Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.125 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.85 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.890 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I42d [122]
Hall
I 4 2bw
Point Group
42m
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 22187 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
LiGaO2 (mp-5854) <0 1 1> <0 0 1> 0.009 214.8
InP (mp-20351) <1 1 0> <1 0 1> 0.011 150.9
CdWO4 (mp-19387) <1 0 1> <1 0 0> 0.012 132.9
GdScO3 (mp-5690) <1 1 0> <0 0 1> 0.012 322.2
MoS2 (mp-1434) <0 0 1> <1 1 0> 0.019 281.8
WS2 (mp-224) <0 0 1> <1 1 0> 0.020 281.8
Mg (mp-153) <0 0 1> <1 1 0> 0.020 281.8
MgO (mp-1265) <1 1 1> <0 0 1> 0.022 250.6
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.023 143.2
PbS (mp-21276) <1 0 0> <0 0 1> 0.024 35.8
Ni (mp-23) <1 0 0> <0 0 1> 0.025 322.2
TiO2 (mp-2657) <1 0 0> <0 0 1> 0.039 250.6
InP (mp-20351) <1 0 0> <0 0 1> 0.040 35.8
Mg (mp-153) <1 0 1> <1 0 0> 0.041 132.9
AlN (mp-661) <1 0 0> <1 0 0> 0.043 265.7
BaTiO3 (mp-5986) <1 0 0> <1 1 1> 0.062 100.5
TiO2 (mp-390) <0 0 1> <0 0 1> 0.071 71.6
MgO (mp-1265) <1 0 0> <0 0 1> 0.078 35.8
GaN (mp-804) <1 1 0> <1 0 0> 0.079 265.7
C (mp-48) <0 0 1> <0 0 1> 0.083 250.6
BN (mp-984) <0 0 1> <1 0 1> 0.095 301.8
TbScO3 (mp-31119) <1 1 0> <0 0 1> 0.102 322.2
PbS (mp-21276) <1 1 0> <1 0 1> 0.103 150.9
BaF2 (mp-1029) <1 1 0> <1 0 1> 0.105 226.4
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.113 281.8
AlN (mp-661) <1 1 0> <1 0 1> 0.113 301.8
CdWO4 (mp-19387) <0 0 1> <1 0 1> 0.114 150.9
Cu (mp-30) <1 0 0> <0 0 1> 0.114 322.2
Bi2Se3 (mp-541837) <1 0 0> <0 0 1> 0.118 250.6
SiC (mp-11714) <0 0 1> <0 0 1> 0.119 286.4
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.120 179.0
AlN (mp-661) <1 1 1> <1 0 0> 0.121 199.3
KCl (mp-23193) <1 0 0> <0 0 1> 0.126 322.2
SiC (mp-7631) <0 0 1> <0 0 1> 0.127 286.4
CdWO4 (mp-19387) <0 1 1> <1 1 1> 0.131 201.1
CsI (mp-614603) <1 1 0> <1 0 0> 0.143 265.7
InSb (mp-20012) <1 0 0> <0 0 1> 0.145 179.0
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.149 358.0
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.150 358.0
Fe3O4 (mp-19306) <1 0 0> <0 0 1> 0.152 71.6
CdTe (mp-406) <1 0 0> <0 0 1> 0.168 179.0
NaCl (mp-22862) <1 0 0> <0 0 1> 0.170 286.4
ZnO (mp-2133) <1 0 1> <1 0 0> 0.171 199.3
Al2O3 (mp-1143) <0 0 1> <1 1 1> 0.177 100.5
DyScO3 (mp-31120) <1 1 0> <0 0 1> 0.179 322.2
Ga2O3 (mp-886) <1 0 0> <1 0 0> 0.191 199.3
BaTiO3 (mp-5986) <1 1 0> <1 1 0> 0.196 93.9
TiO2 (mp-2657) <1 1 0> <1 0 0> 0.196 199.3
ZnO (mp-2133) <1 1 1> <0 0 1> 0.197 286.4
LiGaO2 (mp-5854) <1 0 0> <1 1 0> 0.199 281.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
92 43 47 0 0 0
43 92 47 0 0 0
47 47 79 0 0 0
0 0 0 42 0 0
0 0 0 0 42 0
0 0 0 0 0 38
Compliance Tensor Sij (10-12Pa-1)
16.6 -3.8 -7.6 0 0 0
-3.8 16.6 -7.6 0 0 0
-7.6 -7.6 21.8 0 0 0
0 0 0 24 0 0
0 0 0 0 24 0
0 0 0 0 0 26.2
Shear Modulus GV
33 GPa
Bulk Modulus KV
59 GPa
Shear Modulus GR
29 GPa
Bulk Modulus KR
59 GPa
Shear Modulus GVRH
31 GPa
Bulk Modulus KVRH
59 GPa
Elastic Anisotropy
0.65
Poisson's Ratio
0.28

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 0.11137 0.00000 0.00000
0.00000 0.00000 0.00000 0.00000 0.11137 0.00000
0.00000 0.00000 0.00000 0.00000 0.00000 -0.18113
Piezoelectric Modulus ‖eijmax
0.18113 C/m2
Crystallographic Direction vmax
0.00000
1.00000
0.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
14.04 0.00 0.00
0.00 14.04 0.00
0.00 0.00 14.14
Dielectric Tensor εij (total)
16.96 0.00 0.00
0.00 16.96 0.00
0.00 0.00 16.36
Polycrystalline dielectric constant εpoly
(electronic contribution)
14.07
Polycrystalline dielectric constant εpoly
(total)
16.76
Refractive Index n
3.75
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
AlAgSe2 (mp-14091) 0.0401 0.000 3
GaAgS2 (mp-5342) 0.0248 0.000 3
SiHgP2 (mp-1079714) 0.0740 0.042 3
MgSiAs2 (mp-1016197) 0.0361 0.000 3
FeAgSe2 (mp-1096959) 0.0724 0.285 3
Cu2SnHgS4 (mp-1025467) 0.1966 0.000 4
CdCu2SnSe4 (mp-16565) 0.1970 0.007 4
CdCu2SnS4 (mp-1078292) 0.2060 0.000 4
ZnAg2SnS4 (mp-1079889) 0.1934 0.000 4
Cu2SnHgSe4 (mp-16566) 0.1895 0.000 4
BC5 (mp-1077743) 0.2093 0.265 2
BC7 (mp-1078935) 0.2112 0.208 2
BC5 (mp-1018649) 0.2476 0.271 2
BC5 (mp-1077125) 0.2044 0.241 2
BC7 (mp-1079046) 0.1917 0.240 2
Sn (mp-949028) 0.2699 0.012 1
Si (mp-971662) 0.2702 0.062 1
C (mp-569517) 0.4077 0.145 1
C (mp-1078845) 0.3445 0.266 1
Ge (mp-1091415) 0.4032 0.008 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Cd Si As
Final Energy/Atom
-4.0362 eV
Corrected Energy
-32.2895 eV
-32.2895 eV = -32.2895 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 609980
  • 22187
  • 609979
  • 603895
Submitted by
User remarks:
  • Cadmium silicon arsenide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)