Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.015 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.082 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.73 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMoS2 + Mo |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/m [176] |
Hall-P 6c |
Point Group6/m |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 74.8 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 224.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 224.5 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 224.5 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 178.5 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 74.8 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 74.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 224.5 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 299.3 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 178.5 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 299.3 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 178.5 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 299.3 |
BN (mp-984) | <1 0 0> | <1 0 1> | 193.6 |
BN (mp-984) | <1 0 1> | <0 0 1> | 224.5 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 74.8 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 299.3 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 74.8 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 149.6 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 224.5 |
TiO2 (mp-2657) | <1 0 0> | <1 0 1> | 193.6 |
InSb (mp-20012) | <1 0 0> | <1 0 0> | 178.5 |
InSb (mp-20012) | <1 1 1> | <0 0 1> | 74.8 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 74.8 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 299.3 |
C (mp-48) | <0 0 1> | <0 0 1> | 299.3 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 299.3 |
C (mp-48) | <1 0 1> | <0 0 1> | 299.3 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 224.5 |
YAlO3 (mp-3792) | <0 1 1> | <0 0 1> | 149.6 |
YAlO3 (mp-3792) | <1 0 1> | <0 0 1> | 149.6 |
SiC (mp-8062) | <1 1 1> | <0 0 1> | 224.5 |
MgF2 (mp-1249) | <0 0 1> | <0 0 1> | 224.5 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 299.3 |
Ge (mp-32) | <1 1 1> | <0 0 1> | 224.5 |
LiAlO2 (mp-3427) | <1 0 0> | <0 0 1> | 299.3 |
Fe2O3 (mp-24972) | <0 0 1> | <0 0 1> | 299.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
K7(Mo9S11)4 (mp-685514) | 0.6871 | 0.029 | 3 |
Mo3S3Br (mp-29231) | 0.7078 | 0.027 | 3 |
K2Mo15S19 (mp-553922) | 0.7076 | 0.030 | 3 |
Rb4Mo21S25 (mp-579861) | 0.4946 | 0.017 | 3 |
K2Mo9S11 (mp-29784) | 0.7081 | 0.021 | 3 |
Mo9Se11 (mp-638048) | 0.6221 | 0.065 | 2 |
Mo15Se19 (mp-568488) | 0.4589 | 0.065 | 2 |
Mo15Se19 (mp-570170) | 0.4371 | 0.064 | 2 |
Mo3S4 (mp-2164) | 0.5612 | 0.065 | 2 |
Mo3Se4 (mp-21021) | 0.7307 | 0.061 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mo_pv S |
Final Energy/Atom-7.7403 eV |
Corrected Energy-551.5542 eV
-551.5542 eV = -526.3427 eV (uncorrected energy) - 25.2115 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)