material

Li7Sn2

ID:

mp-30767

DOI:

10.17188/1205127


Tags: Lithium stannide (7/2) Lithium tin (7/2)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.378 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
2.97 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Cmmm [65]
Hall
-C 2 2
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 104784 from Topological Materials Database
Topological Classification
TI*
Subclassification
NLC
* Topological insulator
No Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
BaTiO3 (mp-5986) <1 0 1> <1 0 0> 0.002 325.8
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.015 130.3
MgF2 (mp-1249) <1 0 1> <1 1 0> 0.017 79.9
TbScO3 (mp-31119) <0 1 1> <0 1 0> 0.023 323.2
C (mp-48) <0 0 1> <0 1 0> 0.029 230.8
ZrO2 (mp-2858) <1 1 0> <0 1 0> 0.030 323.2
DyScO3 (mp-31120) <0 1 1> <0 1 0> 0.034 323.2
AlN (mp-661) <1 0 1> <1 1 0> 0.036 159.7
C (mp-48) <1 0 0> <0 1 0> 0.038 230.8
NaCl (mp-22862) <1 1 0> <0 0 1> 0.041 135.6
Au (mp-81) <1 0 0> <1 0 0> 0.063 260.7
SiC (mp-11714) <1 0 1> <0 1 0> 0.064 323.2
NdGaO3 (mp-3196) <0 1 1> <1 0 0> 0.066 260.7
NdGaO3 (mp-3196) <1 0 1> <1 1 0> 0.066 159.7
Ni (mp-23) <1 0 0> <1 0 0> 0.066 195.5
BN (mp-984) <0 0 1> <0 1 0> 0.069 323.2
TiO2 (mp-390) <1 0 0> <0 1 0> 0.069 184.7
GaSe (mp-1943) <0 0 1> <0 1 0> 0.071 323.2
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.072 195.5
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.072 65.2
Ag (mp-124) <1 0 0> <1 0 0> 0.073 260.7
LiTaO3 (mp-3666) <0 0 1> <1 0 0> 0.073 325.8
TiO2 (mp-2657) <1 0 1> <1 0 0> 0.074 130.3
LaF3 (mp-905) <1 0 0> <1 0 0> 0.075 325.8
CdTe (mp-406) <1 0 0> <1 0 0> 0.079 130.3
Mg (mp-153) <0 0 1> <1 0 0> 0.079 130.3
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.084 325.8
InSb (mp-20012) <1 0 0> <1 0 0> 0.084 130.3
Ni (mp-23) <1 1 0> <0 1 0> 0.085 138.5
TePb (mp-19717) <1 0 0> <1 0 0> 0.086 130.3
Fe2O3 (mp-24972) <0 0 1> <1 0 0> 0.088 325.8
PbSe (mp-2201) <1 0 0> <1 0 0> 0.090 195.5
Ga2O3 (mp-886) <1 0 0> <0 1 0> 0.090 230.8
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.091 65.2
C (mp-48) <1 0 1> <0 1 0> 0.091 323.2
CdTe (mp-406) <1 1 0> <0 1 0> 0.094 184.7
InSb (mp-20012) <1 1 0> <0 1 0> 0.098 184.7
LiGaO2 (mp-5854) <0 1 0> <0 1 0> 0.100 323.2
TiO2 (mp-2657) <1 1 1> <0 1 0> 0.102 230.8
TePb (mp-19717) <1 1 0> <0 1 0> 0.102 184.7
GaSb (mp-1156) <1 0 0> <1 0 0> 0.104 195.5
LiF (mp-1138) <1 1 0> <1 1 0> 0.109 239.6
CdS (mp-672) <1 0 0> <0 1 0> 0.110 323.2
LiNbO3 (mp-3731) <0 0 1> <1 0 0> 0.112 325.8
TiO2 (mp-2657) <1 0 0> <0 1 0> 0.114 138.5
CdSe (mp-2691) <1 0 0> <1 0 0> 0.116 195.5
GaN (mp-804) <1 0 1> <0 1 0> 0.118 230.8
GaN (mp-804) <1 0 0> <1 1 0> 0.123 239.6
BN (mp-984) <1 0 0> <0 1 0> 0.126 230.8
BaTiO3 (mp-5986) <1 0 0> <0 1 0> 0.127 184.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
53 19 14 0 0 0
19 65 -6 0 0 0
14 -6 78 0 0 0
0 0 0 11 0 0
0 0 0 0 32 0
0 0 0 0 0 38
Compliance Tensor Sij (10-12Pa-1)
23 -7.3 -4.8 0 0 0
-7.3 17.9 2.8 0 0 0
-4.8 2.8 14 0 0 0
0 0 0 88.3 0 0
0 0 0 0 31.2 0
0 0 0 0 0 26.5
Shear Modulus GV
27 GPa
Bulk Modulus KV
28 GPa
Shear Modulus GR
22 GPa
Bulk Modulus KR
28 GPa
Shear Modulus GVRH
25 GPa
Bulk Modulus KVRH
28 GPa
Elastic Anisotropy
1.35
Poisson's Ratio
0.16

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Li3(RuO3)2 (mp-675354) 0.7120 0.368 3
Na2TbO3 (mp-686281) 0.6083 0.279 3
Li17(MnAs2)4 (mp-673685) 0.7163 0.059 3
RbMg6Mo (mp-1100163) 0.6454 0.523 3
RbMg6Ti (mp-1099315) 0.6924 0.409 3
LiMg (mp-976262) 0.6645 0.028 2
Tl7Sb2 (mp-621624) 0.6662 0.000 2
Li9Al4 (mp-568404) 0.5707 0.006 2
Zr3Pd4 (mp-12712) 0.6668 0.005 2
Li7Ge2 (mp-29630) 0.2284 0.011 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Li_sv Sn_d
Final Energy/Atom
-2.7496 eV
Corrected Energy
-49.4927 eV
-49.4927 eV = -49.4927 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 291023
  • 104784
Submitted by
User remarks:
  • Lithium stannide (7/2)