Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.082 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.79 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.369 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaTe (mp-542812) | <0 0 1> | <1 1 0> | 308.1 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 121.0 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 121.0 |
CaF2 (mp-2741) | <1 1 0> | <1 1 0> | 136.9 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 314.6 |
SiC (mp-8062) | <1 1 0> | <1 1 0> | 102.7 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 193.6 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 314.6 |
ZnTe (mp-2176) | <1 1 0> | <1 1 0> | 102.7 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 121.0 |
CaCO3 (mp-3953) | <1 0 1> | <1 1 0> | 171.1 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 102.7 |
GdScO3 (mp-5690) | <0 0 1> | <1 1 0> | 273.8 |
KP(HO2)2 (mp-23959) | <1 0 0> | <1 0 0> | 217.8 |
Ge (mp-32) | <1 0 0> | <1 0 0> | 314.6 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 121.0 |
KP(HO2)2 (mp-23959) | <0 1 1> | <1 1 0> | 102.7 |
MgF2 (mp-1249) | <1 1 0> | <1 0 0> | 363.1 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 290.4 |
Mg (mp-153) | <1 1 0> | <1 1 0> | 273.8 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 102.7 |
CaF2 (mp-2741) | <1 1 1> | <1 1 1> | 167.7 |
SiC (mp-8062) | <1 1 1> | <1 1 1> | 125.8 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 239.6 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 217.8 |
CsI (mp-614603) | <1 1 0> | <1 1 0> | 273.8 |
NdGaO3 (mp-3196) | <0 1 1> | <1 1 0> | 273.8 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 0> | 290.4 |
WS2 (mp-224) | <1 0 1> | <1 1 0> | 239.6 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 121.0 |
SiC (mp-11714) | <1 0 0> | <1 1 0> | 273.8 |
Au (mp-81) | <1 1 0> | <1 1 0> | 102.7 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 273.8 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 314.6 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 217.8 |
BaTiO3 (mp-5986) | <1 1 0> | <1 1 1> | 251.5 |
C (mp-66) | <1 1 0> | <1 0 0> | 121.0 |
C (mp-66) | <1 1 1> | <1 0 0> | 169.4 |
CdWO4 (mp-19387) | <0 1 1> | <1 1 0> | 273.8 |
TbScO3 (mp-31119) | <0 0 1> | <1 1 0> | 273.8 |
MgF2 (mp-1249) | <1 0 1> | <1 0 0> | 217.8 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 266.2 |
CaCO3 (mp-3953) | <0 0 1> | <1 0 0> | 169.4 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 125.8 |
Fe2O3 (mp-24972) | <0 0 1> | <1 1 1> | 167.7 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 121.0 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 169.4 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 0> | 314.6 |
SrTiO3 (mp-4651) | <1 0 0> | <1 1 0> | 136.9 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 290.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
18.63 | 0.00 | 0.00 |
0.00 | 18.63 | 0.00 |
0.00 | 0.00 | 18.63 |
Dielectric Tensor εij (total) |
||
---|---|---|
40.17 | 0.00 | 0.00 |
0.00 | 40.17 | 0.00 |
0.00 | 0.00 | 40.17 |
Polycrystalline dielectric constant
εpoly∞
18.63
|
Polycrystalline dielectric constant
εpoly
40.17
|
Refractive Index n4.32 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ba2ScSbO6 (mp-20709) | 0.0000 | 2.193 | 4 |
Sr2GaSbO6 (mp-6065) | 0.0003 | 0.039 | 4 |
YbBa2SbO6 (mp-14223) | 0.0000 | 1.748 | 4 |
Ba2YSbO6 (mp-14226) | 0.0000 | 2.084 | 4 |
Cs2LiYCl6 (mp-567652) | 0.0001 | 0.000 | 4 |
Mn4N (mp-505622) | 0.0000 | 0.000 | 2 |
Sr3P2 (mp-1013552) | 0.0000 | 0.403 | 2 |
Sr3Sb2 (mp-1013583) | 0.0000 | 0.379 | 2 |
Ba3Sb2 (mp-1013582) | 0.0000 | 0.415 | 2 |
Sr3Bi2 (mp-1013587) | 0.0000 | 0.372 | 2 |
Sr3SbN (mp-7752) | 0.0000 | 0.000 | 3 |
CeRh3C (mp-22519) | 0.0000 | 0.152 | 3 |
Sc3TlC (mp-4230) | 0.0000 | 0.000 | 3 |
Co3SnC (mp-20679) | 0.0000 | 0.058 | 3 |
KMgF3 (mp-3448) | 0.0000 | 0.000 | 3 |
SrLaNbZnO6 (mp-41918) | 0.0385 | 0.126 | 5 |
BaLaMgBiO6 (mp-41414) | 0.0288 | 0.095 | 5 |
BaCaLaBiO6 (mp-39886) | 0.0711 | 0.155 | 5 |
BaLaTaZnO6 (mp-42054) | 0.0630 | 0.120 | 5 |
BaLaMgTaO6 (mp-40251) | 0.0443 | 0.080 | 5 |
Ba3LaZnReWO12 (mp-705508) | 0.6831 | 0.061 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: N Ca_sv Bi |
Final Energy/Atom-4.6657 eV |
Corrected Energy-23.3284 eV
-23.3284 eV = -23.3284 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)