material

Li2SbPt

ID:

mp-3158

DOI:

10.17188/1205761


Tags: High pressure experimental phase Lithium platinum antimonide (2/1/1)

Material Details

Final Magnetic Moment
-0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Non-magnetic
Formation Energy / Atom
-0.680 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.53 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
F43m [216]
Hall
F 4 2 3
Point Group
43m
Crystal System
cubic

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
NaCl (mp-22862) <1 0 0> <1 0 0> 0.000 161.9
PbS (mp-21276) <1 0 0> <1 0 0> 0.001 323.9
GaP (mp-2490) <1 1 0> <1 1 0> 0.001 171.8
GaP (mp-2490) <1 1 1> <1 1 1> 0.001 210.4
CaF2 (mp-2741) <1 1 0> <1 1 0> 0.002 171.8
CaF2 (mp-2741) <1 1 1> <1 1 1> 0.002 210.4
Ag (mp-124) <1 1 1> <1 1 1> 0.003 210.4
Au (mp-81) <1 1 1> <1 1 1> 0.004 210.4
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.005 81.0
CdWO4 (mp-19387) <1 0 0> <1 1 1> 0.005 280.5
YVO4 (mp-19133) <1 1 0> <1 0 0> 0.010 323.9
WS2 (mp-224) <0 0 1> <1 0 0> 0.013 283.4
LiTaO3 (mp-3666) <0 0 1> <1 1 1> 0.013 70.1
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.013 283.4
YVO4 (mp-19133) <1 0 0> <1 1 0> 0.015 229.0
SiC (mp-8062) <1 0 0> <1 0 0> 0.019 323.9
MgO (mp-1265) <1 0 0> <1 0 0> 0.020 161.9
Al (mp-134) <1 0 0> <1 0 0> 0.023 81.0
MgO (mp-1265) <1 1 0> <1 1 0> 0.023 229.0
MgO (mp-1265) <1 1 1> <1 1 1> 0.024 280.5
Te2W (mp-22693) <1 0 1> <1 0 0> 0.035 202.4
Mg (mp-153) <0 0 1> <1 0 0> 0.037 283.4
NdGaO3 (mp-3196) <0 1 0> <1 1 0> 0.037 171.8
Cu (mp-30) <1 0 0> <1 0 0> 0.038 323.9
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.038 323.9
Mg (mp-153) <1 0 0> <1 0 0> 0.041 202.4
Bi2Se3 (mp-541837) <0 0 1> <1 1 0> 0.041 229.0
AlN (mp-661) <1 0 0> <1 0 0> 0.044 283.4
KCl (mp-23193) <1 0 0> <1 0 0> 0.044 40.5
Te2Mo (mp-602) <0 0 1> <1 1 1> 0.045 210.4
MgF2 (mp-1249) <1 1 1> <1 1 1> 0.049 210.4
GaN (mp-804) <0 0 1> <1 1 1> 0.049 280.5
LaF3 (mp-905) <0 0 1> <1 1 0> 0.050 229.0
KCl (mp-23193) <1 1 0> <1 1 0> 0.051 57.3
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.051 81.0
KCl (mp-23193) <1 1 1> <1 1 1> 0.053 70.1
LiNbO3 (mp-3731) <0 0 1> <1 1 1> 0.058 70.1
Ni (mp-23) <1 0 0> <1 0 0> 0.062 161.9
CdS (mp-672) <0 0 1> <1 1 0> 0.062 229.0
SiO2 (mp-6930) <0 0 1> <1 1 1> 0.066 280.5
Ni (mp-23) <1 1 1> <1 1 1> 0.074 280.5
LiGaO2 (mp-5854) <1 1 0> <1 0 0> 0.075 242.9
Te2Mo (mp-602) <1 0 1> <1 1 1> 0.075 280.5
InP (mp-20351) <1 0 0> <1 0 0> 0.083 323.9
ZnO (mp-2133) <0 0 1> <1 0 0> 0.088 323.9
AlN (mp-661) <0 0 1> <1 1 0> 0.091 171.8
YAlO3 (mp-3792) <1 0 1> <1 0 0> 0.095 242.9
AlN (mp-661) <1 0 1> <1 0 0> 0.102 283.4
Si (mp-149) <1 1 0> <1 1 0> 0.110 171.8
LiGaO2 (mp-5854) <0 1 0> <1 0 0> 0.113 161.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
93 75 75 0 0 0
75 93 75 0 0 0
75 75 93 0 0 0
0 0 0 58 0 0
0 0 0 0 58 0
0 0 0 0 0 58
Compliance Tensor Sij (10-12Pa-1)
38.9 -17.4 -17.4 0 0 0
-17.4 38.9 -17.4 0 0 0
-17.4 -17.4 38.9 0 0 0
0 0 0 17.2 0 0
0 0 0 0 17.2 0
0 0 0 0 0 17.2
Shear Modulus GV
38 GPa
Bulk Modulus KV
81 GPa
Shear Modulus GR
18 GPa
Bulk Modulus KR
81 GPa
Shear Modulus GVRH
28 GPa
Bulk Modulus KVRH
81 GPa
Elastic Anisotropy
5.65
Poisson's Ratio
0.34

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TiFeCoSi (mp-998971) 0.0000 0.027 4
TiFeCoAs (mp-998974) 0.0000 0.146 4
LiMgSbPd (mp-10179) 0.0000 0.067 4
MnGaFeCo (mp-999552) 0.0000 0.045 4
TiGaFeCo (mp-998964) 0.0000 0.000 4
Cs3Sb (mp-10378) 0.0000 0.000 2
Li3Bi (mp-23222) 0.0000 0.000 2
Li3Pd (mp-11489) 0.0000 0.000 2
LiZn (mp-1934) 0.0000 0.000 2
Rb3Bi (mp-23304) 0.0000 0.030 2
HoInAu2 (mp-30388) 0.0000 0.000 3
FeCo2Si (mp-5436) 0.0000 0.000 3
FeCo2Ge (mp-22300) 0.0000 0.000 3
LiNi2Sn (mp-13915) 0.0000 0.000 3
NbAlNi2 (mp-4813) 0.0000 0.000 3
Dy (mp-10751) 0.0000 0.139 1
La (mp-10023) 0.0000 0.143 1
Rb (mp-70) 0.0000 0.000 1
Cs (mp-1) 0.0000 0.002 1
Eu (mp-20071) 0.0000 0.082 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Li_sv Sb Pt
Final Energy/Atom
-4.1803 eV
Corrected Energy
-16.7212 eV
-16.7212 eV = -16.7212 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 642284
  • 44895
Submitted by
User remarks:
  • High pressure experimental phase
  • Lithium platinum antimonide (2/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)