material

ZrGa3

ID:

mp-30685

DOI:

10.17188/1205054


Tags: Gallium zirconium (3/1)

Material Details

Final Magnetic Moment
0.003 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.481 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.008 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.06 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
ZrGa3
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4/mmm [139]
Hall
-I 4 2
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 104043 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ag (mp-124) <1 0 0> <0 0 1> 0.000 138.5
Ni (mp-23) <1 0 0> <0 0 1> 0.000 61.6
YAlO3 (mp-3792) <0 1 1> <1 0 0> 0.002 144.1
Al2O3 (mp-1143) <0 0 1> <1 1 1> 0.004 159.6
SiC (mp-8062) <1 0 0> <0 0 1> 0.006 76.9
CdSe (mp-2691) <1 0 0> <0 0 1> 0.008 76.9
CsI (mp-614603) <1 0 0> <0 0 1> 0.009 61.6
Au (mp-81) <1 0 0> <0 0 1> 0.019 138.5
GaSb (mp-1156) <1 0 0> <0 0 1> 0.021 76.9
GaN (mp-804) <1 1 0> <1 1 0> 0.022 203.7
ZnTe (mp-2176) <1 0 0> <0 0 1> 0.023 76.9
InAs (mp-20305) <1 0 0> <0 0 1> 0.033 76.9
NdGaO3 (mp-3196) <1 1 0> <0 0 1> 0.033 61.6
C (mp-48) <1 1 0> <1 0 1> 0.033 235.0
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.036 138.5
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.038 30.8
PbSe (mp-2201) <1 0 0> <0 0 1> 0.044 76.9
Mg (mp-153) <1 1 0> <1 1 0> 0.046 203.7
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.054 200.0
C (mp-66) <1 1 0> <1 0 1> 0.058 235.0
TiO2 (mp-2657) <1 1 1> <1 1 0> 0.071 203.7
MgO (mp-1265) <1 1 1> <1 0 0> 0.076 252.1
GdScO3 (mp-5690) <0 1 1> <1 0 1> 0.080 274.2
WS2 (mp-224) <0 0 1> <0 0 1> 0.081 169.3
GdScO3 (mp-5690) <0 0 1> <1 1 0> 0.082 254.7
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.082 169.3
BN (mp-984) <1 0 1> <0 0 1> 0.087 200.0
YAlO3 (mp-3792) <1 1 0> <0 0 1> 0.089 277.0
CaF2 (mp-2741) <1 0 0> <0 0 1> 0.092 30.8
SrTiO3 (mp-4651) <1 1 0> <0 0 1> 0.099 61.6
CdS (mp-672) <1 0 1> <1 0 0> 0.109 324.2
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.110 138.5
CdS (mp-672) <1 0 0> <1 1 0> 0.118 203.7
TeO2 (mp-2125) <0 0 1> <1 1 0> 0.127 254.7
TeO2 (mp-2125) <0 1 0> <1 1 0> 0.145 203.7
Bi2Se3 (mp-541837) <0 0 1> <1 0 1> 0.152 274.2
SiC (mp-11714) <1 0 1> <1 0 0> 0.152 288.1
GaP (mp-2490) <1 0 0> <0 0 1> 0.158 30.8
CaCO3 (mp-3953) <0 0 1> <1 0 1> 0.158 352.5
Mg (mp-153) <0 0 1> <0 0 1> 0.158 169.3
LiGaO2 (mp-5854) <1 0 1> <1 0 0> 0.163 180.1
CdWO4 (mp-19387) <1 0 0> <1 0 0> 0.164 216.1
C (mp-66) <1 1 1> <1 0 1> 0.165 352.5
TePb (mp-19717) <1 1 0> <1 0 0> 0.171 180.1
GaP (mp-2490) <1 1 1> <1 0 1> 0.172 156.7
TiO2 (mp-2657) <1 0 1> <1 1 0> 0.177 50.9
CdS (mp-672) <0 0 1> <1 0 1> 0.178 274.2
TbScO3 (mp-31119) <0 1 1> <1 0 1> 0.190 274.2
Mg (mp-153) <1 1 1> <1 0 0> 0.190 180.1
SiO2 (mp-6930) <0 0 1> <1 0 1> 0.193 352.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
172 87 45 0 0 0
87 172 45 0 0 0
45 45 179 0 0 0
0 0 0 74 0 0
0 0 0 0 74 0
0 0 0 0 0 114
Compliance Tensor Sij (10-12Pa-1)
8 -3.8 -1.1 0 0 0
-3.8 8 -1.1 0 0 0
-1.1 -1.1 6.1 0 0 0
0 0 0 13.5 0 0
0 0 0 0 13.5 0
0 0 0 0 0 8.8
Shear Modulus GV
76 GPa
Bulk Modulus KV
97 GPa
Shear Modulus GR
68 GPa
Bulk Modulus KR
97 GPa
Shear Modulus GVRH
72 GPa
Bulk Modulus KVRH
97 GPa
Elastic Anisotropy
0.53
Poisson's Ratio
0.20

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Pa3W (mp-982597) 0.0171 0.302 2
ScBi3 (mp-973175) 0.0128 0.170 2
TmBi3 (mp-971906) 0.0429 0.119 2
HfGa3 (mp-11387) 0.0383 0.000 2
ZrSn3 (mp-1094312) 0.0214 0.184 2
Ba (mp-1058581) 0.6679 0.019 1
Cs (mp-1012110) 0.6399 0.046 1
Ga (mp-140) 0.3731 0.029 1
Sb (mp-10631) 0.6598 0.302 1
In (mp-1055994) 0.7129 0.030 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Zr_sv Ga_d
Final Energy/Atom
-4.8892 eV
Corrected Energy
-19.5566 eV
-19.5566 eV = -19.5566 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 104043
Submitted by
User remarks:
  • Gallium zirconium (3/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)