material

Ba(AlGe)2

ID:

mp-31059

DOI:

10.17188/1205386


Tags: Barium aluminium germanide (1/2/2) - beta

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.395 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.004 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.64 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Ba(AlGe)2
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4/mmm [139]
Hall
-I 4 2
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 98515 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Fe3O4 (mp-19306) <1 0 0> <0 0 1> 0.000 72.8
KCl (mp-23193) <1 0 0> <0 0 1> 0.000 163.7
ZnO (mp-2133) <1 0 1> <0 0 1> 0.002 218.3
MgO (mp-1265) <1 1 1> <0 0 1> 0.003 345.6
MoS2 (mp-1434) <1 0 0> <0 0 1> 0.004 272.9
MgO (mp-1265) <1 0 0> <0 0 1> 0.007 18.2
TiO2 (mp-390) <0 0 1> <0 0 1> 0.009 72.8
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.010 145.5
MgF2 (mp-1249) <1 1 1> <1 1 0> 0.012 239.7
YAlO3 (mp-3792) <0 1 0> <0 0 1> 0.017 272.9
Te2W (mp-22693) <0 0 1> <1 0 1> 0.019 178.1
MgO (mp-1265) <1 1 0> <0 0 1> 0.020 127.3
C (mp-48) <0 0 1> <0 0 1> 0.021 127.3
ZnSe (mp-1190) <1 0 0> <0 0 1> 0.021 163.7
PbS (mp-21276) <1 1 0> <0 0 1> 0.024 254.7
MgF2 (mp-1249) <1 0 1> <1 0 1> 0.026 237.4
BaTiO3 (mp-5986) <1 0 0> <1 0 1> 0.031 118.7
Al (mp-134) <1 0 0> <0 0 1> 0.033 145.5
TeO2 (mp-2125) <0 0 1> <0 0 1> 0.034 291.1
PbS (mp-21276) <1 0 0> <0 0 1> 0.038 36.4
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.039 145.5
GaAs (mp-2534) <1 0 0> <0 0 1> 0.041 163.7
SiO2 (mp-6930) <1 1 1> <1 1 0> 0.042 159.8
NdGaO3 (mp-3196) <0 0 1> <0 0 1> 0.044 309.3
NaCl (mp-22862) <1 0 0> <0 0 1> 0.049 163.7
ZrO2 (mp-2858) <0 1 1> <0 0 1> 0.050 272.9
TeO2 (mp-2125) <0 1 1> <1 0 0> 0.054 226.0
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.055 109.1
BN (mp-984) <0 0 1> <0 0 1> 0.058 54.6
Al2O3 (mp-1143) <1 0 0> <1 1 0> 0.063 319.6
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.063 91.0
Mg (mp-153) <1 1 0> <1 1 0> 0.067 319.6
C (mp-48) <1 1 1> <0 0 1> 0.068 200.1
NdGaO3 (mp-3196) <0 1 0> <0 0 1> 0.070 345.6
LiGaO2 (mp-5854) <0 1 1> <0 0 1> 0.071 218.3
LaAlO3 (mp-2920) <1 0 0> <1 0 0> 0.073 282.5
ZrO2 (mp-2858) <1 1 0> <1 0 1> 0.075 118.7
YAlO3 (mp-3792) <1 0 1> <1 0 1> 0.077 296.8
LiNbO3 (mp-3731) <1 0 0> <1 0 1> 0.080 296.8
Ge (mp-32) <1 0 0> <0 0 1> 0.087 163.7
Te2W (mp-22693) <0 1 1> <0 0 1> 0.089 291.1
SiO2 (mp-6930) <1 1 0> <1 0 1> 0.090 237.4
C (mp-66) <1 0 0> <0 0 1> 0.091 163.7
Al2O3 (mp-1143) <1 1 0> <0 0 1> 0.091 109.1
Ga2O3 (mp-886) <1 1 -1> <0 0 1> 0.096 163.7
AlN (mp-661) <1 1 1> <0 0 1> 0.101 309.3
Bi2Se3 (mp-541837) <1 0 0> <0 0 1> 0.107 127.3
NdGaO3 (mp-3196) <1 0 0> <0 0 1> 0.110 345.6
InAs (mp-20305) <1 1 1> <0 0 1> 0.111 327.4
CdS (mp-672) <0 0 1> <0 0 1> 0.114 91.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
62 52 39 0 0 0
52 62 39 0 0 0
39 39 37 0 0 0
0 0 0 21 0 0
0 0 0 0 21 0
0 0 0 0 0 32
Compliance Tensor Sij (10-12Pa-1)
66.8 -34.6 -34.1 0 0 0
-34.6 66.8 -34.1 0 0 0
-34.1 -34.1 99 0 0 0
0 0 0 47 0 0
0 0 0 0 47 0
0 0 0 0 0 31.7
Shear Modulus GV
17 GPa
Bulk Modulus KV
47 GPa
Shear Modulus GR
9 GPa
Bulk Modulus KR
37 GPa
Shear Modulus GVRH
13 GPa
Bulk Modulus KVRH
42 GPa
Elastic Anisotropy
4.93
Poisson's Ratio
0.36

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Sr(CrAs)2 (mp-570031) 0.2648 0.188 3
Sr(PRh)2 (mp-8581) 0.2688 0.000 3
Ba(CuSe)2 (mp-10437) 0.2593 0.037 3
Ba(AlSi)2 (mp-12863) 0.1502 0.009 3
Ba(CuS)2 (mp-4255) 0.2748 0.015 3
KLiZnS2 (mp-774907) 0.4983 0.000 4
SrBiClO2 (mp-547244) 0.7447 0.000 4
LuBi2ClO4 (mp-550805) 0.7374 0.000 4
KLiMnS2 (mp-753940) 0.4778 0.000 4
BiPbClO2 (mp-23084) 0.5746 0.000 4
NbS2 (mp-1008860) 0.7372 0.269 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ba_sv Al Ge_d
Final Energy/Atom
-4.1236 eV
Corrected Energy
-20.6179 eV
-20.6179 eV = -20.6179 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 98515
Submitted by
User remarks:
  • Barium aluminium germanide (1/2/2) - beta

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)