Final Magnetic Moment1.309 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.063 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.002 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.43 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLaMg12 + LaMg3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 1> | <1 0 1> | 140.5 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 278.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 278.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 278.8 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 278.8 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 278.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 210.8 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 210.8 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 105.4 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 278.8 |
Ag (mp-124) | <1 1 1> | <1 1 0> | 182.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 278.8 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 92.9 |
Al (mp-134) | <1 1 0> | <1 0 0> | 210.8 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 278.8 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 92.9 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 1> | 140.5 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 185.9 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 105.4 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 278.8 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 92.9 |
LaF3 (mp-905) | <1 0 1> | <1 0 1> | 140.5 |
Au (mp-81) | <1 1 1> | <0 0 1> | 92.9 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 278.8 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 278.8 |
ZrO2 (mp-2858) | <1 0 0> | <0 0 1> | 278.8 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 278.8 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 278.8 |
CdWO4 (mp-19387) | <0 0 1> | <1 1 0> | 182.6 |
ZnO (mp-2133) | <1 0 0> | <0 0 1> | 278.8 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 278.8 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 278.8 |
Ge(Bi3O5)4 (mp-23352) | <1 0 0> | <1 0 0> | 105.4 |
Fe2O3 (mp-24972) | <1 0 0> | <1 0 1> | 140.5 |
YAlO3 (mp-3792) | <0 0 1> | <0 0 1> | 278.8 |
YAlO3 (mp-3792) | <0 1 1> | <0 0 1> | 92.9 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 278.8 |
Cu (mp-30) | <1 0 0> | <1 0 0> | 105.4 |
Cu (mp-30) | <1 1 1> | <1 1 0> | 182.6 |
LiAlO2 (mp-3427) | <0 0 1> | <0 0 1> | 278.8 |
Fe2O3 (mp-24972) | <0 0 1> | <0 0 1> | 92.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Y(Al5Fe)2 (mp-16744) | 0.7351 | 0.000 | 3 |
Ce(Al5Ru)2 (mp-31364) | 0.6724 | 0.000 | 3 |
U(Al5Fe)2 (mp-20548) | 0.7151 | 0.000 | 3 |
Th(Al5Fe)2 (mp-568030) | 0.6827 | 0.000 | 3 |
Ce2(Al5Ru)3 (mp-567554) | 0.6983 | 0.000 | 3 |
Ce2Zn17 (mp-978252) | 0.1637 | 0.010 | 2 |
Tb2Zn17 (mp-30880) | 0.1178 | 0.002 | 2 |
Dy2Zn17 (mp-570071) | 0.1033 | 0.002 | 2 |
U2Zn17 (mp-569518) | 0.1035 | 0.002 | 2 |
Sr2Mg17 (mp-1116) | 0.1904 | 0.005 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: La Mg_pv |
Final Energy/Atom-2.0115 eV |
Corrected Energy-76.4368 eV
-76.4368 eV = -76.4368 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)