Final Magnetic Moment10.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.649 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.017 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.73 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiMn6P7O24 + LiPO3 |
Band Gap3.987 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP2/c [13] |
Hall-P 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 361.9 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 144.8 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 361.9 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 108.6 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 361.9 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 325.7 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 144.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 181.0 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 144.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 181.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 144.8 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 289.5 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 289.5 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 325.7 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 181.0 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 72.4 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 144.8 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 289.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 136.7 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 181.0 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 289.5 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 325.7 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 144.8 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 259.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 289.5 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 72.4 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 217.2 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 253.4 |
Te2W (mp-22693) | <0 0 1> | <1 0 -1> | 133.0 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 108.6 |
Te2W (mp-22693) | <1 1 0> | <0 0 1> | 108.6 |
C (mp-66) | <1 0 0> | <0 0 1> | 181.0 |
C (mp-66) | <1 1 0> | <0 0 1> | 36.2 |
C (mp-66) | <1 1 1> | <0 0 1> | 181.0 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 253.4 |
YVO4 (mp-19133) | <1 0 0> | <1 0 1> | 136.7 |
YVO4 (mp-19133) | <1 0 1> | <1 0 -1> | 133.0 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 108.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 289.5 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 72.4 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 217.2 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 144.8 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 144.8 |
KP(HO2)2 (mp-23959) | <0 1 1> | <0 0 1> | 108.6 |
BN (mp-984) | <0 0 1> | <0 0 1> | 108.6 |
BN (mp-984) | <1 0 0> | <0 0 1> | 253.4 |
BN (mp-984) | <1 0 1> | <1 1 0> | 160.1 |
BN (mp-984) | <1 1 0> | <0 0 1> | 325.7 |
BN (mp-984) | <1 1 1> | <0 0 1> | 325.7 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 181.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
FeSiO3 (mp-650392) | 0.5957 | 0.021 | 3 |
MnSiO3 (mp-565815) | 0.5743 | 0.007 | 3 |
Cr4Si4O13 (mp-768078) | 0.6020 | 0.079 | 3 |
MnSiO3 (mp-19528) | 0.6159 | 0.007 | 3 |
Mn5(P3O11)2 (mp-31954) | 0.6194 | 0.028 | 3 |
Li3Co2P5O16 (mp-585240) | 0.2352 | 0.019 | 4 |
Li3Co2P5O16 (mp-31618) | 0.2838 | 0.019 | 4 |
Li3Fe2P5O16 (mp-31885) | 0.1714 | 0.018 | 4 |
Li3V2P5O16 (mp-32508) | 0.2814 | 0.037 | 4 |
Li3Fe2P5O16 (mp-695779) | 0.2543 | 0.018 | 4 |
LiMnV(P2O7)2 (mp-764615) | 0.5667 | 0.007 | 5 |
Li4MnV3(P2O7)4 (mp-766112) | 0.5488 | 0.008 | 5 |
LiMnV(P2O7)2 (mp-764480) | 0.5668 | 0.007 | 5 |
Li2MnV(P2O7)2 (mp-778770) | 0.5663 | 0.018 | 5 |
Li3MnV(P2O7)2 (mp-850951) | 0.5690 | 0.000 | 5 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.7227 | 0.002 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv P O |
Final Energy/Atom-7.0985 eV |
Corrected Energy-398.3198 eV
-398.3198 eV = -369.1231 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)