Final Magnetic Moment5.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.583 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.061 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.37 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiMnPO4 |
Band Gap3.264 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFdd2 [43] |
HallF 2 2d |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LiF (mp-1138) | <1 0 0> | <0 1 0> | 65.8 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 329.0 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 263.2 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 273.5 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 329.0 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 273.5 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 171.1 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 263.2 |
GaSe (mp-1943) | <1 0 0> | <0 1 1> | 256.7 |
BN (mp-984) | <1 0 0> | <0 1 0> | 197.4 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 109.4 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 108.1 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 197.4 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 263.2 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 328.2 |
Al (mp-134) | <1 0 0> | <0 1 0> | 65.8 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 65.8 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 273.5 |
Al (mp-134) | <1 1 0> | <0 0 1> | 164.1 |
Al (mp-134) | <1 1 1> | <0 1 0> | 329.0 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 329.0 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 108.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 218.8 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 263.2 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 273.5 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 65.8 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 218.8 |
TeO2 (mp-2125) | <1 0 0> | <0 0 1> | 218.8 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 329.0 |
SiC (mp-7631) | <1 0 1> | <1 0 1> | 242.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 126.5 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 273.5 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 54.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 126.5 |
InAs (mp-20305) | <1 1 1> | <0 1 1> | 256.7 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 65.8 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 273.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 65.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 164.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 329.0 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 329.0 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 164.1 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 54.7 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 328.2 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 273.5 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 242.2 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 121.1 |
C (mp-66) | <1 0 0> | <0 0 1> | 218.8 |
GdScO3 (mp-5690) | <0 0 1> | <1 1 0> | 126.5 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 273.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.73363 | -0.60359 | -0.82812 | 0.00000 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.57014 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.47348 | 0.00000 |
Piezoelectric Modulus ‖eij‖max1.26029 C/m2 |
Crystallographic Direction vmax |
---|
-1.00000 |
0.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.04 | 0.00 | 0.00 |
0.00 | 3.00 | -0.00 |
0.00 | -0.00 | 3.00 |
Dielectric Tensor εij (total) |
||
---|---|---|
13.70 | 0.00 | 0.00 |
0.00 | 12.17 | -0.00 |
0.00 | -0.00 | 10.99 |
Polycrystalline dielectric constant
εpoly∞
3.01
|
Polycrystalline dielectric constant
εpoly
12.29
|
Refractive Index n1.74 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na2SeO4 (mp-5141) | 0.3261 | 0.000 | 3 |
Na2FeO4 (mp-775050) | 0.4779 | 0.203 | 3 |
Na2MoO4 (mp-25068) | 0.3400 | 0.018 | 3 |
Cd2SiO4 (mp-4530) | 0.2019 | 0.000 | 3 |
Na2SO4 (mp-4770) | 0.4942 | 0.000 | 3 |
LiFePO4 (mp-763758) | 0.1250 | 0.065 | 4 |
LiVPO4 (mp-763489) | 0.2188 | 0.083 | 4 |
LiNiPO4 (mp-765817) | 0.1747 | 0.072 | 4 |
LiCrPO4 (mp-31647) | 0.4240 | 0.022 | 4 |
LiCuPO4 (mp-584808) | 0.5258 | 0.037 | 4 |
Li2CrPO4F (mp-763748) | 0.5775 | 0.175 | 5 |
Li2FePO4F (mp-763745) | 0.6288 | 0.219 | 5 |
Li2VPO4F (mp-763730) | 0.6312 | 0.053 | 5 |
Li2MnPO4F (mp-762824) | 0.5976 | 0.039 | 5 |
Na2MnPO4F (mp-566286) | 0.6313 | 0.595 | 5 |
Explore more synthesis descriptions for materials of composition LiMnPO4.
Text computed by synthesisproject.org.
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv P O |
Final Energy/Atom-7.1237 eV |
Corrected Energy-108.7121 eV
-108.7121 eV = -99.7321 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction) - 3.3617 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)