@article{Moriarty1965, author = "Moriarty, J.L.jr. and Gordon, R.O. and Humphreys, J.E.", title = "Some new intermetallic compounds of holmium and erbium with Ag, Au, Pt, Al, In, Tl, and Ge", journal = "Acta Crystallographica (1,1948-23,1967)", year = "1965", volume = "19", pages = "285-286", ASTM_id = "ACCRA9" }