Final Magnetic Moment3.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.666 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.32 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.841 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2 [5] |
HallC 2y |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 -1> | 230.8 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 215.0 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 -1> | 230.8 |
LaAlO3 (mp-2920) | <1 1 0> | <0 1 0> | 259.8 |
AlN (mp-661) | <0 0 1> | <1 0 -1> | 230.8 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 231.0 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 346.5 |
AlN (mp-661) | <1 1 1> | <1 1 1> | 310.4 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 231.0 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 216.1 |
BaF2 (mp-1029) | <1 1 1> | <0 1 0> | 202.1 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 232.8 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 202.1 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 305.1 |
SiO2 (mp-6930) | <1 0 1> | <1 1 -1> | 322.6 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 144.0 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 281.6 |
KCl (mp-23193) | <1 1 1> | <0 1 0> | 202.1 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 222.1 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 144.0 |
AlN (mp-661) | <1 0 1> | <1 1 -1> | 193.6 |
CeO2 (mp-20194) | <1 1 0> | <1 1 -1> | 322.6 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 144.0 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 144.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 161.2 |
BaF2 (mp-1029) | <1 0 0> | <1 1 0> | 281.6 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 202.1 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 288.1 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 231.0 |
CdS (mp-672) | <1 0 1> | <1 0 -1> | 230.8 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 317.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 268.7 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 185.0 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 216.1 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 215.0 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 202.1 |
Te2W (mp-22693) | <0 1 1> | <1 0 1> | 288.1 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 288.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 259.1 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 216.1 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 202.1 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 231.0 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 317.6 |
Te2Mo (mp-602) | <1 0 1> | <1 1 -1> | 322.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 185.0 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 310.4 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 57.7 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 259.1 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 173.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 0> | 140.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.21283 | 0.00000 | 1.16140 |
0.01255 | 0.32955 | 0.00455 | 0.00000 | 0.22058 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | -0.39213 | 0.00000 | -1.36545 |
Piezoelectric Modulus ‖eij‖max1.84510 C/m2 |
Crystallographic Direction vmax |
---|
-1.00000 |
0.00000 |
1.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.35 | 0.00 | 0.03 |
0.00 | 3.33 | 0.00 |
0.03 | 0.00 | 3.43 |
Dielectric Tensor εij (total) |
||
---|---|---|
18.60 | 0.00 | -14.55 |
0.00 | 6.87 | 0.00 |
-14.55 | 0.00 | 26.97 |
Polycrystalline dielectric constant
εpoly∞
3.37
|
Polycrystalline dielectric constant
εpoly
17.48
|
Refractive Index n1.84 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr3(P2O7)2 (mp-569271) | 0.4411 | 0.001 | 3 |
Cr3(P2O7)2 (mp-774562) | 0.4409 | 0.001 | 3 |
P4W3O14 (mvc-1031) | 0.4097 | 0.315 | 3 |
MnSiO3 (mp-25041) | 0.5385 | 0.016 | 3 |
Ni2P3O10 (mp-25610) | 0.5289 | 0.052 | 3 |
LiTiP2O7 (mp-752926) | 0.1297 | 0.077 | 4 |
LiFeP2O7 (mp-31785) | 0.1147 | 0.000 | 4 |
LiNiP2O7 (mp-32338) | 0.1503 | 0.065 | 4 |
LiCoP2O7 (mp-31519) | 0.0946 | 0.022 | 4 |
LiVP2O7 (mp-32405) | 0.0681 | 0.000 | 4 |
VO2 (mvc-6918) | 0.7452 | 0.095 | 2 |
MoO2 (mvc-6944) | 0.6593 | 0.281 | 2 |
Li7Sc9Fe(SiO3)20 (mp-764979) | 0.5223 | 0.040 | 5 |
Li2V2Sn(PO4)3 (mp-771573) | 0.5440 | 0.159 | 5 |
KLiTi2(PO5)2 (mp-774482) | 0.5142 | 0.027 | 5 |
Li7Sc9Fe(SiO3)20 (mp-851054) | 0.5320 | 0.060 | 5 |
Li2MnV(PO4)3 (mp-770135) | 0.5314 | 0.216 | 5 |
NaCa3ScZn3(SiO3)8 (mp-693463) | 0.5822 | 0.029 | 6 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.5766 | 0.257 | 6 |
NaCa2ScZn2(SiO3)6 (mp-534778) | 0.5825 | 0.025 | 6 |
KCa5Mg5Al(SiO3)12 (mp-534793) | 0.5695 | 0.033 | 6 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.5427 | 0.020 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.6158 | 0.068 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Li_sv Cr_pv P O |
Final Energy/Atom-7.2200 eV |
Corrected Energy-86.3491 eV
-86.3491 eV = -79.4201 eV (uncorrected energy) - 4.9160 eV (MP Anion Correction) - 2.0130 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)