
Submitted by
User remarks:
  • Copper hafnium (1/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)