Final Magnetic Moment14.199 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingUnknown |
Formation Energy / Atom-0.207 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.008 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.39 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToErNi5 + Ni |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 176.8 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 0> | 228.4 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 58.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 131.9 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 228.4 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 228.4 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 58.9 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 228.4 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 65.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 176.8 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 197.8 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 235.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 58.9 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 329.7 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 263.7 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 263.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 263.7 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 65.9 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 228.4 |
BN (mp-984) | <0 0 1> | <0 0 1> | 235.7 |
BN (mp-984) | <1 0 1> | <1 0 0> | 263.7 |
BN (mp-984) | <1 1 1> | <0 0 1> | 235.7 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 0> | 228.4 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 263.7 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 329.7 |
Al (mp-134) | <1 0 0> | <1 0 0> | 65.9 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 294.6 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 131.9 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 235.7 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 65.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 65.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 329.7 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 294.6 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 263.7 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 329.7 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 197.8 |
LiTaO3 (mp-3666) | <1 0 0> | <1 1 0> | 228.4 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 263.7 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 176.8 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 235.7 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 235.7 |
C (mp-66) | <1 1 0> | <0 0 1> | 294.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 176.8 |
BN (mp-984) | <1 0 0> | <1 0 0> | 197.8 |
BN (mp-984) | <1 1 0> | <1 0 1> | 265.3 |
GdScO3 (mp-5690) | <1 0 0> | <1 1 0> | 228.4 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 65.9 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 263.7 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 131.9 |
Al (mp-134) | <1 1 0> | <1 0 0> | 329.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Pu2Ni17 (mp-567327) | 0.0653 | 0.013 | 2 |
Th2Ni17 (mp-30810) | 0.1000 | 0.016 | 2 |
Gd2Ni17 (mp-580102) | 0.0666 | 0.013 | 2 |
Tm2Ni17 (mp-11527) | 0.0232 | 0.006 | 2 |
Tb2Ni17 (mp-569945) | 0.0477 | 0.004 | 2 |
Ce(Al5Ru)2 (mp-31364) | 0.6154 | 0.000 | 3 |
Nd2Zn15Ge2 (mp-542178) | 0.5874 | 0.043 | 3 |
U(Al5Fe)2 (mp-20548) | 0.6143 | 0.000 | 3 |
ThCo9Si2 (mp-17474) | 0.6041 | 0.000 | 3 |
SmCo9Si2 (mp-17623) | 0.6024 | 0.031 | 3 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points12 |
U Values-- |
PseudopotentialsVASP PAW: Ni_pv Er_3 |
Final Energy/Atom-5.8570 eV |
Corrected Energy-222.5674 eV
-222.5674 eV = -222.5674 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)