Final Magnetic Moment6.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.645 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.036 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.00 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi3Cr2(PO4)3 |
Band Gap2.946 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP2/c [13] |
Hall-P 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 222.0 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 296.0 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 107.2 |
BaF2 (mp-1029) | <1 1 1> | <1 0 1> | 132.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 296.0 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 148.0 |
InAs (mp-20305) | <1 1 1> | <1 0 1> | 132.6 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 265.2 |
Te2Mo (mp-602) | <1 0 0> | <1 0 1> | 265.2 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 296.0 |
Ag (mp-124) | <1 1 1> | <1 0 1> | 265.2 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 132.6 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 107.2 |
GaSe (mp-1943) | <0 0 1> | <1 0 1> | 265.2 |
BN (mp-984) | <1 1 0> | <1 0 1> | 132.6 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 107.2 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 296.0 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 296.0 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 214.4 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 222.0 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 296.0 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 222.0 |
TeO2 (mp-2125) | <1 0 0> | <1 0 0> | 214.4 |
LiTaO3 (mp-3666) | <1 0 0> | <0 1 0> | 207.7 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 74.0 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 296.0 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 296.0 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 74.0 |
Fe3O4 (mp-19306) | <1 1 0> | <1 0 0> | 107.2 |
C (mp-66) | <1 1 0> | <1 0 0> | 107.2 |
C (mp-66) | <1 1 1> | <1 0 1> | 132.6 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 296.0 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 148.0 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 148.0 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 74.0 |
PbSe (mp-2201) | <1 1 1> | <1 0 1> | 132.6 |
PbSe (mp-2201) | <1 1 0> | <1 0 0> | 107.2 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 1> | 255.0 |
MoSe2 (mp-1634) | <1 1 0> | <1 0 1> | 265.2 |
Au (mp-81) | <1 0 0> | <0 0 1> | 296.0 |
CdSe (mp-2691) | <1 1 1> | <1 0 1> | 132.6 |
Ga2O3 (mp-886) | <1 1 0> | <1 0 0> | 214.4 |
CdSe (mp-2691) | <1 1 0> | <1 0 0> | 107.2 |
C (mp-48) | <1 1 0> | <1 0 1> | 132.6 |
C (mp-48) | <1 1 1> | <0 0 1> | 296.0 |
WSe2 (mp-1821) | <1 1 0> | <1 0 1> | 265.2 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 296.0 |
WSe2 (mp-1821) | <1 0 1> | <0 1 1> | 255.0 |
WSe2 (mp-1821) | <1 1 1> | <1 0 1> | 265.2 |
CaCO3 (mp-3953) | <1 0 0> | <1 0 1> | 265.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ni2PO5 (mp-769619) | 0.5692 | 0.035 | 3 |
Mn2PO5 (mp-770540) | 0.5411 | 0.016 | 3 |
MnCrO4 (mp-769911) | 0.6186 | 0.041 | 3 |
Fe4(PO4)3 (mp-31780) | 0.5794 | 0.019 | 3 |
MnMoO4 (mp-19081) | 0.5954 | 0.000 | 3 |
Li3Cr2(PO4)3 (mp-774463) | 0.2635 | 0.044 | 4 |
Li3Fe2(PO4)3 (mp-504385) | 0.2273 | 0.037 | 4 |
Li3V2(PO4)3 (mp-32530) | 0.1525 | 0.039 | 4 |
Li3V2(PO4)3 (mp-705382) | 0.1429 | 0.039 | 4 |
Li3Fe2(PO4)3 (mp-705422) | 0.2012 | 0.037 | 4 |
Li3MnV(PO4)3 (mp-775639) | 0.1759 | 0.069 | 5 |
Li6MnV3(PO4)6 (mp-764585) | 0.1865 | 0.057 | 5 |
Li6CrFe3(PO4)6 (mp-767788) | 0.2463 | 0.044 | 5 |
Li6MnCr3(PO4)6 (mp-767775) | 0.2481 | 0.047 | 5 |
Li6VFe3(PO4)6 (mp-761511) | 0.2441 | 0.046 | 5 |
Li4Mn2CrNi3(PO4)6 (mp-775171) | 0.3438 | 0.087 | 6 |
Li2Ti2MnCr2(PO4)6 (mp-743387) | 0.3648 | 0.013 | 6 |
Na2Li4Ti3Al(PO4)6 (mp-769069) | 0.3552 | 0.089 | 6 |
Li4V3Cr2Co(PO4)6 (mp-771298) | 0.3397 | 0.077 | 6 |
Li4TiCu2Ni3(PO4)6 (mp-776613) | 0.3462 | 0.100 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Li_sv Cr_pv P O |
Final Energy/Atom-7.0413 eV |
Corrected Energy-613.1170 eV
-613.1170 eV = -563.3030 eV (uncorrected energy) - 33.7099 eV (MP Anion Correction) - 16.1040 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)