Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-4.150 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.89 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap5.456 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 0> | 295.9 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 295.9 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 221.9 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 295.9 |
GaN (mp-804) | <0 0 1> | <1 1 -1> | 241.8 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 174.2 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 295.9 |
SiO2 (mp-6930) | <1 0 1> | <1 0 -1> | 287.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 295.9 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 230.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 307.4 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 295.9 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 230.5 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 295.9 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 221.9 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 117.7 |
Te2W (mp-22693) | <0 0 1> | <1 1 -1> | 241.8 |
YVO4 (mp-19133) | <1 1 0> | <1 0 -1> | 191.3 |
Te2Mo (mp-602) | <0 0 1> | <1 1 -1> | 120.9 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 117.7 |
BN (mp-984) | <1 0 0> | <1 0 0> | 76.8 |
BN (mp-984) | <1 0 1> | <1 0 0> | 307.4 |
BN (mp-984) | <1 1 1> | <1 0 0> | 307.4 |
GaSe (mp-1943) | <0 0 1> | <1 0 -1> | 191.3 |
BN (mp-984) | <0 0 1> | <1 1 0> | 213.3 |
BN (mp-984) | <1 1 0> | <1 0 0> | 230.5 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 235.4 |
Al (mp-134) | <1 1 1> | <1 0 0> | 230.5 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 153.7 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 307.4 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 -1> | 241.8 |
CdTe (mp-406) | <1 1 0> | <1 0 -1> | 191.3 |
C (mp-66) | <1 1 0> | <1 0 -1> | 287.0 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 117.7 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 230.5 |
TbScO3 (mp-31119) | <0 1 0> | <0 1 0> | 295.9 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 0> | 230.5 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 307.4 |
Ni (mp-23) | <1 1 0> | <1 0 1> | 174.2 |
InSb (mp-20012) | <1 1 0> | <1 0 -1> | 191.3 |
BaTiO3 (mp-5986) | <0 0 1> | <0 1 0> | 221.9 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 0> | 230.5 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 307.4 |
BaTiO3 (mp-5986) | <1 0 1> | <0 1 0> | 295.9 |
NdGaO3 (mp-3196) | <0 1 0> | <0 1 0> | 295.9 |
NdGaO3 (mp-3196) | <1 0 0> | <1 0 0> | 307.4 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 307.4 |
SiC (mp-11714) | <0 0 1> | <1 0 0> | 230.5 |
SiC (mp-11714) | <1 0 0> | <1 0 0> | 153.7 |
MoSe2 (mp-1634) | <1 0 0> | <1 0 0> | 153.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BaYF5 (mp-752675) | 0.6555 | 0.000 | 3 |
CeSmI4 (mp-570470) | 0.7357 | 0.080 | 3 |
CeNdI4 (mp-570728) | 0.7264 | 0.081 | 3 |
Cu2PPd2 (mp-1001022) | 0.7134 | 0.004 | 3 |
UF4 (mp-287) | 0.1229 | 0.000 | 2 |
ThF4 (mp-31034) | 0.1067 | 0.000 | 2 |
CeF4 (mp-542001) | 0.0786 | 0.000 | 2 |
NpF4 (mp-504787) | 0.0602 | 0.000 | 2 |
NpF4 (mp-864802) | 0.3983 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Hf_pv F |
Final Energy/Atom-7.2782 eV |
Corrected Energy-218.3449 eV
-218.3449 eV = -218.3449 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)