Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.117 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.93 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2221 [20] |
HallC 2c 2 |
Point Group222 |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 248.1 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 162.4 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 209.5 |
InAs (mp-20305) | <1 1 0> | <0 1 1> | 162.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 162.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 248.1 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 194.1 |
GaSe (mp-1943) | <1 0 0> | <0 1 0> | 209.5 |
LiNbO3 (mp-3731) | <1 1 0> | <0 0 1> | 124.0 |
TeO2 (mp-2125) | <0 0 1> | <1 1 0> | 194.1 |
Al (mp-134) | <1 0 0> | <0 1 1> | 162.4 |
LiTaO3 (mp-3666) | <1 1 0> | <0 0 1> | 124.0 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 124.0 |
C (mp-66) | <1 1 0> | <0 1 1> | 162.4 |
GdScO3 (mp-5690) | <0 0 1> | <1 1 0> | 194.1 |
TbScO3 (mp-31119) | <1 1 1> | <0 1 0> | 209.5 |
PbSe (mp-2201) | <1 1 0> | <0 1 1> | 162.4 |
BaTiO3 (mp-5986) | <1 0 1> | <0 1 0> | 209.5 |
CdSe (mp-2691) | <1 1 0> | <0 1 1> | 162.4 |
SiC (mp-8062) | <1 1 0> | <0 1 1> | 162.4 |
MgAl2O4 (mp-3536) | <1 1 0> | <1 1 0> | 194.1 |
GaSb (mp-1156) | <1 1 0> | <0 1 1> | 162.4 |
Fe2O3 (mp-24972) | <1 1 0> | <0 0 1> | 124.0 |
ZnTe (mp-2176) | <1 1 0> | <0 1 1> | 162.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li12Al3Si4 (mp-14378) | 0.6711 | 0.094 | 3 |
Li8Zn2Ge3 (mp-569373) | 0.6055 | 0.000 | 3 |
Li2BiAu (mp-1078700) | 0.6158 | 0.040 | 3 |
Hf8Ni21 (mp-27165) | 0.4652 | 0.041 | 2 |
Hf3Ni7 (mp-27166) | 0.5399 | 0.032 | 2 |
Zr8Ni21 (mp-30260) | 0.4597 | 0.024 | 2 |
Mg4Si3 (mp-1074549) | 0.4522 | 0.217 | 2 |
Na2Tl (mp-30795) | 0.2710 | 0.000 | 2 |
Pu (mp-542606) | 0.7414 | 1.065 | 1 |
Nb (mp-1094120) | 0.5198 | 0.190 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv In_d |
Final Energy/Atom-1.9088 eV |
Corrected Energy-45.8124 eV
Uncorrected energy = -45.8124 eV
Corrected energy = -45.8124 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)