material

ZnPt3

ID:

mp-30856

DOI:

10.17188/1205212


Tags: Platinum zinc (3/1)

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.313 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
17.72 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pm3m [221]
Hall
-P 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 105853 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.000 31.0
CdS (mp-672) <0 0 1> <1 1 1> 0.001 107.3
PbSe (mp-2201) <1 0 0> <1 0 0> 0.001 77.5
GaN (mp-804) <1 1 0> <1 1 0> 0.002 87.6
GaSb (mp-1156) <1 0 0> <1 0 0> 0.002 77.5
GaN (mp-804) <0 0 1> <1 1 1> 0.003 26.8
Au (mp-81) <1 0 0> <1 0 0> 0.003 139.4
Au (mp-81) <1 1 0> <1 1 0> 0.004 197.2
PbS (mp-21276) <1 1 1> <1 1 1> 0.012 187.9
CsI (mp-614603) <1 0 0> <1 0 0> 0.012 62.0
CsI (mp-614603) <1 1 0> <1 1 0> 0.013 87.6
CsI (mp-614603) <1 1 1> <1 1 1> 0.013 107.3
CdSe (mp-2691) <1 0 0> <1 0 0> 0.013 77.5
SrTiO3 (mp-4651) <1 0 1> <1 1 1> 0.015 53.7
SiC (mp-11714) <0 0 1> <1 1 1> 0.019 107.3
SiC (mp-7631) <0 0 1> <1 1 1> 0.024 107.3
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.024 278.9
SrTiO3 (mp-4651) <1 1 0> <1 0 0> 0.027 62.0
SrTiO3 (mp-4651) <1 0 0> <1 1 0> 0.027 43.8
Al2O3 (mp-1143) <0 0 1> <1 1 1> 0.050 80.5
Ag (mp-124) <1 0 0> <1 0 0> 0.052 139.4
TiO2 (mp-2657) <1 1 1> <1 0 0> 0.053 232.4
Ag (mp-124) <1 1 0> <1 1 0> 0.055 197.2
Ni (mp-23) <1 0 0> <1 0 0> 0.056 62.0
GaSe (mp-1943) <0 0 1> <1 1 1> 0.059 241.5
C (mp-66) <1 1 0> <1 1 0> 0.072 197.2
Bi2Se3 (mp-541837) <0 0 1> <1 1 1> 0.072 107.3
NdGaO3 (mp-3196) <1 0 0> <1 1 0> 0.085 43.8
MgF2 (mp-1249) <1 0 1> <1 1 0> 0.094 131.5
SiC (mp-8062) <1 0 0> <1 0 0> 0.101 77.5
CdWO4 (mp-19387) <1 0 0> <1 1 0> 0.116 219.1
KCl (mp-23193) <1 1 0> <1 1 0> 0.117 175.3
Mg (mp-153) <1 1 0> <1 1 0> 0.129 87.6
CdWO4 (mp-19387) <1 0 1> <1 0 0> 0.144 309.9
CdS (mp-672) <1 1 0> <1 1 0> 0.150 197.2
C (mp-48) <1 0 0> <1 1 0> 0.154 175.3
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.154 139.4
NdGaO3 (mp-3196) <1 0 1> <1 1 1> 0.159 53.7
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.169 77.5
Te2Mo (mp-602) <1 0 1> <1 0 0> 0.184 278.9
ZnO (mp-2133) <1 1 1> <1 1 0> 0.187 219.1
SiC (mp-8062) <1 1 0> <1 1 0> 0.189 241.0
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.189 62.0
CdWO4 (mp-19387) <0 1 0> <1 1 0> 0.195 131.5
InAs (mp-20305) <1 0 0> <1 0 0> 0.199 77.5
TeO2 (mp-2125) <0 1 1> <1 1 0> 0.204 153.4
GaN (mp-804) <1 0 0> <1 1 0> 0.208 153.4
TiO2 (mp-390) <1 1 0> <1 1 0> 0.219 262.9
BaTiO3 (mp-5986) <1 0 1> <1 0 0> 0.226 46.5
SiC (mp-11714) <1 0 0> <1 1 0> 0.226 284.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
274 183 183 0 0 0
183 274 183 0 0 0
183 183 274 0 0 0
0 0 0 90 0 0
0 0 0 0 90 0
0 0 0 0 0 90
Compliance Tensor Sij (10-12Pa-1)
7.9 -3.2 -3.2 0 0 0
-3.2 7.9 -3.2 0 0 0
-3.2 -3.2 7.9 0 0 0
0 0 0 11.1 0 0
0 0 0 0 11.1 0
0 0 0 0 0 11.1
Shear Modulus GV
72 GPa
Bulk Modulus KV
213 GPa
Shear Modulus GR
64 GPa
Bulk Modulus KR
213 GPa
Shear Modulus GVRH
68 GPa
Bulk Modulus KVRH
213 GPa
Elastic Anisotropy
0.60
Poisson's Ratio
0.36

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ZnCu2Ni (mp-30593) 0.1125 0.005 3
CrCoPt2 (mp-570863) 0.0492 0.000 3
LiCa6Ge (mp-12609) 0.0000 0.180 3
GaFeNi2 (mp-1065359) 0.0412 0.066 3
GaCo2Ni (mp-1018060) 0.0157 0.075 3
Cr8Ni50Mo15W2 (mp-767372) 0.2155 0.028 4
CrFeCoNi (mp-1012640) 0.3608 0.118 4
CrFeCoNi (mp-1096923) 0.4019 0.193 4
GdIn3 (mp-991709) 0.0000 0.000 2
CePb3 (mp-20225) 0.0000 0.000 2
CaPb3 (mp-20549) 0.0000 0.000 2
HfPt3 (mp-1018054) 0.0000 0.005 2
FeH3 (mp-1064077) 0.0000 0.194 2
Na (mp-974558) 0.0000 0.001 1
Br (mp-998870) 0.0000 0.666 1
Mn (mp-8634) 0.0000 0.083 1
Pb (mp-20483) 0.0000 0.000 1
Cu (mp-30) 0.0000 0.000 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Zn Pt
Final Energy/Atom
-5.1808 eV
Corrected Energy
-20.7232 eV
-20.7232 eV = -20.7232 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 105853
Submitted by
User remarks:
  • Platinum zinc (3/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)