material

BaZnSn

ID:

mp-31148

DOI:

10.17188/1205461


Tags: Barium tin zinc (1/1/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.532 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.47 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 106317 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
BN (mp-984) <0 0 1> <0 0 1> 0.000 136.5
LaF3 (mp-905) <0 0 1> <0 0 1> 0.000 136.5
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.001 253.6
Al (mp-134) <1 1 1> <0 0 1> 0.004 253.6
SiO2 (mp-6930) <1 0 0> <1 0 0> 0.020 332.3
KP(HO2)2 (mp-23959) <0 1 0> <1 0 1> 0.028 154.0
SiC (mp-7631) <0 0 1> <0 0 1> 0.029 58.5
SiC (mp-11714) <0 0 1> <0 0 1> 0.034 58.5
Ni (mp-23) <1 1 1> <0 0 1> 0.036 253.6
GaSe (mp-1943) <0 0 1> <1 0 0> 0.039 189.9
LiGaO2 (mp-5854) <1 0 1> <0 0 1> 0.051 312.1
LiAlO2 (mp-3427) <1 1 1> <0 0 1> 0.052 273.1
MoS2 (mp-1434) <1 0 1> <1 0 1> 0.056 205.3
LiAlO2 (mp-3427) <1 0 0> <1 1 0> 0.062 164.4
GdScO3 (mp-5690) <0 1 1> <1 1 0> 0.065 164.4
MgO (mp-1265) <1 1 0> <1 0 0> 0.065 284.8
CdWO4 (mp-19387) <1 0 1> <1 0 1> 0.071 307.9
ZrO2 (mp-2858) <1 0 0> <0 0 1> 0.075 312.1
Mg (mp-153) <0 0 1> <0 0 1> 0.076 78.0
YAlO3 (mp-3792) <0 0 1> <0 0 1> 0.082 312.1
CdWO4 (mp-19387) <1 1 0> <1 0 1> 0.085 205.3
AlN (mp-661) <1 0 1> <1 1 0> 0.085 246.6
MgF2 (mp-1249) <1 0 0> <1 0 1> 0.089 102.6
C (mp-66) <1 1 0> <1 0 0> 0.092 142.4
ZnO (mp-2133) <0 0 1> <0 0 1> 0.094 175.6
AlN (mp-661) <0 0 1> <0 0 1> 0.094 58.5
GaN (mp-804) <1 0 0> <1 1 1> 0.098 84.5
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.098 156.1
TbScO3 (mp-31119) <0 1 1> <1 1 0> 0.105 164.4
PbS (mp-21276) <1 1 1> <0 0 1> 0.115 253.6
MoS2 (mp-1434) <1 0 0> <1 0 1> 0.118 205.3
Mg (mp-153) <1 0 0> <1 1 1> 0.120 84.5
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.125 78.0
NdGaO3 (mp-3196) <0 1 1> <0 0 1> 0.126 156.1
TePb (mp-19717) <1 0 0> <1 0 1> 0.127 256.6
Ag (mp-124) <1 0 0> <0 0 1> 0.132 136.5
GaAs (mp-2534) <1 1 0> <0 0 1> 0.133 234.1
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.138 78.0
ZnSe (mp-1190) <1 1 0> <0 0 1> 0.139 234.1
WS2 (mp-224) <0 0 1> <0 0 1> 0.139 78.0
Ge (mp-32) <1 1 0> <0 0 1> 0.139 234.1
Ge (mp-32) <1 1 1> <0 0 1> 0.141 58.5
Ag (mp-124) <1 1 0> <0 0 1> 0.142 97.5
InSb (mp-20012) <1 1 0> <1 0 0> 0.145 189.9
SiO2 (mp-6930) <1 0 1> <1 0 0> 0.146 142.4
MgF2 (mp-1249) <1 1 1> <1 0 0> 0.150 237.3
CdTe (mp-406) <1 1 0> <1 0 0> 0.165 189.9
Ag (mp-124) <1 1 1> <1 0 0> 0.170 237.3
TiO2 (mp-2657) <1 1 1> <1 0 0> 0.172 237.3
Al2O3 (mp-1143) <1 0 0> <1 0 0> 0.172 189.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
79 16 20 0 0 0
16 79 20 0 0 0
20 20 48 0 0 0
0 0 0 23 0 0
0 0 0 0 23 0
0 0 0 0 0 31
Compliance Tensor Sij (10-12Pa-1)
14.3 -1.7 -5.2 0 0 0
-1.7 14.3 -5.2 0 0 0
-5.2 -5.2 25.1 0 0 0
0 0 0 43 0 0
0 0 0 0 43 0
0 0 0 0 0 32
Shear Modulus GV
26 GPa
Bulk Modulus KV
35 GPa
Shear Modulus GR
24 GPa
Bulk Modulus KR
34 GPa
Shear Modulus GVRH
25 GPa
Bulk Modulus KVRH
35 GPa
Elastic Anisotropy
0.30
Poisson's Ratio
0.21

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
SrZnSi (mp-9556) 0.0368 0.000 3
SrAsPt (mp-8456) 0.0156 0.000 3
BaCuAs (mp-9898) 0.0249 0.000 3
SrAsPd (mp-9743) 0.0369 0.000 3
KTeAu (mp-3553) 0.0224 0.000 3
NbB2 (mp-450) 0.0694 0.000 2
TiB2 (mp-1145) 0.0340 0.000 2
CaSi2 (mp-12892) 0.0575 0.078 2
EuGa2 (mp-21168) 0.0645 0.045 2
EuSi2 (mp-19862) 0.0636 0.011 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ba_sv Zn Sn_d
Final Energy/Atom
-2.9218 eV
Corrected Energy
-17.5308 eV
Uncorrected energy = -17.5308 eV Corrected energy = -17.5308 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 106317
Submitted by
User remarks:
  • Barium tin zinc (1/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)