Final Magnetic Moment5.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.565 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.020 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.50 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiFe(PO3)4 |
Band Gap2.698 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCc [9] |
HallC 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 1> | <0 1 0> | 141.8 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 283.6 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 261.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 212.7 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 191.9 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 133.7 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 283.6 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 -1> | 151.8 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 283.6 |
MgO (mp-1265) | <1 1 1> | <0 1 0> | 283.6 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 0> | 219.5 |
LiTaO3 (mp-3666) | <1 0 1> | <1 0 0> | 219.5 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 -1> | 151.8 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 212.7 |
Mg (mp-153) | <1 1 0> | <1 1 0> | 261.3 |
GaP (mp-2490) | <1 1 0> | <1 0 0> | 219.5 |
TbScO3 (mp-31119) | <0 1 0> | <0 1 0> | 212.7 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 283.6 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 -1> | 151.8 |
PbSe (mp-2201) | <1 0 0> | <1 0 1> | 191.9 |
SiC (mp-11714) | <1 1 1> | <1 1 -1> | 167.5 |
NdGaO3 (mp-3196) | <1 0 0> | <1 0 0> | 219.5 |
MoSe2 (mp-1634) | <1 0 0> | <0 1 0> | 212.7 |
WS2 (mp-224) | <1 0 0> | <0 0 1> | 133.7 |
C (mp-48) | <1 0 0> | <0 0 1> | 133.7 |
C (mp-48) | <1 0 1> | <1 0 0> | 219.5 |
CdSe (mp-2691) | <1 0 0> | <1 0 1> | 191.9 |
ZrO2 (mp-2858) | <1 0 0> | <0 1 0> | 141.8 |
ZrO2 (mp-2858) | <1 1 0> | <0 1 0> | 283.6 |
YAlO3 (mp-3792) | <0 1 1> | <0 1 0> | 141.8 |
YAlO3 (mp-3792) | <0 0 1> | <0 1 0> | 141.8 |
YAlO3 (mp-3792) | <1 1 0> | <0 1 0> | 283.6 |
SiC (mp-8062) | <1 0 0> | <1 0 1> | 191.9 |
CdWO4 (mp-19387) | <0 1 1> | <0 1 0> | 283.6 |
CdWO4 (mp-19387) | <1 1 0> | <0 1 0> | 283.6 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 219.5 |
TiO2 (mp-390) | <1 1 1> | <1 1 -1> | 167.5 |
CdWO4 (mp-19387) | <1 0 0> | <1 0 0> | 219.5 |
TiO2 (mp-390) | <1 0 1> | <0 1 0> | 283.6 |
MgF2 (mp-1249) | <0 0 1> | <0 0 1> | 133.7 |
MgF2 (mp-1249) | <1 0 0> | <1 0 0> | 219.5 |
MgF2 (mp-1249) | <1 1 1> | <0 1 0> | 212.7 |
ZnO (mp-2133) | <1 0 0> | <1 1 0> | 261.3 |
ZnO (mp-2133) | <1 0 1> | <1 0 0> | 219.5 |
GaSb (mp-1156) | <1 0 0> | <1 0 1> | 191.9 |
SrTiO3 (mp-4651) | <1 0 0> | <1 0 0> | 219.5 |
LiAlO2 (mp-3427) | <1 1 1> | <0 1 0> | 283.6 |
CaF2 (mp-2741) | <1 1 0> | <1 0 0> | 219.5 |
Fe2O3 (mp-24972) | <1 0 0> | <1 0 0> | 219.5 |
ZnTe (mp-2176) | <1 0 0> | <1 0 1> | 191.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ni4P7O24 (mp-504245) | 0.4623 | 0.049 | 3 |
Fe4P7O24 (mp-504312) | 0.4569 | 0.173 | 3 |
Fe5(P3O11)2 (mp-31872) | 0.4403 | 0.366 | 3 |
Cr2P4O13 (mp-562181) | 0.4685 | 0.011 | 3 |
Cr4P7O24 (mp-585323) | 0.4392 | 0.080 | 3 |
LiCo(PO3)4 (mp-31603) | 0.1930 | 0.032 | 4 |
LiCr(PO3)4 (mp-31638) | 0.0801 | 0.032 | 4 |
LiV(PO3)4 (mp-32523) | 0.1807 | 0.000 | 4 |
LiNi(PO3)4 (mp-32352) | 0.2729 | 0.054 | 4 |
LiCo(PO3)4 (mp-697728) | 0.2875 | 0.032 | 4 |
Cr19O48 (mp-850874) | 0.7235 | 0.167 | 2 |
LiMnV(P2O7)2 (mp-764454) | 0.4947 | 0.007 | 5 |
LiVFe(P2O7)2 (mp-765127) | 0.5167 | 0.161 | 5 |
LiVCr(P2O7)2 (mp-765163) | 0.5168 | 0.044 | 5 |
LiVCr(P2O7)2 (mp-765180) | 0.4965 | 0.208 | 5 |
LiVFe(P2O7)2 (mp-765188) | 0.4933 | 0.007 | 5 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.6877 | 0.257 | 6 |
CsAlBP2HO9 (mp-542129) | 0.6845 | 0.000 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv P O |
Final Energy/Atom-7.0232 eV |
Corrected Energy-275.1572 eV
-275.1572 eV = -252.8363 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 5.4660 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)