material

YZn5

ID:

mp-30885

DOI:

10.17188/1205238


Tags: Yttrium zinc (1/5)

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.296 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.008 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.67 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Y3Zn11 + Y2Zn17
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P6/mmm [191]
Hall
-P 6 2
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 106228 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
ZnSe (mp-1190) <1 1 1> <0 0 1> 0.000 171.3
Cu (mp-30) <1 1 1> <0 0 1> 0.004 293.7
GaAs (mp-2534) <1 1 1> <0 0 1> 0.004 171.3
PbS (mp-21276) <1 1 1> <1 1 0> 0.013 311.5
PbS (mp-21276) <1 0 0> <1 0 0> 0.013 179.8
BaTiO3 (mp-5986) <1 0 0> <1 0 0> 0.013 67.4
MoSe2 (mp-1634) <1 0 1> <1 0 0> 0.015 157.3
PbSe (mp-2201) <1 0 0> <1 0 1> 0.015 232.6
GaSb (mp-1156) <1 0 0> <1 0 1> 0.019 232.6
GaN (mp-804) <0 0 1> <0 0 1> 0.021 171.3
CdSe (mp-2691) <1 0 0> <1 0 1> 0.026 232.6
Ge (mp-32) <1 1 1> <0 0 1> 0.027 171.3
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.035 97.9
MgO (mp-1265) <1 0 0> <1 0 0> 0.042 89.9
BN (mp-984) <1 0 1> <1 0 1> 0.044 99.7
Te2W (mp-22693) <1 0 1> <1 0 0> 0.046 202.3
Fe2O3 (mp-24972) <1 1 0> <1 0 0> 0.048 247.2
AlN (mp-661) <1 0 0> <1 0 0> 0.051 157.3
BN (mp-984) <0 0 1> <0 0 1> 0.058 171.3
BN (mp-984) <1 0 0> <1 1 1> 0.060 229.9
NdGaO3 (mp-3196) <1 1 1> <1 1 0> 0.062 272.5
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.070 293.7
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.071 220.3
SiC (mp-8062) <1 0 0> <1 0 1> 0.075 232.6
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.078 171.3
SiC (mp-11714) <1 0 1> <1 1 0> 0.081 194.7
MgF2 (mp-1249) <1 1 0> <1 0 1> 0.083 166.1
KP(HO2)2 (mp-23959) <0 0 1> <1 0 0> 0.090 224.8
ZnO (mp-2133) <1 1 0> <1 0 0> 0.090 89.9
InP (mp-20351) <1 0 0> <1 0 0> 0.094 179.8
TiO2 (mp-390) <1 1 1> <0 0 1> 0.096 269.2
TiO2 (mp-2657) <1 0 0> <1 1 1> 0.097 138.0
Mg (mp-153) <1 0 0> <1 0 0> 0.100 67.4
ZnTe (mp-2176) <1 0 0> <1 0 1> 0.110 232.6
GaSe (mp-1943) <0 0 1> <1 0 0> 0.110 112.4
C (mp-48) <1 1 1> <1 0 0> 0.114 67.4
SrTiO3 (mp-4651) <1 0 1> <0 0 1> 0.121 318.2
InAs (mp-20305) <1 0 0> <1 0 1> 0.125 232.6
ZnO (mp-2133) <0 0 1> <1 0 0> 0.130 247.2
SiC (mp-11714) <0 0 1> <0 0 1> 0.132 24.5
KTaO3 (mp-3614) <1 0 0> <1 1 1> 0.133 275.9
YAlO3 (mp-3792) <1 0 1> <0 0 1> 0.133 48.9
NdGaO3 (mp-3196) <1 0 1> <0 0 1> 0.137 318.2
Ni (mp-23) <1 0 0> <1 1 0> 0.138 194.7
DyScO3 (mp-31120) <1 0 0> <0 0 1> 0.140 318.2
Ga2O3 (mp-886) <1 0 -1> <1 0 1> 0.141 265.8
SiC (mp-7631) <0 0 1> <0 0 1> 0.142 24.5
TePb (mp-19717) <1 1 1> <0 0 1> 0.147 73.4
NaCl (mp-22862) <1 1 1> <0 0 1> 0.152 171.3
Al (mp-134) <1 0 0> <1 1 1> 0.152 275.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
132 53 44 0 0 0
53 132 44 0 0 0
44 44 162 0 0 0
0 0 0 55 0 0
0 0 0 0 55 0
0 0 0 0 0 40
Compliance Tensor Sij (10-12Pa-1)
9.4 -3.2 -1.7 0 0 0
-3.2 9.4 -1.7 0 0 0
-1.7 -1.7 7.1 0 0 0
0 0 0 18.1 0 0
0 0 0 0 18.1 0
0 0 0 0 0 25.3
Shear Modulus GV
49 GPa
Bulk Modulus KV
79 GPa
Shear Modulus GR
48 GPa
Bulk Modulus KR
79 GPa
Shear Modulus GVRH
48 GPa
Bulk Modulus KVRH
79 GPa
Elastic Anisotropy
0.14
Poisson's Ratio
0.25

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
UAl3Ni2 (mp-2903) 0.0884 0.108 3
CeGa3Pd2 (mp-3494) 0.0319 0.000 3
UAl3Pd2 (mp-4561) 0.0576 0.080 3
UGa3Pd2 (mp-20899) 0.0615 0.041 3
LaGa3Pd2 (mp-21201) 0.0473 0.000 3
CeZn5 (mp-394) 0.0030 0.014 2
SmZn5 (mp-567406) 0.0094 0.003 2
LaCu5 (mp-2613) 0.0000 0.000 2
NdNi5 (mp-991142) 0.0104 0.000 2
PrNi5 (mp-2370) 0.0114 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Y_sv Zn
Final Energy/Atom
-2.4232 eV
Corrected Energy
-14.5393 eV
Uncorrected energy = -14.5393 eV Corrected energy = -14.5393 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 106228
Submitted by
User remarks:
  • Yttrium zinc (1/5)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)