Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.437 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.85 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.433 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 232.0 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 227.7 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 227.7 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 151.8 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 232.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 227.7 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 303.6 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 303.6 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 227.7 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 227.7 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 303.6 |
SiC (mp-7631) | <1 0 0> | <1 0 -1> | 145.2 |
TiO2 (mp-2657) | <1 0 0> | <1 0 1> | 165.4 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 151.8 |
NdGaO3 (mp-3196) | <0 1 1> | <1 0 0> | 151.8 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 227.7 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 303.6 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 227.7 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 227.7 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 227.7 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 227.7 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 227.7 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 135.8 |
BN (mp-984) | <1 0 1> | <1 0 0> | 303.6 |
Al (mp-134) | <1 0 0> | <1 0 0> | 227.7 |
Al (mp-134) | <1 1 0> | <1 0 0> | 227.7 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 303.6 |
Ga2O3 (mp-886) | <1 0 1> | <0 1 0> | 232.0 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 0> | 303.6 |
WS2 (mp-224) | <1 0 0> | <0 0 1> | 135.8 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 227.7 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 0> | 227.7 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 0> | 227.7 |
C (mp-48) | <1 0 0> | <0 0 1> | 135.8 |
C (mp-48) | <1 0 1> | <1 0 0> | 303.6 |
C (mp-48) | <1 1 1> | <1 0 0> | 227.7 |
NaCl (mp-22862) | <1 0 0> | <0 1 0> | 232.0 |
NaCl (mp-22862) | <1 1 0> | <1 0 0> | 227.7 |
NaCl (mp-22862) | <1 1 1> | <1 0 0> | 227.7 |
LaF3 (mp-905) | <0 0 1> | <1 0 0> | 303.6 |
ZrO2 (mp-2858) | <0 1 0> | <1 0 0> | 303.6 |
ZrO2 (mp-2858) | <1 0 1> | <1 0 0> | 303.6 |
ZrO2 (mp-2858) | <1 1 -1> | <0 1 1> | 178.6 |
TbScO3 (mp-31119) | <0 1 0> | <1 0 0> | 227.7 |
TbScO3 (mp-31119) | <1 0 0> | <1 0 0> | 227.7 |
InSb (mp-20012) | <1 1 0> | <1 0 0> | 303.6 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 227.7 |
YAlO3 (mp-3792) | <0 1 1> | <1 0 -1> | 145.2 |
YAlO3 (mp-3792) | <1 0 1> | <1 0 0> | 151.8 |
SiC (mp-8062) | <1 1 1> | <1 0 0> | 303.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Al2CuCl8 (mp-23434) | 0.4469 | 0.000 | 3 |
Al2PdCl8 (mp-27452) | 0.1976 | 0.000 | 3 |
Ga2CuCl8 (mp-29300) | 0.4236 | 0.000 | 3 |
Al(SeCl)4 (mp-683984) | 0.7263 | 0.000 | 3 |
Ga2PdBr8 (mp-30945) | 0.1975 | 0.000 | 3 |
KP2AuS7 (mp-976587) | 0.5890 | 0.007 | 4 |
Cs4P2PdSe8 (mp-866688) | 0.6477 | 0.000 | 4 |
Cs6Si2NiO8 (mp-628279) | 0.6153 | 0.018 | 4 |
Ba4Mg(SiN3)2 (mp-1019517) | 0.7472 | 0.000 | 4 |
Cs4K2Cu(SiO4)2 (mp-628617) | 0.7053 | 0.000 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ga_d Pd I |
Final Energy/Atom-2.5668 eV |
Corrected Energy-31.2672 eV
Uncorrected energy = -28.2352 eV
Composition-based energy adjustment (-0.379 eV/atom x 8.0 atoms) = -3.0320 eV
Corrected energy = -31.2672 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)