material

YZn3

ID:

mp-30884

DOI:

10.17188/1205237


Tags: Yttrium zinc (1/3)

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.372 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.35 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pnma [62]
Hall
-P 2ac 2n
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SiC (mp-11714) <1 1 0> <1 1 0> 0.004 162.4
MgO (mp-1265) <1 0 0> <1 0 0> 0.004 271.8
TeO2 (mp-2125) <1 1 0> <0 0 1> 0.006 294.8
C (mp-66) <1 0 0> <1 0 0> 0.007 203.8
SiO2 (mp-6930) <1 0 0> <1 0 1> 0.009 222.2
Ga2O3 (mp-886) <0 1 0> <0 1 1> 0.013 213.4
CdWO4 (mp-19387) <0 0 1> <1 1 0> 0.025 243.6
TiO2 (mp-390) <1 1 1> <1 1 0> 0.026 162.4
TeO2 (mp-2125) <0 0 1> <1 1 1> 0.032 259.2
CdS (mp-672) <1 1 1> <1 1 1> 0.049 259.2
Cu (mp-30) <1 1 1> <0 0 1> 0.057 294.8
ZnO (mp-2133) <1 0 1> <0 1 1> 0.057 160.0
WSe2 (mp-1821) <1 0 1> <1 0 0> 0.061 203.8
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.062 88.5
InSb (mp-20012) <1 0 0> <0 0 1> 0.066 88.5
TiO2 (mp-2657) <1 1 1> <0 1 1> 0.066 320.1
LiGaO2 (mp-5854) <0 0 1> <1 0 1> 0.067 222.2
AlN (mp-661) <1 0 0> <0 1 0> 0.070 222.3
CdTe (mp-406) <1 0 0> <0 0 1> 0.070 88.5
InP (mp-20351) <1 0 0> <0 0 1> 0.073 176.9
TiO2 (mp-2657) <1 0 1> <1 1 1> 0.074 259.2
ZrO2 (mp-2858) <0 1 1> <0 1 0> 0.076 311.2
BN (mp-984) <0 0 1> <0 0 1> 0.076 88.5
BaF2 (mp-1029) <1 0 0> <0 0 1> 0.080 117.9
GaSe (mp-1943) <0 0 1> <1 0 0> 0.093 203.8
SiO2 (mp-6930) <1 1 1> <0 1 0> 0.100 266.7
NdGaO3 (mp-3196) <1 0 1> <0 0 1> 0.100 324.3
CdWO4 (mp-19387) <1 0 1> <0 1 1> 0.103 266.7
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.104 294.8
GaSe (mp-1943) <1 1 0> <0 0 1> 0.114 117.9
ZnO (mp-2133) <1 1 1> <0 0 1> 0.123 353.8
BaTiO3 (mp-5986) <1 0 0> <0 1 0> 0.123 222.3
SiC (mp-11714) <1 1 1> <1 1 0> 0.125 162.4
WSe2 (mp-1821) <1 0 0> <1 0 0> 0.126 203.8
PbSe (mp-2201) <1 0 0> <0 0 1> 0.126 117.9
Al2O3 (mp-1143) <1 0 0> <0 1 1> 0.128 320.1
Au (mp-81) <1 1 0> <0 1 0> 0.133 222.3
SiC (mp-11714) <1 0 0> <0 1 0> 0.137 222.3
LiF (mp-1138) <1 1 0> <0 1 1> 0.138 213.4
SrTiO3 (mp-4651) <1 0 1> <0 0 1> 0.151 324.3
GaSb (mp-1156) <1 0 0> <0 0 1> 0.157 117.9
GdScO3 (mp-5690) <0 1 1> <1 0 1> 0.166 222.2
MoSe2 (mp-1634) <1 0 0> <1 0 0> 0.166 203.8
BN (mp-984) <1 1 0> <0 1 0> 0.167 133.4
GaN (mp-804) <1 0 1> <0 1 1> 0.171 213.4
GdScO3 (mp-5690) <0 0 1> <0 0 1> 0.176 324.3
CdS (mp-672) <1 1 0> <0 0 1> 0.178 147.4
BaTiO3 (mp-5986) <1 0 1> <0 1 1> 0.180 213.4
BaTiO3 (mp-5986) <1 1 0> <0 0 1> 0.185 265.4
CdSe (mp-2691) <1 0 0> <0 0 1> 0.186 117.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
97 56 52 0 0 0
56 121 41 0 0 0
52 41 129 0 0 0
0 0 0 38 0 0
0 0 0 0 52 0
0 0 0 0 0 41
Compliance Tensor Sij (10-12Pa-1)
16.4 -6.1 -4.7 0 0 0
-6.1 11.5 -1.2 0 0 0
-4.7 -1.2 10 0 0 0
0 0 0 26.5 0 0
0 0 0 0 19.1 0
0 0 0 0 0 24.5
Shear Modulus GV
39 GPa
Bulk Modulus KV
72 GPa
Shear Modulus GR
37 GPa
Bulk Modulus KR
71 GPa
Shear Modulus GVRH
38 GPa
Bulk Modulus KVRH
71 GPa
Elastic Anisotropy
0.38
Poisson's Ratio
0.27

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
SmGePt (mp-20293) 0.5008 0.013 3
SrLiBi (mp-30456) 0.5069 0.000 3
LiEuSb (mp-1095425) 0.4762 0.000 3
LiEuBi (mp-1095380) 0.4873 0.000 3
DyZn3 (mp-30626) 0.0917 0.000 2
HoZn3 (mp-30736) 0.0730 0.000 2
SrHg2 (mp-568526) 0.4958 0.008 2
Mg3Si4 (mp-1075131) 0.4866 0.242 2
TmCu2 (mp-1077209) 0.4900 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Y_sv Zn
Final Energy/Atom
-2.9331 eV
Corrected Energy
-46.9291 eV
-46.9291 eV = -46.9291 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 106227
Submitted by
User remarks:
  • Yttrium zinc (1/3)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)