Final Magnetic Moment0.406 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.638 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density18.93 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Topological ClassificationTI*
|
SubclassificationSEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 202.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 256.5 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 144.3 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 250.0 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 283.9 |
CeO2 (mp-20194) | <1 1 0> | <1 1 1> | 287.7 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 199.5 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 162.2 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 228.0 |
BaF2 (mp-1029) | <1 0 0> | <1 1 0> | 200.0 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 199.5 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 283.9 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 250.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 85.5 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 162.2 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 250.0 |
GaAs (mp-2534) | <1 1 1> | <1 0 1> | 283.9 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 142.5 |
KCl (mp-23193) | <1 0 0> | <1 1 0> | 200.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 250.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 114.0 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 121.7 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 324.5 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 200.0 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 228.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 228.0 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 57.0 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 250.0 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 121.7 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 259.8 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 114.0 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 28.5 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 288.7 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 259.8 |
InAs (mp-20305) | <1 0 0> | <1 1 0> | 200.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 199.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 162.2 |
ZnSe (mp-1190) | <1 1 1> | <1 0 1> | 283.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 202.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 114.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 28.5 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 199.5 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 341.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 85.5 |
Te2Mo (mp-602) | <1 0 0> | <1 0 1> | 283.9 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 144.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 114.0 |
YVO4 (mp-19133) | <0 0 1> | <1 0 1> | 202.8 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 250.0 |
GaSe (mp-1943) | <1 0 0> | <1 0 1> | 202.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr8Ni50Mo15W2 (mp-767372) | 0.3712 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.2834 | 0.118 | 4 |
CrFeCoNi (mp-1096923) | 0.4221 | 0.193 | 4 |
YbTa (mp-981458) | 0.0640 | 0.691 | 2 |
USn (mp-972495) | 0.0204 | 0.114 | 2 |
NaCu (mp-976292) | 0.0358 | 0.385 | 2 |
PaPt3 (mp-862858) | 0.0544 | 0.000 | 2 |
MgCd5 (mp-1094742) | 0.0407 | 0.013 | 2 |
Cr (mp-89) | 0.1114 | 0.420 | 1 |
Er (mp-99) | 0.1962 | 0.010 | 1 |
Ce (mp-20736) | 0.0319 | 0.097 | 1 |
Ho (mp-144) | 0.1963 | 0.014 | 1 |
Tm (mp-143) | 0.1996 | 0.003 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: U Pt |
Final Energy/Atom-8.0141 eV |
Corrected Energy-64.1127 eV
-64.1127 eV = -64.1127 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)