Final Magnetic Moment3.871 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.413 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.165 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.90 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi3Mn3(PO4)4 + Li3PO4 |
Band Gap0.025 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [148] |
Hall-R 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 249.9 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 312.3 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 312.3 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 187.4 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 62.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 62.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 249.9 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 62.5 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 249.9 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 312.3 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 187.4 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 312.3 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 194.3 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 62.5 |
Al (mp-134) | <1 1 1> | <0 0 1> | 249.9 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 187.4 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 312.3 |
C (mp-66) | <1 0 0> | <0 0 1> | 312.3 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 187.4 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 187.4 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 312.3 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 62.5 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 62.5 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 249.9 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 249.9 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 62.5 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 187.4 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 312.3 |
Au (mp-81) | <1 0 0> | <0 0 1> | 312.3 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 62.5 |
WS2 (mp-224) | <1 1 1> | <0 0 1> | 249.9 |
WSe2 (mp-1821) | <1 1 1> | <0 0 1> | 249.9 |
WSe2 (mp-1821) | <1 0 0> | <0 0 1> | 249.9 |
WSe2 (mp-1821) | <1 1 0> | <0 0 1> | 249.9 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 187.4 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <0 0 1> | 187.4 |
YAlO3 (mp-3792) | <0 1 0> | <0 0 1> | 312.3 |
YAlO3 (mp-3792) | <1 0 0> | <0 0 1> | 312.3 |
ZnO (mp-2133) | <1 0 0> | <0 0 1> | 312.3 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 249.9 |
Cu (mp-30) | <1 0 0> | <0 0 1> | 312.3 |
GaTe (mp-542812) | <0 0 1> | <0 0 1> | 312.3 |
GaTe (mp-542812) | <1 0 -1> | <0 0 1> | 312.3 |
GaTe (mp-542812) | <1 0 0> | <0 0 1> | 187.4 |
ZnTe (mp-2176) | <1 0 0> | <0 0 1> | 187.4 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 62.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
PRhO4 (mp-28870) | 0.4384 | 0.000 | 3 |
MgCrO4 (mp-540704) | 0.4470 | 0.902 | 3 |
CdSiO3 (mp-776023) | 0.4362 | 0.027 | 3 |
V2Co2O7 (mp-547693) | 0.4525 | 0.164 | 3 |
CrPO4 (mp-19401) | 0.4239 | 0.000 | 3 |
Li3Co2(PO4)3 (mp-775012) | 0.1812 | 0.065 | 4 |
Li3V2(PO4)3 (mp-850900) | 0.1412 | 0.019 | 4 |
Li3Cr2(PO4)3 (mp-31706) | 0.1207 | 0.009 | 4 |
Li3Fe2(PO4)3 (mp-19430) | 0.1038 | 0.193 | 4 |
Li3Ti2(PO4)3 (mp-26883) | 0.0939 | 0.059 | 4 |
CrO2 (mvc-11581) | 0.7237 | 0.166 | 2 |
VO2 (mp-777469) | 0.6269 | 0.038 | 2 |
VO2 (mvc-6918) | 0.6448 | 0.095 | 2 |
MoO2 (mvc-6944) | 0.5327 | 0.281 | 2 |
Li6MnV3(PO4)6 (mp-775325) | 0.1653 | 0.030 | 5 |
Li6MnV3(PO4)6 (mp-779201) | 0.1502 | 0.021 | 5 |
Li6MnV3(PO4)6 (mp-778983) | 0.1681 | 0.027 | 5 |
Li3MnV(PO4)3 (mp-778888) | 0.0994 | 0.044 | 5 |
Li3MnV(PO4)3 (mp-774297) | 0.1621 | 0.192 | 5 |
Li4Mn3CrCo2(PO4)6 (mp-763479) | 0.5785 | 0.080 | 6 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.6072 | 0.257 | 6 |
NaLi3Ti2Fe2(PO4)6 (mp-850140) | 0.4529 | 0.114 | 6 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.4762 | 0.020 | 6 |
Li4CrFe2Ni3(PO4)6 (mp-776753) | 0.5953 | 0.778 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.7301 | 0.068 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv P O |
Final Energy/Atom-6.8066 eV |
Corrected Energy-295.8413 eV
-295.8413 eV = -272.2629 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)