material

ZrNiBi

ID:

mp-31452

DOI:

10.17188/1205667


Tags: Zirconium nickel bismuthide (1/1/1)

Material Details

Final Magnetic Moment
0.004 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.309 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.071 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
9.57 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Zr8Bi13 + ZrNi3 + ZrBi
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
F43m [216]
Hall
F 4 2 3
Point Group
43m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 107121 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Fe2O3 (mp-24972) <0 0 1> <1 1 1> 0.000 68.6
Bi2Te3 (mp-34202) <0 0 1> <1 1 1> 0.000 68.6
C (mp-48) <0 0 1> <1 1 1> 0.000 68.6
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.003 197.9
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.003 356.3
BaF2 (mp-1029) <1 1 1> <1 1 1> 0.006 68.6
BaF2 (mp-1029) <1 1 0> <1 1 0> 0.006 56.0
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.006 39.6
WS2 (mp-224) <0 0 1> <1 1 1> 0.009 274.3
MoS2 (mp-1434) <0 0 1> <1 1 1> 0.009 274.3
Y3Fe5O12 (mp-19648) <1 0 0> <1 0 0> 0.011 158.4
Te2Mo (mp-602) <1 0 0> <1 1 1> 0.018 274.3
DyScO3 (mp-31120) <1 1 0> <1 0 0> 0.020 316.7
TbScO3 (mp-31119) <1 1 0> <1 0 0> 0.024 316.7
CeO2 (mp-20194) <1 1 1> <1 1 1> 0.034 205.7
CeO2 (mp-20194) <1 1 0> <1 1 0> 0.035 168.0
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.039 356.3
Si (mp-149) <1 1 1> <1 1 1> 0.039 205.7
Si (mp-149) <1 1 0> <1 1 0> 0.040 168.0
Mg (mp-153) <0 0 1> <1 1 1> 0.045 274.3
TiO2 (mp-2657) <1 1 1> <1 1 1> 0.046 205.7
InP (mp-20351) <1 0 0> <1 0 0> 0.055 316.7
C (mp-66) <1 0 0> <1 0 0> 0.059 316.7
Cu (mp-30) <1 1 1> <1 1 1> 0.059 68.6
Cu (mp-30) <1 1 0> <1 1 0> 0.060 56.0
Ni (mp-23) <1 1 1> <1 1 1> 0.079 274.3
Ni (mp-23) <1 0 0> <1 0 0> 0.083 158.4
Ga2O3 (mp-886) <1 0 0> <1 1 1> 0.085 274.3
ZnO (mp-2133) <1 0 1> <1 1 0> 0.091 279.9
Au (mp-81) <1 1 0> <1 1 0> 0.092 223.9
Au (mp-81) <1 0 0> <1 0 0> 0.097 158.4
GaN (mp-804) <0 0 1> <1 0 0> 0.102 316.7
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.103 79.2
ZnO (mp-2133) <1 1 0> <1 1 0> 0.103 335.9
InSb (mp-20012) <1 0 0> <1 0 0> 0.114 356.3
CdWO4 (mp-19387) <0 0 1> <1 1 1> 0.134 274.3
ZnO (mp-2133) <1 1 1> <1 1 0> 0.138 223.9
C (mp-48) <1 0 1> <1 1 0> 0.138 335.9
CdTe (mp-406) <1 0 0> <1 0 0> 0.139 356.3
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.140 316.7
Te2W (mp-22693) <1 0 1> <1 0 0> 0.141 197.9
Ni (mp-23) <1 1 0> <1 1 0> 0.183 335.9
AlN (mp-661) <0 0 1> <1 1 0> 0.187 168.0
Ag (mp-124) <1 1 0> <1 1 0> 0.196 223.9
C (mp-66) <1 1 0> <1 1 1> 0.200 274.3
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.204 197.9
Ag (mp-124) <1 0 0> <1 0 0> 0.205 158.4
TiO2 (mp-390) <0 0 1> <1 0 0> 0.214 356.3
LiF (mp-1138) <1 1 1> <1 1 1> 0.220 205.7
Ga2O3 (mp-886) <1 1 0> <1 1 0> 0.220 223.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
176 69 69 0 0 0
69 176 69 0 0 0
69 69 176 0 0 0
0 0 0 30 0 0
0 0 0 0 30 0
0 0 0 0 0 30
Compliance Tensor Sij (10-12Pa-1)
7.3 -2.1 -2.1 0 0 0
-2.1 7.3 -2.1 0 0 0
-2.1 -2.1 7.3 0 0 0
0 0 0 33 0 0
0 0 0 0 33 0
0 0 0 0 0 33
Shear Modulus GV
39 GPa
Bulk Modulus KV
104 GPa
Shear Modulus GR
37 GPa
Bulk Modulus KR
104 GPa
Shear Modulus GVRH
38 GPa
Bulk Modulus KVRH
104 GPa
Elastic Anisotropy
0.39
Poisson's Ratio
0.34

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
MgCuBi (mp-30449) 0.0000 0.041 3
HoBiPt (mp-30455) 0.0000 0.000 3
YNiBi (mp-30460) 0.0000 0.000 3
HfSbRu (mp-31456) 0.0000 0.030 3
MgCuSn (mp-11361) 0.0000 0.000 3
AcH2 (mp-24147) 0.0000 0.000 2
Mg2Ge (mp-408) 0.0000 0.000 2
PbF2 (mp-315) 0.0000 0.000 2
K2Te (mp-1747) 0.0000 0.000 2
UN2 (mp-1776) 0.0000 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Zr_sv Ni_pv Bi
Final Energy/Atom
-6.3803 eV
Corrected Energy
-19.1410 eV
-19.1410 eV = -19.1410 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 107121
Submitted by
User remarks:
  • Zirconium nickel bismuthide (1/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)