material

BaPt

ID:

mp-31498

DOI:

10.17188/1205708


Tags: Barium platinum (1/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.749 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.71 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 55492 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.001 208.7
LiGaO2 (mp-5854) <1 1 1> <0 0 1> 0.003 278.3
LiGaO2 (mp-5854) <1 0 0> <1 0 0> 0.003 141.5
Si (mp-149) <1 1 0> <1 0 0> 0.009 84.9
Ni (mp-23) <1 1 1> <0 0 1> 0.010 278.3
CeO2 (mp-20194) <1 1 0> <1 0 0> 0.011 84.9
GaN (mp-804) <1 0 1> <0 0 1> 0.016 324.7
NdGaO3 (mp-3196) <0 1 0> <1 0 0> 0.020 84.9
Ga2O3 (mp-886) <1 0 0> <1 0 0> 0.025 198.1
LiGaO2 (mp-5854) <1 0 1> <1 0 0> 0.032 226.4
Te2Mo (mp-602) <1 0 1> <0 0 1> 0.042 278.3
TePb (mp-19717) <1 1 1> <0 0 1> 0.045 301.5
CdTe (mp-406) <1 1 1> <0 0 1> 0.050 301.5
ZrO2 (mp-2858) <1 1 -1> <1 1 1> 0.051 271.1
LiNbO3 (mp-3731) <1 0 0> <1 0 1> 0.056 73.2
TiO2 (mp-390) <1 0 1> <0 0 1> 0.056 278.3
CdWO4 (mp-19387) <1 0 0> <0 0 1> 0.063 92.8
InSb (mp-20012) <1 1 1> <0 0 1> 0.063 301.5
AlN (mp-661) <1 1 1> <1 1 0> 0.070 343.1
GaP (mp-2490) <1 1 0> <1 0 0> 0.075 84.9
BaF2 (mp-1029) <1 1 0> <0 0 1> 0.077 278.3
AlN (mp-661) <0 0 1> <1 0 0> 0.078 84.9
Mg (mp-153) <1 0 1> <0 0 1> 0.080 324.7
LiAlO2 (mp-3427) <1 0 1> <1 0 0> 0.086 84.9
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.086 23.2
LiAlO2 (mp-3427) <1 0 0> <1 0 0> 0.090 198.1
MgF2 (mp-1249) <1 1 1> <0 0 1> 0.094 208.7
LaAlO3 (mp-2920) <0 0 1> <1 0 0> 0.094 254.7
GaTe (mp-542812) <1 0 0> <1 0 0> 0.095 226.4
ZrO2 (mp-2858) <1 1 1> <1 0 0> 0.098 311.2
SiO2 (mp-6930) <1 0 1> <1 1 0> 0.101 245.0
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.107 69.6
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.109 23.2
MgO (mp-1265) <1 1 1> <0 0 1> 0.113 92.8
C (mp-48) <0 0 1> <0 0 1> 0.117 69.6
GdScO3 (mp-5690) <0 1 0> <1 0 0> 0.128 311.2
NdGaO3 (mp-3196) <0 1 1> <1 0 0> 0.128 311.2
LiTaO3 (mp-3666) <1 0 0> <1 0 1> 0.129 73.2
CaF2 (mp-2741) <1 1 0> <1 0 0> 0.130 84.9
CdWO4 (mp-19387) <0 0 1> <0 0 1> 0.131 92.8
Fe2O3 (mp-24972) <1 1 0> <1 1 0> 0.137 245.0
GdScO3 (mp-5690) <1 1 1> <1 1 1> 0.138 216.9
SiO2 (mp-6930) <1 1 0> <1 0 0> 0.146 141.5
ZrO2 (mp-2858) <0 1 1> <0 0 1> 0.148 116.0
CdWO4 (mp-19387) <1 0 1> <1 1 1> 0.150 271.1
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.150 141.5
WS2 (mp-224) <0 0 1> <1 0 0> 0.151 141.5
Mg (mp-153) <0 0 1> <1 0 0> 0.155 141.5
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.156 69.6
LiNbO3 (mp-3731) <1 0 1> <1 0 0> 0.161 311.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
70 36 34 0 0 0
36 70 34 0 0 0
34 34 106 0 0 0
0 0 0 17 0 0
0 0 0 0 17 0
0 0 0 0 0 17
Compliance Tensor Sij (10-12Pa-1)
20.5 -8.6 -3.8 0 0 0
-8.6 20.5 -3.8 0 0 0
-3.8 -3.8 11.8 0 0 0
0 0 0 60.3 0 0
0 0 0 0 60.3 0
0 0 0 0 0 58.3
Shear Modulus GV
20 GPa
Bulk Modulus KV
50 GPa
Shear Modulus GR
18 GPa
Bulk Modulus KR
49 GPa
Shear Modulus GVRH
19 GPa
Bulk Modulus KVRH
50 GPa
Elastic Anisotropy
0.34
Poisson's Ratio
0.33

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Cr2SbTe (mp-675700) 0.4465 0.291 3
LiIO3 (mp-1080052) 0.6603 0.868 3
CuBi (mp-569792) 0.4141 0.110 2
InCu (mp-1018053) 0.6449 0.065 2
BaPd (mp-1064367) 0.2252 0.004 2
BPt (mp-2192) 0.3004 0.202 2
TlNi (mp-11524) 0.6278 0.228 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ba_sv Pt
Final Energy/Atom
-4.7440 eV
Corrected Energy
-18.9761 eV
Uncorrected energy = -18.9761 eV Corrected energy = -18.9761 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 55492
Submitted by
User remarks:
  • Barium platinum (1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)