Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-4.522 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.03 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap6.537 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 146.2 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 172.6 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 275.0 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 286.6 |
GaN (mp-804) | <1 1 0> | <1 0 -1> | 118.5 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 95.5 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 275.0 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 286.6 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 264.8 |
CeO2 (mp-20194) | <1 0 0> | <1 0 -1> | 118.5 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 286.6 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 146.2 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 286.6 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 286.6 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 286.6 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 286.6 |
Mg (mp-153) | <1 1 1> | <1 0 -1> | 118.5 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 286.6 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 286.6 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 275.0 |
PbSe (mp-2201) | <1 0 0> | <0 1 0> | 275.0 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 0> | 95.5 |
MoSe2 (mp-1634) | <0 0 1> | <0 1 0> | 183.4 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 286.6 |
TiO2 (mp-390) | <1 0 1> | <1 0 -1> | 118.5 |
Si (mp-149) | <1 0 0> | <1 0 -1> | 118.5 |
ZnO (mp-2133) | <1 0 0> | <1 0 0> | 191.1 |
ZnO (mp-2133) | <1 0 1> | <0 1 0> | 275.0 |
ZnO (mp-2133) | <1 1 0> | <1 0 -1> | 118.5 |
CdSe (mp-2691) | <1 0 0> | <0 1 0> | 275.0 |
GaSb (mp-1156) | <1 0 0> | <0 1 0> | 275.0 |
C (mp-48) | <0 0 1> | <1 0 -1> | 237.1 |
Cu (mp-30) | <1 0 0> | <1 0 -1> | 118.5 |
WSe2 (mp-1821) | <0 0 1> | <0 1 0> | 183.4 |
ZrO2 (mp-2858) | <0 1 0> | <1 0 0> | 191.1 |
ZrO2 (mp-2858) | <1 0 -1> | <1 0 0> | 286.6 |
ZrO2 (mp-2858) | <1 0 0> | <1 0 0> | 286.6 |
ZrO2 (mp-2858) | <1 1 0> | <0 1 0> | 275.0 |
YAlO3 (mp-3792) | <0 0 1> | <1 0 0> | 286.6 |
ZnTe (mp-2176) | <1 0 0> | <0 1 0> | 275.0 |
CdWO4 (mp-19387) | <0 1 0> | <1 0 -1> | 237.1 |
MgF2 (mp-1249) | <1 0 0> | <0 1 0> | 275.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BaYF5 (mp-752675) | 0.6945 | 0.000 | 3 |
CeSmI4 (mp-570470) | 0.7156 | 0.080 | 3 |
CeNdI4 (mp-570728) | 0.7037 | 0.081 | 3 |
Cu2PPd2 (mp-1001022) | 0.7124 | 0.004 | 3 |
UF4 (mp-287) | 0.1349 | 0.000 | 2 |
HfF4 (mp-31033) | 0.1067 | 0.000 | 2 |
CeF4 (mp-542001) | 0.0943 | 0.000 | 2 |
NpF4 (mp-504787) | 0.0952 | 0.000 | 2 |
NpF4 (mp-864802) | 0.4018 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Th F |
Final Energy/Atom-7.1416 eV |
Corrected Energy-214.2494 eV
-214.2494 eV = -214.2494 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)