Final Magnetic Moment0.011 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom0.139 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.205 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density10.44 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTh2Fe7 + Th7Fe3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [166] |
Hall-R 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Topological ClassificationTI*
|
SubclassificationSEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 160.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 366.9 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 137.6 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 298.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 206.4 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 257.9 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 344.0 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 160.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 206.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 206.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 366.9 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 91.7 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 275.2 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 298.1 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 206.4 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 275.2 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 275.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 68.8 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 91.7 |
BN (mp-984) | <0 0 1> | <1 0 1> | 131.0 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 275.2 |
Al (mp-134) | <1 1 1> | <0 0 1> | 206.4 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 137.6 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 275.2 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 298.1 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 275.2 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 68.8 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 160.5 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 22.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 275.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 183.4 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 321.0 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 257.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 22.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 321.0 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 252.2 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 160.5 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 366.9 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 91.7 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 275.2 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 206.4 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 206.4 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 68.8 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 206.4 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 344.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 114.7 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 275.2 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 68.8 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 275.2 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 321.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YbAl2Cu (mp-977428) | 0.2168 | 0.000 | 3 |
GdMg2Ni9 (mp-567249) | 0.2788 | 0.451 | 3 |
SmMg2Ni9 (mp-569494) | 0.2895 | 0.000 | 3 |
CaMg2Ni9 (mp-12695) | 0.2573 | 0.013 | 3 |
Ca3Al7Ag2 (mp-11430) | 0.2312 | 0.000 | 3 |
HoCo3 (mp-1095334) | 0.1152 | 0.028 | 2 |
HoFe3 (mp-30634) | 0.1136 | 0.000 | 2 |
YbNi3 (mp-1095559) | 0.1054 | 0.000 | 2 |
YbCo3 (mp-1095601) | 0.0914 | 0.000 | 2 |
ThFe3 (mp-30638) | 0.0285 | 0.205 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Th Fe_pv |
Final Energy/Atom-8.0668 eV |
Corrected Energy-96.8014 eV
-96.8014 eV = -96.8014 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)