material

CaGaPt

ID:

mp-31152

DOI:

10.17188/1205464


Tags: Calcium gallium platinum (1/1/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.922 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.28 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pnma [62]
Hall
-P 2ac 2n
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 106340 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Plane
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Mg (mp-153) <1 0 0> <0 1 1> 0.004 234.0
LiGaO2 (mp-5854) <0 1 1> <1 1 0> 0.007 128.9
CdS (mp-672) <1 0 0> <0 0 1> 0.011 288.7
MgO (mp-1265) <1 0 0> <0 0 1> 0.025 288.7
Ga2O3 (mp-886) <1 0 0> <0 1 0> 0.034 272.6
AlN (mp-661) <1 1 1> <0 0 1> 0.036 256.6
Te2Mo (mp-602) <1 0 1> <0 0 1> 0.040 224.5
GaSe (mp-1943) <1 0 1> <1 0 0> 0.042 273.4
CdWO4 (mp-19387) <0 1 1> <1 1 0> 0.042 322.1
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.046 256.6
KCl (mp-23193) <1 0 0> <0 1 0> 0.048 204.4
GaN (mp-804) <0 0 1> <0 0 1> 0.049 224.5
LaF3 (mp-905) <1 0 0> <0 0 1> 0.050 160.4
Bi2Te3 (mp-34202) <0 0 1> <0 1 0> 0.051 34.1
BaTiO3 (mp-5986) <1 0 1> <0 0 1> 0.055 256.6
AlN (mp-661) <1 0 1> <0 0 1> 0.060 160.4
GaSe (mp-1943) <1 0 0> <1 0 0> 0.061 273.4
CaCO3 (mp-3953) <1 0 1> <0 1 0> 0.064 272.6
GdScO3 (mp-5690) <0 1 0> <0 0 1> 0.064 352.8
LiTaO3 (mp-3666) <1 1 1> <0 0 1> 0.067 128.3
InP (mp-20351) <1 0 0> <0 0 1> 0.067 352.8
TiO2 (mp-390) <0 0 1> <0 0 1> 0.068 160.4
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.070 288.7
CeO2 (mp-20194) <1 0 0> <0 1 0> 0.071 238.5
LiGaO2 (mp-5854) <1 1 1> <0 1 1> 0.071 280.8
Si (mp-149) <1 0 0> <0 1 0> 0.073 238.5
TbScO3 (mp-31119) <0 1 0> <0 0 1> 0.076 352.8
WS2 (mp-224) <1 0 0> <0 0 1> 0.077 320.7
LiAlO2 (mp-3427) <1 0 0> <0 1 1> 0.078 327.6
LiGaO2 (mp-5854) <1 0 0> <0 0 1> 0.079 320.7
TiO2 (mp-390) <1 0 0> <0 0 1> 0.081 256.6
LaF3 (mp-905) <0 0 1> <1 0 0> 0.083 273.4
Au (mp-81) <1 1 0> <1 0 0> 0.085 218.7
CdSe (mp-2691) <1 1 0> <0 1 0> 0.085 272.6
BN (mp-984) <1 0 0> <0 1 0> 0.086 136.3
GaSb (mp-1156) <1 1 0> <0 1 0> 0.091 272.6
TeO2 (mp-2125) <1 0 1> <0 1 0> 0.093 306.7
TiO2 (mp-390) <1 1 1> <0 1 1> 0.096 327.6
LiF (mp-1138) <1 1 1> <0 1 0> 0.097 204.4
BaTiO3 (mp-5986) <1 1 0> <1 1 0> 0.098 193.3
Al2O3 (mp-1143) <0 0 1> <1 1 0> 0.100 322.1
C (mp-66) <1 1 0> <0 1 0> 0.100 272.6
TiO2 (mp-2657) <1 1 1> <1 1 1> 0.102 143.9
PbSe (mp-2201) <1 1 0> <0 1 0> 0.107 272.6
GaSe (mp-1943) <0 0 1> <0 1 0> 0.113 102.2
WSe2 (mp-1821) <1 0 1> <1 1 0> 0.113 257.7
YAlO3 (mp-3792) <1 0 1> <0 1 0> 0.114 340.7
SrTiO3 (mp-4651) <1 0 0> <0 1 0> 0.114 306.7
LiNbO3 (mp-3731) <1 1 1> <0 0 1> 0.114 128.3
ZnTe (mp-2176) <1 1 0> <0 1 0> 0.117 272.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
108 59 64 0 0 0
59 115 84 0 0 0
64 84 112 0 0 0
0 0 0 40 0 0
0 0 0 0 18 0
0 0 0 0 0 26
Compliance Tensor Sij (10-12Pa-1)
14.6 -3.1 -6 0 0 0
-3.1 19.9 -13.2 0 0 0
-6 -13.2 22.3 0 0 0
0 0 0 24.8 0 0
0 0 0 0 55.5 0
0 0 0 0 0 38.8
Shear Modulus GV
25 GPa
Bulk Modulus KV
83 GPa
Shear Modulus GR
22 GPa
Bulk Modulus KR
82 GPa
Shear Modulus GVRH
24 GPa
Bulk Modulus KVRH
83 GPa
Elastic Anisotropy
0.70
Poisson's Ratio
0.37

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
EuSnPd (mp-913389) 0.1707 0.000 3
EuSnPt (mp-608517) 0.1825 0.000 3
YbNiSn (mp-22162) 0.2145 0.000 3
EuSnPd (mp-22031) 0.2063 0.000 3
TbAlAu (mp-1095572) 0.2263 0.000 3
RbHg2 (mp-9827) 0.5881 0.000 2
KHg2 (mp-30717) 0.6330 0.000 2
CaAg2 (mp-13270) 0.6191 0.000 2
ScGa2 (mp-11412) 0.6393 0.003 2
PuCu2 (mp-1025032) 0.6095 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ca_sv Ga_d Pt
Final Energy/Atom
-4.6210 eV
Corrected Energy
-55.4521 eV
Uncorrected energy = -55.4521 eV Corrected energy = -55.4521 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 106340
Submitted by
User remarks:
  • Calcium gallium platinum (1/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)