material

Sn4Ir

ID:

mp-31277

DOI:

10.17188/1205552


Tags: Iridium tetrastannide - beta

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.219 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
9.27 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I41/acd [142]
Hall
I 4bw 2aw 1bw
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 412573 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
ZnSe (mp-1190) <1 0 0> <0 0 1> 0.000 164.7
GaAs (mp-2534) <1 0 0> <0 0 1> 0.008 164.7
KCl (mp-23193) <1 0 0> <0 0 1> 0.031 41.2
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.037 247.1
KCl (mp-23193) <1 1 0> <0 0 1> 0.037 288.3
Ge (mp-32) <1 0 0> <0 0 1> 0.042 164.7
C (mp-66) <1 0 0> <0 0 1> 0.046 164.7
ZnO (mp-2133) <0 0 1> <0 0 1> 0.046 329.5
GaN (mp-804) <0 0 1> <0 0 1> 0.051 288.3
LiGaO2 (mp-5854) <0 1 0> <0 0 1> 0.058 164.7
Al (mp-134) <1 0 0> <0 0 1> 0.062 82.4
MgO (mp-1265) <1 0 0> <0 0 1> 0.068 164.7
SiC (mp-8062) <1 0 0> <0 0 1> 0.070 329.5
YAlO3 (mp-3792) <1 0 1> <0 0 1> 0.095 247.1
LiF (mp-1138) <1 0 0> <0 0 1> 0.098 82.4
YVO4 (mp-19133) <1 1 0> <0 0 1> 0.101 329.5
Ni (mp-23) <1 1 0> <0 0 1> 0.123 329.5
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.123 82.4
YVO4 (mp-19133) <0 0 1> <0 0 1> 0.146 205.9
PbS (mp-21276) <1 0 0> <0 0 1> 0.158 329.5
Ni (mp-23) <1 0 0> <0 0 1> 0.168 205.9
Cu (mp-30) <1 0 0> <0 0 1> 0.172 205.9
NaCl (mp-22862) <1 0 0> <0 0 1> 0.184 164.7
CdS (mp-672) <1 1 1> <0 0 1> 0.213 205.9
Te2W (mp-22693) <0 0 1> <1 0 1> 0.228 154.5
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.254 329.5
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.256 329.5
LiAlO2 (mp-3427) <1 0 0> <0 0 1> 0.332 164.7
YVO4 (mp-19133) <1 0 0> <0 0 1> 0.334 329.5
GaN (mp-804) <1 0 0> <0 0 1> 0.349 205.9
CdS (mp-672) <0 0 1> <0 0 1> 0.383 329.5
C (mp-48) <0 0 1> <0 0 1> 0.434 205.9
Te2W (mp-22693) <1 0 1> <0 0 1> 0.441 205.9
LiAlO2 (mp-3427) <1 1 0> <0 0 1> 0.446 288.3
SiC (mp-11714) <1 0 1> <0 0 1> 0.447 288.3
GdScO3 (mp-5690) <1 1 0> <0 0 1> 0.450 329.5
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.454 205.9
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.454 205.9
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.458 205.9
Mg (mp-153) <1 0 0> <0 0 1> 0.475 205.9
TiO2 (mp-2657) <1 1 1> <0 0 1> 0.488 205.9
Cu (mp-30) <1 1 1> <0 0 1> 0.502 205.9
AlN (mp-661) <0 0 1> <0 0 1> 0.505 205.9
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.506 82.4
AlN (mp-661) <1 0 0> <0 0 1> 0.509 288.3
TiO2 (mp-2657) <1 1 0> <1 0 1> 0.517 154.5
ZnO (mp-2133) <1 0 0> <0 0 1> 0.524 205.9
AlN (mp-661) <1 0 1> <0 0 1> 0.526 288.3
MgF2 (mp-1249) <1 1 1> <0 0 1> 0.570 205.9
Ge(Bi3O5)4 (mp-23352) <1 0 0> <0 0 1> 0.593 205.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
127 49 48 0 0 0
49 127 48 0 0 0
48 48 109 0 0 0
0 0 0 33 0 0
0 0 0 0 33 0
0 0 0 0 0 41
Compliance Tensor Sij (10-12Pa-1)
10.1 -2.7 -3.2 0 0 0
-2.7 10.1 -3.2 0 0 0
-3.2 -3.2 12 0 0 0
0 0 0 30.4 0 0
0 0 0 0 30.4 0
0 0 0 0 0 24.3
Shear Modulus GV
36 GPa
Bulk Modulus KV
72 GPa
Shear Modulus GR
36 GPa
Bulk Modulus KR
72 GPa
Shear Modulus GVRH
36 GPa
Bulk Modulus KVRH
72 GPa
Elastic Anisotropy
0.06
Poisson's Ratio
0.29

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
LaNdI4 (mp-569670) 0.6587 0.105 3
BaSrI4 (mp-754199) 0.5698 0.042 3
BaCaI4 (mp-753709) 0.6349 0.069 3
CeSmI4 (mp-570470) 0.6486 0.080 3
CeNdI4 (mp-570728) 0.6382 0.081 3
U2Te2PO (mp-1095312) 0.7176 0.000 4
Sn4Pt (mp-20662) 0.2963 0.000 2
Sn4Pd (mp-2128) 0.1712 0.000 2
Sn4Au (mp-1393) 0.4149 0.000 2
UTe3 (mp-8357) 0.6383 0.042 2
Sn4Ir (mp-1080586) 0.0906 0.007 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Sn_d Ir
Final Energy/Atom
-5.1801 eV
Corrected Energy
-103.6030 eV
-103.6030 eV = -103.6030 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 412573
Submitted by
User remarks:
  • Iridium tetrastannide - beta

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)