Final Magnetic Moment8.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingUnknown |
Formation Energy / Atom-2.437 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.070 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.15 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCrPO4 + LiCrP2O7 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 167.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 292.9 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 251.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 334.8 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 334.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 292.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 292.9 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 334.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 83.7 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 114.7 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 334.8 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 125.5 |
Te2Mo (mp-602) | <0 0 1> | <1 0 1> | 229.4 |
Ag (mp-124) | <1 1 0> | <1 0 -1> | 221.6 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 334.8 |
BN (mp-984) | <0 0 1> | <0 0 1> | 292.9 |
BN (mp-984) | <1 0 0> | <0 0 1> | 251.1 |
BN (mp-984) | <1 0 1> | <0 0 1> | 334.8 |
BN (mp-984) | <1 1 1> | <0 0 1> | 251.1 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 251.1 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 251.1 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 334.8 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 167.4 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 334.8 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 83.7 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 167.4 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 -1> | 221.6 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 1> | 165.0 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 292.9 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 -1> | 221.6 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 292.9 |
MoS2 (mp-1434) | <1 0 1> | <0 0 1> | 209.2 |
Al (mp-134) | <1 0 0> | <0 0 1> | 292.9 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 292.9 |
TeO2 (mp-2125) | <1 1 1> | <0 0 1> | 209.2 |
MgO (mp-1265) | <1 1 1> | <1 0 -1> | 221.6 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 -1> | 221.6 |
MgO (mp-1265) | <1 1 0> | <1 0 1> | 229.4 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 334.8 |
TiO2 (mp-2657) | <1 0 0> | <1 1 -1> | 194.3 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 209.2 |
C (mp-66) | <1 0 0> | <0 0 1> | 125.5 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 125.5 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 292.9 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 -1> | 221.6 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 83.7 |
Mg (mp-153) | <1 1 0> | <1 0 1> | 114.7 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 125.5 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 -1> | 221.6 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 125.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MgV6(FeO6)4 (mvc-14468) | 0.4400 | 0.108 | 4 |
LiFe2(PO4)3 (mp-699352) | 0.2362 | 0.102 | 4 |
LiMn2(PO4)3 (mp-32023) | 0.1585 | 0.066 | 4 |
LiNi2P3O11 (mp-32389) | 0.4219 | 0.081 | 4 |
LiNi2(PO4)3 (mp-32397) | 0.3614 | 0.137 | 4 |
MoO2 (mvc-6944) | 0.5226 | 0.290 | 2 |
NiO2 (mvc-6939) | 0.5802 | 0.400 | 2 |
FeO2 (mvc-11999) | 0.5790 | 0.354 | 2 |
VO2 (mp-777469) | 0.4414 | 0.039 | 2 |
Cr5O12 (mp-19575) | 0.4466 | 0.025 | 2 |
Cr3InO8 (mp-569317) | 0.3783 | 0.107 | 3 |
LiCr3O8 (mp-566811) | 0.3520 | 0.002 | 3 |
Ni3(PO4)4 (mp-697806) | 0.3987 | 0.183 | 3 |
LiCr3O8 (mp-699330) | 0.3656 | 0.003 | 3 |
LiCr3O8 (mp-774328) | 0.3172 | 0.002 | 3 |
Li3MnV(PO4)3 (mp-775267) | 0.4984 | 0.036 | 5 |
Li6MnV3(PO4)6 (mp-775325) | 0.5050 | 0.025 | 5 |
LiMnPO4F (mp-762774) | 0.5105 | 0.054 | 5 |
Li3MnV(PO4)3 (mp-774297) | 0.5149 | 0.035 | 5 |
KLiTi2(PO5)2 (mp-774482) | 0.4719 | 0.030 | 5 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.5731 | 0.040 | 6 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.6206 | 0.001 | 6 |
NaLi3Ti2Fe2(PO4)6 (mp-850140) | 0.6057 | 0.011 | 6 |
Na2Gd2MgSi4(O6F)2 (mp-557538) | 0.6469 | 0.000 | 6 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.6051 | 0.020 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.6453 | 0.002 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-points21 |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Li_sv O P Cr_pv |
Final Energy/Atom-7.1137 eV |
Corrected Energy-281.0001 eV
-281.0001 eV = -256.0932 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 8.0520 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)