Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.351 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.055 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.37 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCoPO4 + LiPO3 |
Band Gap0.991 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 1 0> | 111.2 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 276.1 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 235.6 |
CeO2 (mp-20194) | <1 1 1> | <1 -1 0> | 251.5 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 166.9 |
GaAs (mp-2534) | <1 1 0> | <1 1 -1> | 234.6 |
BaF2 (mp-1029) | <1 0 0> | <1 0 -1> | 279.2 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 277.1 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 285.1 |
GaN (mp-804) | <1 0 1> | <1 0 -1> | 209.4 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 220.8 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 282.8 |
AlN (mp-661) | <1 0 1> | <1 -1 1> | 197.3 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 235.6 |
CeO2 (mp-20194) | <1 0 0> | <0 1 1> | 331.3 |
GaAs (mp-2534) | <1 1 1> | <1 1 -1> | 234.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 199.3 |
GaN (mp-804) | <1 0 0> | <0 1 -1> | 171.3 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 188.5 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 141.4 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 237.5 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 277.1 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 285.1 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 220.8 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 356.2 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 -1> | 234.6 |
DyScO3 (mp-31120) | <1 0 1> | <1 -1 1> | 263.0 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 141.4 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 309.7 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 277.1 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 166.9 |
ZnSe (mp-1190) | <1 1 0> | <1 1 -1> | 234.6 |
ZnSe (mp-1190) | <1 1 1> | <1 1 -1> | 234.6 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 1> | 114.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 -1> | 234.6 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 309.7 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 228.1 |
CdS (mp-672) | <1 0 0> | <1 -1 1> | 197.3 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 220.8 |
CdS (mp-672) | <1 1 0> | <1 -1 1> | 197.3 |
CdS (mp-672) | <1 1 1> | <1 0 -1> | 209.4 |
LiF (mp-1138) | <1 0 0> | <1 1 1> | 114.0 |
LiF (mp-1138) | <1 1 0> | <1 1 -1> | 234.6 |
Te2W (mp-22693) | <0 0 1> | <0 1 -1> | 114.2 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 221.2 |
Te2W (mp-22693) | <1 1 0> | <1 0 0> | 221.2 |
Te2W (mp-22693) | <1 1 1> | <1 1 1> | 114.0 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 220.8 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 277.1 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 316.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
FeSiO3 (mp-630331) | 0.4706 | 0.038 | 3 |
FeSiO3 (mp-650392) | 0.4255 | 0.821 | 3 |
ZnSiO3 (mp-619034) | 0.4447 | 0.054 | 3 |
Ni5(P3O11)2 (mp-32359) | 0.4527 | 0.098 | 3 |
Mn5(P3O11)2 (mp-705036) | 0.4633 | 0.065 | 3 |
LiNiP2O7 (mp-540272) | 0.1933 | 0.050 | 4 |
LiCrP2O7 (mp-31642) | 0.1221 | 0.011 | 4 |
LiFeP2O7 (mp-31830) | 0.1162 | 0.005 | 4 |
LiTiP2O7 (mp-26629) | 0.3383 | 0.055 | 4 |
LiVP2O7 (mp-32411) | 0.1253 | 0.009 | 4 |
Li2MnV(P2O7)2 (mp-778770) | 0.3960 | 0.172 | 5 |
Li2MnV(PO4)3 (mp-770223) | 0.3787 | 0.225 | 5 |
Li2MnV(PO4)3 (mp-770135) | 0.3869 | 0.216 | 5 |
Li2MnV(P2O7)2 (mp-764603) | 0.3925 | 0.097 | 5 |
Li2MnV(P2O7)2 (mp-774358) | 0.3971 | 0.130 | 5 |
NaLi5Ti3Cr3(PO4)9 (mp-744549) | 0.6601 | 0.059 | 6 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.5740 | 0.003 | 6 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.6800 | 0.028 | 6 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.4960 | 0.041 | 6 |
Li4Mn2VNi3(PO4)6 (mp-770417) | 0.6907 | 0.075 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.5726 | 0.068 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Co P O |
Final Energy/Atom-6.6867 eV |
Corrected Energy-160.0015 eV
Uncorrected energy = -147.1075 eV
Composition-based energy adjustment (-0.687 eV/atom x 14.0 atoms) = -9.6180 eV
Composition-based energy adjustment (-1.638 eV/atom x 2.0 atoms) = -3.2760 eV
Corrected energy = -160.0015 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)