material

BaSnO3

ID:

mp-3163

DOI:

10.17188/1205802


Tags: Barium catena-stannate Barium stannate - nanopowder Barium stannate Barium tin trioxide Barium stannate(IV) Barium stannate(IV) - dry Barium stannate - Pr-doted (2%)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-2.587 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.87 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.395 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pm3m [221]
Hall
-P 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 27049 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.000 157.9
BaF2 (mp-1029) <1 1 0> <1 1 0> 0.000 223.3
KCl (mp-23193) <1 1 1> <1 1 1> 0.001 212.7
Y3Fe5O12 (mp-19648) <1 0 0> <1 0 0> 0.001 157.9
CdTe (mp-406) <1 0 0> <1 0 0> 0.003 87.7
ZnO (mp-2133) <0 0 1> <1 1 1> 0.003 121.6
BN (mp-984) <0 0 1> <1 1 1> 0.004 212.7
Fe2O3 (mp-24972) <0 0 1> <1 1 1> 0.007 91.2
Ge3(BiO3)4 (mp-23560) <1 0 0> <1 0 0> 0.007 228.1
InSb (mp-20012) <1 0 0> <1 0 0> 0.007 87.7
Te2W (mp-22693) <1 1 0> <1 1 0> 0.010 223.3
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.016 87.7
Cu (mp-30) <1 1 0> <1 1 0> 0.028 74.4
Cu (mp-30) <1 1 1> <1 1 1> 0.028 91.2
DyScO3 (mp-31120) <1 1 0> <1 0 0> 0.031 315.8
KP(HO2)2 (mp-23959) <1 0 0> <1 0 0> 0.034 228.1
ZrO2 (mp-2858) <0 1 0> <1 1 0> 0.034 223.3
NaCl (mp-22862) <1 1 0> <1 1 0> 0.039 272.9
Ge(Bi3O5)4 (mp-23352) <1 1 0> <1 1 0> 0.042 148.9
CdS (mp-672) <0 0 1> <1 0 0> 0.044 122.8
TbScO3 (mp-31119) <1 1 0> <1 0 0> 0.050 315.8
Au (mp-81) <1 0 0> <1 0 0> 0.051 17.5
Au (mp-81) <1 1 0> <1 1 0> 0.051 24.8
Au (mp-81) <1 1 1> <1 1 1> 0.052 30.4
LiAlO2 (mp-3427) <1 0 0> <1 0 0> 0.052 263.2
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.061 223.3
CaF2 (mp-2741) <1 1 1> <1 1 1> 0.061 212.7
Al2O3 (mp-1143) <1 0 1> <1 1 0> 0.065 198.5
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.081 87.7
AlN (mp-661) <1 1 1> <1 1 0> 0.087 198.5
InP (mp-20351) <1 0 0> <1 0 0> 0.094 35.1
InP (mp-20351) <1 1 0> <1 1 0> 0.095 49.6
GaTe (mp-542812) <1 0 1> <1 1 0> 0.097 99.2
Bi2Se3 (mp-541837) <0 0 1> <1 0 0> 0.101 122.8
C (mp-48) <1 0 1> <1 1 0> 0.109 322.6
GaP (mp-2490) <1 1 1> <1 1 1> 0.118 212.7
Bi2Te3 (mp-34202) <0 0 1> <1 1 1> 0.120 121.6
Ni (mp-23) <1 0 0> <1 0 0> 0.130 157.9
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.132 87.7
Ag (mp-124) <1 0 0> <1 0 0> 0.133 17.5
Ag (mp-124) <1 1 0> <1 1 0> 0.134 24.8
Ag (mp-124) <1 1 1> <1 1 1> 0.135 30.4
Ga2O3 (mp-886) <0 1 0> <1 1 1> 0.153 212.7
CdS (mp-672) <1 0 1> <1 0 0> 0.154 193.0
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.161 223.3
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.199 315.8
Al2O3 (mp-1143) <0 0 1> <1 1 0> 0.215 99.2
TePb (mp-19717) <1 0 0> <1 0 0> 0.216 87.7
CdWO4 (mp-19387) <1 0 0> <1 1 0> 0.235 124.1
PbSe (mp-2201) <1 0 0> <1 0 0> 0.236 157.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
250 76 76 0 0 0
76 250 76 0 0 0
76 76 250 0 0 0
0 0 0 92 0 0
0 0 0 0 92 0
0 0 0 0 0 92
Compliance Tensor Sij (10-12Pa-1)
4.7 -1.1 -1.1 0 0 0
-1.1 4.7 -1.1 0 0 0
-1.1 -1.1 4.7 0 0 0
0 0 0 10.9 0 0
0 0 0 0 10.9 0
0 0 0 0 0 10.9
Shear Modulus GV
90 GPa
Bulk Modulus KV
134 GPa
Shear Modulus GR
90 GPa
Bulk Modulus KR
134 GPa
Shear Modulus GVRH
90 GPa
Bulk Modulus KVRH
134 GPa
Elastic Anisotropy
0.00
Poisson's Ratio
0.23

