@article{Donkersloot1976, author = "Donkersloot, H.C. and van Vucht, J.H.N.", title = "The crystal structure of Ir Li, Ir3 Li and Li Rh3", journal = "Journal of the Less-Common Metals", year = "1976", volume = "50", pages = "279-282", ASTM_id = "JCOMAH" }