material

ZrMo3

ID:

mp-30790

DOI:

10.17188/1205152


Tags: Molybdenum zirconium (3/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
0.228 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.332 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.92 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
ZrMo2 + Mo
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pm3n [223]
Hall
-P 4n 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 105118 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
MoS2 (mp-1434) <0 0 1> <1 1 1> 0.003 140.8
WS2 (mp-224) <0 0 1> <1 1 1> 0.003 140.8
GaN (mp-804) <0 0 1> <1 1 1> 0.004 187.8
C (mp-66) <1 0 0> <1 0 0> 0.004 216.8
CaF2 (mp-2741) <1 1 0> <1 1 0> 0.005 345.0
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.005 108.4
CaF2 (mp-2741) <1 0 0> <1 0 0> 0.006 243.9
Mg (mp-153) <0 0 1> <1 1 1> 0.008 140.8
PbS (mp-21276) <1 1 1> <1 1 1> 0.008 187.8
MgO (mp-1265) <1 1 0> <1 1 0> 0.008 76.7
PbS (mp-21276) <1 1 0> <1 1 0> 0.009 153.3
LaAlO3 (mp-2920) <0 0 1> <1 1 1> 0.012 328.6
ZnO (mp-2133) <1 0 1> <1 0 0> 0.014 298.1
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.026 243.9
C (mp-48) <1 0 1> <1 0 0> 0.027 298.1
LiTaO3 (mp-3666) <1 0 0> <1 0 0> 0.031 216.8
GaP (mp-2490) <1 1 0> <1 1 0> 0.036 345.0
AlN (mp-661) <0 0 1> <1 1 1> 0.040 328.6
GaP (mp-2490) <1 0 0> <1 0 0> 0.040 243.9
KCl (mp-23193) <1 1 0> <1 1 0> 0.042 115.0
Al2O3 (mp-1143) <0 0 1> <1 1 1> 0.042 140.8
TePb (mp-19717) <1 0 0> <1 0 0> 0.042 216.8
ZrO2 (mp-2858) <0 1 0> <1 1 0> 0.044 306.6
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.064 216.8
LiNbO3 (mp-3731) <0 0 1> <1 0 0> 0.079 189.7
Mg (mp-153) <1 1 1> <1 0 0> 0.082 243.9
YAlO3 (mp-3792) <1 0 1> <1 1 0> 0.102 345.0
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.109 27.1
Mg (mp-153) <1 1 0> <1 1 0> 0.117 115.0
BaTiO3 (mp-5986) <1 0 0> <1 1 0> 0.118 153.3
NdGaO3 (mp-3196) <0 1 0> <1 1 0> 0.153 345.0
Te2Mo (mp-602) <0 0 1> <1 1 1> 0.170 140.8
LiTaO3 (mp-3666) <0 0 1> <1 0 0> 0.172 189.7
C (mp-48) <0 0 1> <1 1 0> 0.191 191.6
LaF3 (mp-905) <1 0 0> <1 0 0> 0.206 54.2
CsI (mp-614603) <1 0 0> <1 0 0> 0.211 243.9
CdTe (mp-406) <1 0 0> <1 0 0> 0.227 216.8
YAlO3 (mp-3792) <0 1 1> <1 0 0> 0.246 189.7
LaF3 (mp-905) <1 1 0> <1 1 1> 0.247 93.9
LiGaO2 (mp-5854) <1 1 0> <1 1 0> 0.255 191.6
GaN (mp-804) <1 1 0> <1 1 0> 0.266 115.0
InSb (mp-20012) <1 0 0> <1 0 0> 0.272 216.8
MgAl2O4 (mp-3536) <1 0 0> <1 0 0> 0.275 135.5
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.304 38.3
LiF (mp-1138) <1 0 0> <1 0 0> 0.311 135.5
SrTiO3 (mp-4651) <1 0 1> <1 1 1> 0.316 328.6
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.334 108.4
LiAlO2 (mp-3427) <1 0 1> <1 0 0> 0.334 216.8
CdWO4 (mp-19387) <0 1 1> <1 1 1> 0.335 328.6
Ga2O3 (mp-886) <1 0 0> <1 1 0> 0.346 268.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
337 125 125 0 0 0
125 337 125 0 0 0
125 125 337 0 0 0
0 0 0 14 0 0
0 0 0 0 14 0
0 0 0 0 0 14
Compliance Tensor Sij (10-12Pa-1)
3.7 -1 -1 0 0 0
-1 3.7 -1 0 0 0
-1 -1 3.7 0 0 0
0 0 0 69.6 0 0
0 0 0 0 69.6 0
0 0 0 0 0 69.6
Shear Modulus GV
51 GPa
Bulk Modulus KV
196 GPa
Shear Modulus GR
22 GPa
Bulk Modulus KR
196 GPa
Shear Modulus GVRH
36 GPa
Bulk Modulus KVRH
196 GPa
Elastic Anisotropy
6.61
Poisson's Ratio
0.41

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Mo3Os (mp-801) 0.0000 0.011 2
Nb3Al (mp-796) 0.0000 0.046 2
Mo3Pt (mp-1232) 0.0000 0.047 2
V3Pb (mp-30830) 0.0000 0.247 2
V3Ge (mp-1078697) 0.0000 0.000 2
Cs (mp-949029) 0.0000 0.047 1
F2 (mp-21848) 0.0000 0.000 1
Rb (mp-974620) 0.0000 0.036 1
Cr (mp-17) 0.0000 0.085 1
W (mp-11334) 0.0000 0.087 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Zr_sv Mo_pv
Final Energy/Atom
-10.0435 eV
Corrected Energy
-80.3481 eV
-80.3481 eV = -80.3481 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 105118
Submitted by
User remarks:
  • Molybdenum zirconium (3/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)