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
5.47 0.00 0.00
0.00 5.47 0.00
0.00 0.00 5.47
Dielectric Tensor εij (total)
22.51 0.00 0.00
0.00 22.51 0.00
0.00 0.00 22.51
Polycrystalline dielectric constant εpoly
(electronic contribution)
5.47
Polycrystalline dielectric constant εpoly
(total)
22.51
Refractive Index n
2.34
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ni3SnN (mp-1017632) 0.0000 0.080 3
Ba3SbN (mp-1013708) 0.0000 1.397 3
Ca3AsP (mp-1013642) 0.0000 0.171 3
Ba3SbP (mp-1013737) 0.0000 0.157 3
Sm3AlN (mp-1094052) 0.0000 0.000 3
Ba2VFeO6 (mp-1096778) 0.0000 2.272 4
Ba2ScSbO6 (mp-20709) 0.0000 2.196 4
Ba2YbSbO6 (mp-14223) 0.0000 1.746 4
Ba2YSbO6 (mp-14226) 0.0000 2.078 4
Ba2NbFeO6 (mp-1096853) 0.0000 2.945 4
Fe4N (mp-535) 0.0000 0.070 2
Sr3Sb2 (mp-1013583) 0.0000 0.378 2
Ni4N (mp-20839) 0.0000 2.019 2
Sr3P2 (mp-1013552) 0.0000 0.403 2
Ca3P2 (mp-1013547) 0.0000 0.146 2
BaLaMgBiO6 (mp-41414) 0.0488 0.096 5
BaLaMgNbO6 (mp-39288) 0.0712 0.090 5
SrLaNbZnO6 (mp-41918) 0.0665 0.126 5
SrLaMnCoO6 (mp-40761) 0.0404 0.254 5
Sr6Ca2MnFe7O24 (mp-1075969) 0.0482 0.021 5
Na5Ca2Ce3Ti8Nb2O30 (mp-721094) 0.7380 0.065 6
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

BaSnO3, prepared by solid state reaction, served as starting material for further heat treatment. Appropriate amounts of BaCO3 and dried SnO2 both of purity (>99.5%) were homogenized in a agate mortar [...]
The precursors ASnO3 (A=Ca, Sr and Ba) have been prepared by solid state reactions from ACO3 (Prolabo 99.9%) and SnO2 (Ventron 99.9%). The starting reagents were heated at 400 and 250C, respectively [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition BaSnO3.

Text computed by synthesisproject.org.

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ba_sv Sn_d O
Final Energy/Atom
-6.3298 eV
Corrected Energy
-33.7098 eV
Uncorrected energy = -31.6488 eV Composition-based energy adjustment (-0.687 eV/atom x 3.0 atoms) = -2.0610 eV Corrected energy = -33.7098 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 239582
  • 186899
  • 180138
  • 181091
  • 190601
  • 188149
  • 424820
  • 43138
  • 185615
  • 27049
  • 184338
Submitted by
User remarks:
  • Barium stannate(IV) - dry

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)