Final Magnetic Moment0.068 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.108 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.28 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mcm [140] |
Hall-I 4 2c |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 277.5 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 169.3 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 208.1 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 277.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 277.5 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 277.5 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 277.5 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 183.0 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 69.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 1> | 183.0 |
Al (mp-134) | <1 0 0> | <0 0 1> | 277.5 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 169.3 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 138.8 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 277.5 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 69.4 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 277.5 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 69.4 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 277.5 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 69.4 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 208.1 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 169.3 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 277.5 |
Si (mp-149) | <1 0 0> | <0 0 1> | 277.5 |
Au (mp-81) | <1 0 0> | <0 0 1> | 69.4 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 277.5 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 138.8 |
ZrO2 (mp-2858) | <1 1 0> | <0 0 1> | 277.5 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 277.5 |
ZnO (mp-2133) | <1 1 1> | <0 0 1> | 277.5 |
MgAl2O4 (mp-3536) | <1 0 0> | <0 0 1> | 69.4 |
Ge (mp-32) | <1 0 0> | <0 0 1> | 69.4 |
LiAlO2 (mp-3427) | <0 0 1> | <0 0 1> | 138.8 |
SrTiO3 (mp-4651) | <0 0 1> | <0 0 1> | 277.5 |
GaTe (mp-542812) | <1 0 0> | <1 0 1> | 183.0 |
LiAlO2 (mp-3427) | <1 0 1> | <1 0 0> | 169.3 |
LiAlO2 (mp-3427) | <1 1 1> | <0 0 1> | 277.5 |
CaF2 (mp-2741) | <1 0 0> | <0 0 1> | 277.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ga2Ir (mp-31253) | 0.7025 | 0.000 | 2 |
Tm3Ga5 (mp-30677) | 0.7376 | 0.000 | 2 |
SrIn (mp-608072) | 0.7376 | 0.000 | 2 |
Mg6Si5 (mp-1073933) | 0.7360 | 0.200 | 2 |
SrIn (mp-655461) | 0.7334 | 0.003 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: La Al Br |
Final Energy/Atom-4.6622 eV |
Corrected Energy-121.2159 eV
-121.2159 eV = -121.2159 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)