Final Magnetic Moment15.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.482 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.034 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.44 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCr2P2O7 + Cr2O3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 1 0> | 300.6 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 300.6 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 157.0 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 150.3 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 171.2 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 300.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 225.4 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 85.6 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 256.8 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 157.0 |
BN (mp-984) | <0 0 1> | <0 1 0> | 225.4 |
MoS2 (mp-1434) | <0 0 1> | <1 0 -1> | 140.6 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 256.8 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 -1> | 140.6 |
LiGaO2 (mp-5854) | <1 0 1> | <1 1 0> | 227.8 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 225.4 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 256.8 |
TeO2 (mp-2125) | <0 1 0> | <1 0 -1> | 140.6 |
TeO2 (mp-2125) | <1 1 0> | <0 1 0> | 300.6 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 256.8 |
GdScO3 (mp-5690) | <0 0 1> | <0 1 0> | 225.4 |
Mg (mp-153) | <0 0 1> | <1 0 -1> | 140.6 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 150.3 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 171.2 |
GaP (mp-2490) | <1 1 0> | <0 1 0> | 300.6 |
TbScO3 (mp-31119) | <0 0 1> | <0 1 0> | 225.4 |
InSb (mp-20012) | <1 1 0> | <1 0 0> | 256.8 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 157.0 |
NdGaO3 (mp-3196) | <0 1 0> | <0 1 0> | 300.6 |
SiC (mp-11714) | <1 0 0> | <1 0 0> | 256.8 |
SiC (mp-11714) | <1 0 1> | <1 0 0> | 256.8 |
SiC (mp-11714) | <1 1 0> | <1 0 0> | 256.8 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 256.8 |
Si (mp-149) | <1 1 0> | <0 1 0> | 300.6 |
Au (mp-81) | <1 0 0> | <0 0 1> | 157.0 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 157.0 |
WS2 (mp-224) | <0 0 1> | <1 0 -1> | 140.6 |
C (mp-48) | <0 0 1> | <0 1 0> | 300.6 |
C (mp-48) | <1 0 1> | <0 1 0> | 300.6 |
C (mp-48) | <1 1 1> | <0 1 0> | 300.6 |
ZrO2 (mp-2858) | <0 1 0> | <0 1 0> | 300.6 |
ZrO2 (mp-2858) | <1 0 -1> | <1 0 0> | 256.8 |
ZrO2 (mp-2858) | <1 0 1> | <0 1 0> | 300.6 |
ZrO2 (mp-2858) | <1 1 -1> | <1 1 0> | 227.8 |
YAlO3 (mp-3792) | <1 1 1> | <0 1 0> | 300.6 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <0 0 1> | 157.0 |
SiC (mp-8062) | <1 1 1> | <0 1 0> | 300.6 |
MgF2 (mp-1249) | <1 0 0> | <0 1 1> | 174.0 |
ZnO (mp-2133) | <1 0 0> | <0 1 0> | 300.6 |
GaSb (mp-1156) | <1 0 0> | <0 0 1> | 157.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Fe4(PO4)3 (mp-31780) | 0.3314 | 0.020 | 3 |
Na2W2O7 (mp-25800) | 0.5659 | 0.022 | 3 |
Fe2PO5 (mp-24982) | 0.5307 | 0.018 | 3 |
P4W3O14 (mvc-1031) | 0.5694 | 0.212 | 3 |
Mn4(PO4)3 (mp-32010) | 0.4884 | 0.025 | 3 |
Li2Mn2(SO4)3 (mp-778555) | 0.4114 | 0.005 | 4 |
Li2Fe2(SO4)3 (mp-778400) | 0.3891 | 0.008 | 4 |
Li2Ni2(SO4)3 (mp-770331) | 0.3903 | 0.009 | 4 |
Li2Co2(SO4)3 (mp-778578) | 0.4029 | 0.013 | 4 |
Li2Mg2(SO4)3 (mp-14646) | 0.4438 | 0.000 | 4 |
Li4Mn5V(PO4)6 (mp-778320) | 0.5228 | 0.083 | 5 |
Li4Mn5Fe(PO4)6 (mp-777439) | 0.5017 | 0.066 | 5 |
Li3MnV(PO4)3 (mp-770205) | 0.4881 | 0.032 | 5 |
Li3MnV(PO4)3 (mp-770120) | 0.5039 | 0.042 | 5 |
Li7Fe3Co(PO4)6 (mp-775102) | 0.5167 | 0.069 | 5 |
Li4Mn2CrNi3(PO4)6 (mp-775171) | 0.5561 | 0.087 | 6 |
Li4Mn3CrCo2(PO4)6 (mp-763479) | 0.4942 | 0.081 | 6 |
Li4MnCr2Fe3(PO4)6 (mp-779026) | 0.5546 | 0.513 | 6 |
Li4TiMn3Cr2(PO4)6 (mp-778261) | 0.5282 | 0.081 | 6 |
Li4CrFe2Ni3(PO4)6 (mp-776753) | 0.5386 | 0.399 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Cr_pv P O |
Final Energy/Atom-7.6268 eV |
Corrected Energy-322.7758 eV
-322.7758 eV = -289.8168 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 16.1040 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)